OBSERVATION OF TWIN CONFIGURATIONIN β-SiC WHISKERS
ZHOU Yanchun;CHANG Xin;ZHOU Jing;XIA Fei Institute of Metal Research; Academia Sinica; Shenyang
Cite this article:
ZHOU Yanchun;CHANG Xin;ZHOU Jing;XIA Fei Institute of Metal Research; Academia Sinica; Shenyang. OBSERVATION OF TWIN CONFIGURATIONIN β-SiC WHISKERS. Acta Metall Sin, 1991, 27(1): 121-125.
Abstract The twin configuration of β-SiC whiskers prepared by the vapour-liquid-solid process was investigated under TEM. In the whiskets with "bamboo jo-int" morphology, the β-SiC part is jointed with the one-dimensional disorderedpart by the {111}_β twin boundary, microtwins of several atomic layer thick werepresent in β-SiC region. It was noted that the {111}_β twin boundary divides someβ-SiC regions into two parts. The second-order twin joint was also observed at thewhisker tip and the branching position of the bicrystalline whisker. Electron diffra-ction analysis demonstrated that the twin boundary in the bicrystalline whisker isparallel to the matrix {001)_M plane.
1 Nutt S R. J Am Ceram Soc. 1984; 67: 428--431 2 Nutt S R. J Am Ceram Soc, 1988; 71: 149--156 3 Iwanaga H, Yoshiie T, Katuki H, Egashira M. J Mater Sci Lett, 1986; 5: 946--948 4 Chang Xin, Zhou Yanchun, Xia Fei. Chin J Met Sci Technol, 1987; 3: 289--292 5 周延春,中国科学院金属研究所硕士学位论文,1988 6 Stevens R. J Mater Sci, 1972; 7: 723--726 7 Heuer A H, Fryburg G A, Ogbuji L U, Mitchell TE, Shinozaki S, J Am Ceram Soc, 1978; 61: 406--412