| MECHANISM OF NON-EQUILIBRIUM SEGREGATION OF SOLUTE TO GRAIN BOUNDARIES |
| CHU Youyi;ZHANG Sanhong;HE Xinlai;KE Jun T. Ko Beijing University of Science and Technology |
|
Cite this article:
CHU Youyi;ZHANG Sanhong;HE Xinlai;KE Jun T. Ko Beijing University of Science and Technology. MECHANISM OF NON-EQUILIBRIUM SEGREGATION OF SOLUTE TO GRAIN BOUNDARIES. Acta Metall Sin, 1989, 25(4): 41-47.
|
|
|
Abstract In consideration of the local equilibrium among vacancies, solute atomsand vacancy-solute atom complexes, and the influence of equilibrium grain bound-ary segregation, theoretical dynamic formulas for non-equilibrium grain boundarysegregation of solute have been derived on the basis of the vacancy-draggingmechanism. Theoretical calculation by computer has been carried out for the non-equilibrium segregation of B to austenitic grain boundaries during isothermal hold-ing and continuous cooling after heating at high temperatures. The results agree wellwith those obtained from experiments.
|
|
Received: 18 April 1989
|
1 Williams T M, Stoncham A M, Harries D R. Met Sci, 1976; 10: 14 2 贺信莱,褚幼义,柯俊.金属学报,1982;18:1,11 3 Karlsson L. Ph. D. Thesis, Chalmers Universlty of Technology, Goteborg, Sweden, 1986 4 褚幼义,贺信莱,唐立,徐庭栋,柯俊.金属学报,1987;23:A169 5 贺信莱,褚幼义,唐立,周振新,柯俊.金属学报,1987;23:A291 6 Balluffi R W. Grain-Boundary Structure and Kinetics, Matals Park, Ohio: ASM, 1980: 297 7 Smith A F, Gibbs G B. Met Sci J, 1968; 2: 47 8 Hudson J A, Nelson R S. In: Smallman R E, Harrris J E eds., Vacancies 76, London: The Metal Society, 1977: 126 9 Brailsford A D, Bullough R. J Nucl Mater, 1972; 44: 121 10 Busby P E, Warga M E, Wells C. Trans AIME, 1953; 197: 1463 11 Doyama M. J Nucl Mater, 1978; 69 & 70: 350 12 Rowcliffe A F, Nicholson R B. Acta Metall, 1972; 20: 143 13 De Schepper L, Seger S D, Dorikens-Vanpraet L, Dorikens M, Knuyt G, Stals L M, Moser P. Phys Rev B, 1983; 27: 5257 14 Jandeska W F, Morral J E. Metall Trans, 1972; 3: 2933 15 Chapman M A V, Faulkner R G. Acta Metall, 1983; 31: 677 16 Miller J W. Phys Rev, 1969; 188: 1074 17 McLean D.金属中的晶粒间界(中译本):科学出版社,1965:119 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|