| PHASE DIAGRAM OF Nd-Pd(Nd≤50at.-%) BINARY SYSTEM |
| CHEN Lili;ZHANG Kanghou Institute of Precious Metals; Kunming |
|
Cite this article:
CHEN Lili;ZHANG Kanghou Institute of Precious Metals; Kunming. PHASE DIAGRAM OF Nd-Pd(Nd≤50at.-%) BINARY SYSTEM. Acta Metall Sin, 1991, 27(1): 94-97.
|
|
|
Abstract The region containing O-50at. -%Nd in Nd-Pd phase diagram has beenstudied with X-ray diffraction, differential thermal analysis and micrography. Ithas been found that there are six intermetallic compounds, viz: NdPd_5, NdPd_3, NdPd_2,Nd_2Pd_3, Nd_4Pd_5 and NdPd in the region. NdPd_3, Nd_4Pd_5 and NdPd are solid-liquidcongruent compoundls with melting points of 1217±4℃, 970±4℃ and 952±4℃respectively. It has been determined also that NdPd_5 has a SmPt_5-type structure withα=0.5265nm, b=0.9219nm and c=2.570nm, NdPd_3 a AuCu_3-type structure withα=0.4137nm, and NdPd below 708±4℃ a CrB-type structure with α=0.3827nm.b=1.079nm and c=0.4547nm. There exist three eutectic reactions L?(Pd)+NdPd_5,L?NdPd_2+Nd_2Pd_3 and L?Nd_4Pd_5+NdPd, and three peritectic reactions L+NdPd_3?-NdPd_5, L+NdPd+3?NdPd_2 and L+Nd_4Pd_5?Nd_2Pd_3 in the region.
|
|
Received: 18 January 1991
|
1 Parnell D G, Brett N H, Haines H R, Potter P E. J Less Common Met, 1986; 115: 167 2 Bronger W. J Lees-Common Met, 1967; 12: 63 3 张康侯,陈藜莉,金属学报,1988; 24: B65 4 Loebich O Jr., Raub E. J Less-Common Met, 1973; 30: 47 5 Gschneidner K A Jr., Eyring L R. Handbook on the Physics and Chemistry of Rare Earths, Vol. II, Amsterdam: North-Holland, 1979 6 Vassallo D A, Harden J C. Anal Chem, 1962; 34(1) : 132 7 Barrall E M. Thermochim Acta, 1973; 5: 377 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|