| ACTIVITIES OF COMPONENTS IN MgO-B_2O_3 MELT |
| ZHANG Chengtao;JI Chunlin Northeast University of Technology; Shenyang |
|
Cite this article:
ZHANG Chengtao;JI Chunlin Northeast University of Technology; Shenyang. ACTIVITIES OF COMPONENTS IN MgO-B_2O_3 MELT. Acta Metall Sin, 1989, 25(4): 100-103.
|
|
|
Abstract The activity of MgO in MgO-B_2O_3 melt was experimentally determinedat 1500 and 1550℃ by means of slag-liquid Sn equilibrium. The activity of B_2O_3was calculated by integrating Gibbs-Duhem equation. The standard Gibbs energies offormation of binary compounds 2MgO·B_2O_3 and 3MgO·B_2O_3 were estimated withthe activity data of components in B_2O_3-MgO melt.
|
|
Received: 18 April 1989
|
1 邹元爔,赵彭年.中国科学,1962;11:1287 2 邹元爔,赵彭年,曹兆民.金属学报,1963:6:121 3 魏寿昆.活度在冶金物理化学中的作用,北京:中国工业出版社,1964:67 4 Robert S R. Takinegas. Lawrence P C. Phase Diagrams for Ceramists, Vol. Ⅳ, Am. Ceram. Soc., 1981; 99 |