Abstract  In consideration of the local equilibrium among vacancies, solute atomsand vacancy-solute atom complexes, and the influence of equilibrium grain bound-ary segregation, theoretical dynamic formulas for non-equilibrium grain boundarysegregation of solute have been derived on the basis of the vacancy-draggingmechanism. Theoretical calculation by computer has been carried out for the non-equilibrium segregation of B to austenitic grain boundaries during isothermal hold-ing and continuous cooling after heating at high temperatures. The results agree wellwith those obtained from experiments.
Key words:  solute atoms      non-equilibrium segregation      boron      grain boundary     
Received:  18 April 1989     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1989/V25/I4/41

1 Williams T M, Stoncham A M, Harries D R. Met Sci, 1976; 10: 14
2 贺信莱,褚幼义,柯俊.金属学报,1982;18:1,11
3 Karlsson L. Ph. D. Thesis, Chalmers Universlty of Technology, Goteborg, Sweden, 1986
4 褚幼义,贺信莱,唐立,徐庭栋,柯俊.金属学报,1987;23:A169
5 贺信莱,褚幼义,唐立,周振新,柯俊.金属学报,1987;23:A291
6 Balluffi R W. Grain-Boundary Structure and Kinetics, Matals Park, Ohio: ASM, 1980: 297
7 Smith A F, Gibbs G B. Met Sci J, 1968; 2: 47
8 Hudson J A, Nelson R S. In: Smallman R E, Harrris J E eds., Vacancies 76, London: The Metal Society, 1977: 126
9 Brailsford A D, Bullough R. J Nucl Mater, 1972; 44: 121
10 Busby P E, Warga M E, Wells C. Trans AIME, 1953; 197: 1463
11 Doyama M. J Nucl Mater, 1978; 69 & 70: 350
12 Rowcliffe A F, Nicholson R B. Acta Metall, 1972; 20: 143
13 De Schepper L, Seger S D, Dorikens-Vanpraet L, Dorikens M, Knuyt G, Stals L M, Moser P. Phys Rev B, 1983; 27: 5257
14 Jandeska W F, Morral J E. Metall Trans, 1972; 3: 2933
15 Chapman M A V, Faulkner R G. Acta Metall, 1983; 31: 677
16 Miller J W. Phys Rev, 1969; 188: 1074
17 McLean D.金属中的晶粒间界(中译本):科学出版社,1965:119
[1] CHANG Songtao, ZHANG Fang, SHA Yuhui, ZUO Liang. Recrystallization Texture Competition Mediated by Segregation Element in Body-Centered Cubic Metals[J]. 金属学报, 2023, 59(8): 1065-1074.
[2] XU Yongsheng, ZHANG Weigang, XU Lingchao, DAN Wenjiao. Simulation of Deformation Coordination and Hardening Behavior in Ferrite-Ferrite Grain Boundary[J]. 金属学报, 2023, 59(8): 1042-1050.
[3] ZHANG Haifeng, YAN Haile, FANG Feng, JIA Nan. Molecular Dynamic Simulations of Deformation Mechanisms for FeMnCoCrNi High-Entropy Alloy Bicrystal Micropillars[J]. 金属学报, 2023, 59(8): 1051-1064.
[4] WANG Zongpu, WANG Weiguo, Rohrer Gregory S, CHEN Song, HONG Lihua, LIN Yan, FENG Xiaozheng, REN Shuai, ZHOU Bangxin. {111}/{111} Near Singular Boundaries in an Al-Zn-Mg-Cu Alloy Recrystallized After Rolling at Different Temperatures[J]. 金属学报, 2023, 59(7): 947-960.
[5] LI Fulin, FU Rui, BAI Yunrui, MENG Lingchao, TAN Haibing, ZHONG Yan, TIAN Wei, DU Jinhui, TIAN Zhiling. Effects of Initial Grain Size and Strengthening Phase on Thermal Deformation and Recrystallization Behavior of GH4096 Superalloy[J]. 金属学报, 2023, 59(7): 855-870.
[6] LI Xin, JIANG He, YAO Zhihao, DONG Jianxin. Theoretical Calculation and Analysis of the Effect of Oxygen Atom on the Grain Boundary of Superalloy Matrices Ni, Co and NiCr[J]. 金属学报, 2023, 59(2): 309-318.
[7] YANG Du, BAI Qin, HU Yue, ZHANG Yong, LI Zhijun, JIANG Li, XIA Shuang, ZHOU Bangxin. Fractal Analysis of the Effect of Grain Boundary Character on Te-Induced Brittle Cracking in GH3535 Alloy[J]. 金属学报, 2023, 59(2): 248-256.
[8] LIU Lujun, LIU Zheng, LIU Renhui, LIU Yong. Grain Boundary Structure and Coercivity Enhancement of Nd90Al10 Alloy Modified NdFeB Permanent Magnets by GBD Process[J]. 金属学报, 2023, 59(11): 1457-1465.
[9] WANG Jiangwei, CHEN Yingbin, ZHU Qi, HONG Zhe, ZHANG Ze. Grain Boundary Dominated Plasticity in Metallic Materials[J]. 金属学报, 2022, 58(6): 726-745.
[10] LI Haiyong, LI Saiyi. Effect of Temperature on Migration Behavior of <111> Symmetric Tilt Grain Boundaries in Pure Aluminum Based on Molecular Dynamics Simulations[J]. 金属学报, 2022, 58(2): 250-256.
[11] HU Biao, ZHANG Huaqing, ZHANG Jin, YANG Mingjun, DU Yong, ZHAO Dongdong. Progress in Interfacial Thermodynamics and Grain Boundary Complexion Diagram[J]. 金属学报, 2021, 57(9): 1199-1214.
[12] LIU Zhongwu, HE Jiayi. Several Issues on the Development of Grain Boundary Diffusion Process for Nd-Fe-B Permanent Magnets[J]. 金属学报, 2021, 57(9): 1155-1170.
[13] NI Ke, YANG Yinhui, CAO Jianchun, WANG Liuhang, LIU Zehui, QIAN Hao. Softening Behavior of 18.7Cr-1.0Ni-5.8Mn-0.2N Low Nickel-Type Duplex Stainless Steel During Hot Compression Deformation Under Large Strain[J]. 金属学报, 2021, 57(2): 224-236.
[14] SUN Jia, LI Xuexiong, ZHANG Jinhu, WANG Gang, YANG Mei, WANG Hao, XU Dongsheng. Phase Field Modeling of Formation Mechanism of Grain Boundary Allotriomorph in β→α Phase Transformation in Ti-6Al-4V Alloy[J]. 金属学报, 2020, 56(8): 1113-1122.
[15] LI Xiucheng,SUN Mingyu,ZHAO Jingxiao,WANG Xuelin,SHANG Chengjia. Quantitative Crystallographic Characterization of Boundaries in Ferrite-Bainite/Martensite Dual-Phase Steels[J]. 金属学报, 2020, 56(4): 653-660.
No Suggested Reading articles found!