MODIFICATION EFFECT OF Sr ON Al-Si ALLOY
LIU Qiyang;LI Qingchun;ZHANG Jiren Harbin Institute of Technology
Cite this article: 

LIU Qiyang;LI Qingchun;ZHANG Jiren Harbin Institute of Technology. MODIFICATION EFFECT OF Sr ON Al-Si ALLOY. Acta Metall Sin, 1989, 25(4): 104-109.

Download:  PDF(819KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  By inserting the single crystal silicon seeds into Sr modified A1-22wt-%Si alloy melts, the fact that nucleation and growth of Si-phase are affectedby Sr addition has been confirmed. It is suggested that this effect is caused by theadsorption of Sr on {111}_(si), and the modification of eutectic structure results fromthe variation of leading phase in the eutectic from Si to α-Al
Key words:  Al-Si alloy      Sr      modification     
Received:  18 April 1989     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1989/V25/I4/104

1 Yilmaz F. Elliott R. Met Sci, 1984; 18: 362
2 Glenister S M D. Elliott R. Met Sci, 1981; 15: 181
3 Alker K, Hielscher U. Aluminium. 1972; 48: 362
4 毛晓禹,陈继森,吴占贤,王草原.金属学报,1983;19:A220
5 黄良余,王玉琮,翟春泉,丁文江.金属学报,1986;22:A310
6 郑朝贵,姚连克,张启运.金属学报,1982;18:661
7 朱培钺,贾均,侯廷秀.现代铸造,1982;(2) :1
8 刘启阳.哈尔滨工业大学工学博士学位论文,1987
9 Liu Qiyang(刘启阳),Li Qingchun(李庆春),Zhang Jiren(张吉人).Scr Metall,1988;22:789
10 甘肃师范大学化学系编.简明化学手册,甘肃人民出版社,1980:20
[1] ZHANG Lili, JI Zongwei, ZHAO Jiuzhou, HE Jie, JIANG Hongxiang. Key Factors Influencing Eutectic Si Modification in Al-Si Hypoeutectic Alloy by Trace La[J]. 金属学报, 2023, 59(11): 1541-1546.
[2] GAO Han, LIU Li, ZHOU Xiaoyu, ZHOU Xinyi, CAI Wenjun, ZHOU Hongling. Preparation and Bioactivity of Micro-Nano Structure on Ti6Al4V Surface[J]. 金属学报, 2023, 59(11): 1466-1474.
[3] LIU Lujun, LIU Zheng, LIU Renhui, LIU Yong. Grain Boundary Structure and Coercivity Enhancement of Nd90Al10 Alloy Modified NdFeB Permanent Magnets by GBD Process[J]. 金属学报, 2023, 59(11): 1457-1465.
[4] CUI Zhenduo, ZHU Jiamin, JIANG Hui, WU Shuilin, ZHU Shengli. Research Progress of the Surface Modification of Titanium and Titanium Alloys for Biomedical Application[J]. 金属学报, 2022, 58(7): 837-856.
[5] YANG Lipo, ZHANG Hailong, ZHANG Yongshun. Present Analysis and Trend Prediction of Shape/ Performance Collaborative Control for High-End Cold Rolling Foils[J]. 金属学报, 2021, 57(3): 295-308.
[6] ZHENG Qiuju, YE Zhongfei, JIANG Hongxiang, LU Ming, ZHANG Lili, ZHAO Jiuzhou. Effect of Micro-Alloying Element La on Solidification Microstructure and Mechanical Properties of Hypoeutectic Al-Si Alloys[J]. 金属学报, 2021, 57(1): 103-110.
[7] ZHANG Conghui, RONG Hua, SONG Guodong, HU Kun. Effect of Surface Roughness by Shot Peening on Stress Corrosion Cracking Behavior of Pure Titanium Welded Joints in HCl Solution[J]. 金属学报, 2019, 55(10): 1282-1290.
[8] Guangdong WANG, Ni TIAN, Changshu HE, Gang ZHAO, Liang ZUO. Formation of Second-Phases in a Direct-Chill Casting Al-12Si-0.65Mg-xMn Alloy[J]. 金属学报, 2018, 54(7): 1059-1067.
[9] Di ZHANG, Mengying YUAN, Zhanqiu TAN, Ding-Bang XIONG, Zhiqiang LI. Progress in Interface Modification and Nanoscale Study of Diamond/Cu Composites[J]. 金属学报, 2018, 54(11): 1586-1596.
[10] Yun SHU, Maocheng YAN, Yinghua WEI, Fuchun LIU, En-Hou HAN, Wei KE. Characteristics of SRB Biofilm and Microbial Corrosionof X80 Pipeline Steel[J]. 金属学报, 2018, 54(10): 1408-1416.
[11] Ning LI,Rong ZHANG,Limin ZHANG,Hui XING,Pengfei YIN,Yaoyan WU. Study on Grain Refinement Mechanism of Hypoeutectic Al-7%Si Alloy Under Low Voltage Alternating Current Pulse[J]. 金属学报, 2017, 53(2): 192-200.
[12] Erlin ZHANG, Xiaoyan WANG, Yong HAN. Research Status of Biomedical Porous Ti and Its Alloy in China[J]. 金属学报, 2017, 53(12): 1555-1567.
[13] Zhentao YU, Sen YU, Jun CHENG, Xiqun MA. Development and Application of Novel Biomedical Titanium Alloy Materials[J]. 金属学报, 2017, 53(10): 1238-1264.
[14] Xiao LIN, Jun GE, Shuilin WU, Baohua LIU, Huilin YANG, Lei YANG. Advances in Metallic Biomaterials with both Osteogenic and Anti-Infection Properties[J]. 金属学报, 2017, 53(10): 1284-1302.
[15] Yongchang QING,Zhiwei YANG,Jun XIAN,Jin XU,Maocheng YAN,Tangqing WU,Changkun YU,Libao YU,Cheng SUN. CORROSION BEHAVIOR OF Q235 STEEL UNDER THE INTERACTION OF ALTERNATING CURRENT AND MICROORGANISMS[J]. 金属学报, 2016, 52(9): 1142-1152.
No Suggested Reading articles found!