Please wait a minute...
Acta Metall Sin  1991, Vol. 27 Issue (1): 121-125    DOI:
Current Issue | Archive | Adv Search |
OBSERVATION OF TWIN CONFIGURATIONIN β-SiC WHISKERS
ZHOU Yanchun;CHANG Xin;ZHOU Jing;XIA Fei Institute of Metal Research; Academia Sinica; Shenyang
Cite this article: 

ZHOU Yanchun;CHANG Xin;ZHOU Jing;XIA Fei Institute of Metal Research; Academia Sinica; Shenyang. OBSERVATION OF TWIN CONFIGURATIONIN β-SiC WHISKERS. Acta Metall Sin, 1991, 27(1): 121-125.

Download:  PDF(1234KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The twin configuration of β-SiC whiskers prepared by the vapour-liquid-solid process was investigated under TEM. In the whiskets with "bamboo jo-int" morphology, the β-SiC part is jointed with the one-dimensional disorderedpart by the {111}_β twin boundary, microtwins of several atomic layer thick werepresent in β-SiC region. It was noted that the {111}_β twin boundary divides someβ-SiC regions into two parts. The second-order twin joint was also observed at thewhisker tip and the branching position of the bicrystalline whisker. Electron diffra-ction analysis demonstrated that the twin boundary in the bicrystalline whisker isparallel to the matrix {001)_M plane.
Key words:  SiC whisker      twin      bicrystalline whisker     
Received:  18 January 1991     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1991/V27/I1/121

1 Nutt S R. J Am Ceram Soc. 1984; 67: 428--431
2 Nutt S R. J Am Ceram Soc, 1988; 71: 149--156
3 Iwanaga H, Yoshiie T, Katuki H, Egashira M. J Mater Sci Lett, 1986; 5: 946--948
4 Chang Xin, Zhou Yanchun, Xia Fei. Chin J Met Sci Technol, 1987; 3: 289--292
5 周延春,中国科学院金属研究所硕士学位论文,1988
6 Stevens R. J Mater Sci, 1972; 7: 723--726
7 Heuer A H, Fryburg G A, Ogbuji L U, Mitchell TE, Shinozaki S, J Am Ceram Soc, 1978; 61: 406--412
[1] BAI Jiaming, LIU Jiantao, JIA Jian, ZHANG Yiwen. Creep Properties and Solute Atomic Segregation of High-W and High-Ta Type Powder Metallurgy Superalloy[J]. 金属学报, 2023, 59(9): 1230-1242.
[2] ZHAO Peng, XIE Guang, DUAN Huichao, ZHANG Jian, DU Kui. Recrystallization During Thermo-Mechanical Fatigue of Two High-Generation Ni-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1221-1229.
[3] SHAO Xiaohong, PENG Zhenzhen, JIN Qianqian, MA Xiuliang. Unravelling the {101¯2} Twin Intersection Between LPSO Structure/SFs in Magnesium Alloy[J]. 金属学报, 2023, 59(4): 556-566.
[4] ZHANG Zhefeng, LI Keqiang, CAI Tuo, LI Peng, ZHANG Zhenjun, LIU Rui, YANG Jinbo, ZHANG Peng. Effects of Stacking Fault Energy on the Deformation Mechanisms and Mechanical Properties of Face-Centered Cubic Metals[J]. 金属学报, 2023, 59(4): 467-477.
[5] WAN Tao, CHENG Zhao, LU Lei. Effect of Component Proportion on Mechanical Behaviors of Laminated Nanotwinned Cu[J]. 金属学报, 2023, 59(4): 567-576.
[6] GAO Dong, ZHOU Yu, YU Ze, SANG Baoguang. Selection of Twin Variants in Dynamic Plastic Deformation of Pure Ti at Liquid Nitrogen Temperature[J]. 金属学报, 2022, 58(9): 1141-1149.
[7] ZHOU Hongwei, GAO Jianbing, SHEN Jiaming, ZHAO Wei, BAI Fengmei, HE Yizhu. Twin Boundary Evolution Under Low-Cycle Fatigue of C-HRA-5 Austenitic Heat-Resistant Steel at High Temperature[J]. 金属学报, 2022, 58(8): 1013-1023.
[8] GU Ruicheng, ZHANG Jian, ZHANG Mingyang, LIU Yanyan, WANG Shaogang, JIAO Da, LIU Zengqian, ZHANG Zhefeng. Fabrication of Mg-Based Composites Reinforced by SiC Whisker Scaffolds with Three-Dimensional Interpenetrating-Phase Architecture and Their Mechanical Properties[J]. 金属学报, 2022, 58(7): 857-867.
[9] ZHENG Shijian, YAN Zhe, KONG Xiangfei, ZHANG Ruifeng. Interface Modifications on Strength and Plasticity of Nanolayered Metallic Composites[J]. 金属学报, 2022, 58(6): 709-725.
[10] CHEN Yang, MAO Pingli, LIU Zheng, WANG Zhi, CAO Gengsheng. Detwinning Behaviors and Dynamic Mechanical Properties of Precompressed AZ31 Magnesium Alloy Subjected to High Strain Rates Impact[J]. 金属学报, 2022, 58(5): 660-672.
[11] GUO Xiangru, SHEN Junjie. Modelling of the Plastic Behavior of Cu Crystal with Twinning-Induced Softening and Strengthening Effects[J]. 金属学报, 2022, 58(3): 375-384.
[12] LU Lei, ZHAO Huaizhi. Progress in Strengthening and Toughening Mechanisms of Heterogeneous Nanostructured Metals[J]. 金属学报, 2022, 58(11): 1360-1370.
[13] PAN Qingsong, CUI Fang, TAO Nairong, LU Lei. Strain-Controlled Fatigue Behavior of Nanotwin- Strengthened 304 Austenitic Stainless Steel[J]. 金属学报, 2022, 58(1): 45-53.
[14] DING Ning, WANG Yunfeng, LIU Ke, ZHU Xunming, LI Shubo, DU Wenbo. Microstructure, Texture, and Mechanical Properties of Mg-8Gd-1Er-0.5Zr Alloy by Multi-Directional Forging at High Strain Rate[J]. 金属学报, 2021, 57(8): 1000-1008.
[15] DAI Jincai, MIN Xiaohua, ZHOU Kesong, YAO Kai, WANG Weiqiang. Coupling Effect of Pre-Strain Combined with Isothermal Ageing on Mechanical Properties in a Multilayered Ti-10Mo-1Fe/3Fe Alloy[J]. 金属学报, 2021, 57(6): 767-779.
No Suggested Reading articles found!