PHASE DIAGRAM OF Nd-Pd(Nd≤50at.-%) BINARY SYSTEM
CHEN Lili;ZHANG Kanghou Institute of Precious Metals; Kunming
Cite this article: 

CHEN Lili;ZHANG Kanghou Institute of Precious Metals; Kunming. PHASE DIAGRAM OF Nd-Pd(Nd≤50at.-%) BINARY SYSTEM. Acta Metall Sin, 1991, 27(1): 94-97.

Download:  PDF(382KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The region containing O-50at. -%Nd in Nd-Pd phase diagram has beenstudied with X-ray diffraction, differential thermal analysis and micrography. Ithas been found that there are six intermetallic compounds, viz: NdPd_5, NdPd_3, NdPd_2,Nd_2Pd_3, Nd_4Pd_5 and NdPd in the region. NdPd_3, Nd_4Pd_5 and NdPd are solid-liquidcongruent compoundls with melting points of 1217±4℃, 970±4℃ and 952±4℃respectively. It has been determined also that NdPd_5 has a SmPt_5-type structure withα=0.5265nm, b=0.9219nm and c=2.570nm, NdPd_3 a AuCu_3-type structure withα=0.4137nm, and NdPd below 708±4℃ a CrB-type structure with α=0.3827nm.b=1.079nm and c=0.4547nm. There exist three eutectic reactions L?(Pd)+NdPd_5,L?NdPd_2+Nd_2Pd_3 and L?Nd_4Pd_5+NdPd, and three peritectic reactions L+NdPd_3?-NdPd_5, L+NdPd+3?NdPd_2 and L+Nd_4Pd_5?Nd_2Pd_3 in the region.
Key words:  Nd-Pd binary system      phase diagram      X-ray diffraction      differential thermal analysis     
Received:  18 January 1991     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1991/V27/I1/94

1 Parnell D G, Brett N H, Haines H R, Potter P E. J Less Common Met, 1986; 115: 167
2 Bronger W. J Lees-Common Met, 1967; 12: 63
3 张康侯,陈藜莉,金属学报,1988; 24: B65
4 Loebich O Jr., Raub E. J Less-Common Met, 1973; 30: 47
5 Gschneidner K A Jr., Eyring L R. Handbook on the Physics and Chemistry of Rare Earths, Vol. II, Amsterdam: North-Holland, 1979
6 Vassallo D A, Harden J C. Anal Chem, 1962; 34(1) : 132
7 Barrall E M. Thermochim Acta, 1973; 5: 377
[1] LI Shilei, LI Yang, WANG Youkang, WANG Shengjie, HE Lunhua, SUN Guang'ai, XIAO Tiqiao, WANG Yandong. Multiscale Residual Stress Evaluation of Engineering Materials/Components Based on Neutron and Synchrotron Radiation Technology[J]. 金属学报, 2023, 59(8): 1001-1014.
[2] GAO Xiang, ZHANG Guikai, XIANG Xin, LUO Lizhu, WANG Xiaolin. Effects of Alloying Elements on the Adsorption of Oxygen on V(110) Surfaces: A First-Principles Study[J]. 金属学报, 2020, 56(6): 919-928.
[3] LI Yizhuang,HUANG Mingxin. A Method to Calculate the Dislocation Density of a TWIP Steel Based on Neutron Diffraction and Synchrotron X-Ray Diffraction[J]. 金属学报, 2020, 56(4): 487-493.
[4] LI Changji,ZOU Minjie,ZHANG Lei,WANG Yuanming,WANG Sucheng. High-Resolution X-Ray Diffraction Analysis of Epitaxial Films[J]. 金属学报, 2020, 56(1): 99-111.
[5] Weifeng HE, Xiang LI, Xiangfan NIE, Yinghong LI, Sihai LUO. Study on Stability of Residual Stress Induced by Laser Shock Processing in Titanium Alloy Thin-Components[J]. 金属学报, 2018, 54(3): 411-418.
[6] Yutuo ZHANG,Cong LI,Pei WANG,Dianzhong LI. IN SITU SYNCHROTRON X-RAY DIFFRACTION INVESTIGATION ON TENSILE PROPERTIES OF 9Ni STEEL[J]. 金属学报, 2016, 52(4): 403-409.
[7] Shenghua ZHANG,Pei WANG,Dianzhong LI,Yiyi LI. INVESTIGATION OF TRIP EFFECT IN ZG06Cr13Ni4Mo MARTENSITIC STAINLESS STEEL BY IN SITU SYNCHROTRON HIGH ENERGY X-RAY DIFFRACTION[J]. 金属学报, 2015, 51(11): 1306-1314.
[8] ZHANG Weibin SHA Chunsheng DU Yong WEN Guanghua XIE Wen WANG Shequan. COMPUTER SIMULATIONS AND VERIFICATION OF GRADIENT ZONE FORMATION IN CEMENTED CARBIDES[J]. 金属学报, 2011, 47(10): 1307-1314.
[9] Zhao Ning. THE LIQUID STRUCTURE OF SN-CU LEAD-FREE SOLDERS[J]. 金属学报, 2008, 44(4): 467-472 .
[10] ZHANG Huawei; LI Yanxiang; LIU Yuan. Study of Metal--Hydrogen Binary Phase Diagram in Gasar Process[J]. 金属学报, 2005, 41(1): 55-.
[11] JIANG Chuanhai; WU Jiansheng; WANG Dezun. X--Ray Diffraction Analysis for the Recrystallization Behavior Of SiCw/Al Composite at High Temperature[J]. 金属学报, 2004, 40(10): 1023-1026 .
[12] WANG Huabin; HAN Jiecai; ZHANG Xinhong; DU Shanyi (Center for Composite Materials; Harbin Institute of Technology; Harbin 150001)Correspondent: WANG Huabin; lecturer;Tel: (0451)6414167; Fax: (0451)6415605. REACTION MECHANISM OF CONTINUALLY HEATING Ni AND A1 PARTICLES[J]. 金属学报, 1998, 34(9): 992-998.
[13] ZHANG Jian(Metallurgical Engineering School; University of Science and Technology Beijing; Beijing 100083). CONSISTENCY(OR SIMILARITY) OF THERMODYNAMIC PROPERTIES OF METALLURGICAL MELTS WITH THEIR PHASE DIAGRAMS[J]. 金属学报, 1998, 34(7): 742-752.
[14] PAN Hongge; DU Honglin; CHEN Changpin; HAN Xiufeng; YANG Fuming (Department of Materials Science and Engineering; Zhejiang University; Hangzhou 310027)(State Key Laboratory for Magnetism; Institute of Physics; The Chinese Academy of Sciences; Beijing 100080)(Institute of Chinese Atomic Energy; Beijing 102413). STRUCTURAL CHARACTERIZATION OF THE Y_3(Fe, Mo)_(29) INTERMETALLIC COMPOUND[J]. 金属学报, 1998, 34(5): 473-482.
[15] Zhang Jian (Institute of Metallurgy; University of Science and Technology Beijing; Beijing 100083). CLASSIFICATION OF THERMODYNAMIC PROPERTIES OF BINARY METALLIC MELTS ACCORDING TO THEIR PHASE DIAGRAMS[J]. 金属学报, 1998, 34(1): 75-85.
No Suggested Reading articles found!