| INHERITANCE OF PRECIPITATED V_4 C_3 IN MARTENSITIC TRANSFORMATION |
| XIE Changsheng;SUN Peizhen;ZHAO Jiansheng;SUN Desheng Huazhong University of Science and Technology; Wuhan Correspondent:XIE Changsheng; associate professor; Faculty of Metallic Materiats; Huazhong University of Science and Technology |
|
Cite this article:
XIE Changsheng;SUN Peizhen;ZHAO Jiansheng;SUN Desheng Huazhong University of Science and Technology; Wuhan Correspondent:XIE Changsheng; associate professor; Faculty of Metallic Materiats; Huazhong University of Science and Technology. INHERITANCE OF PRECIPITATED V_4 C_3 IN MARTENSITIC TRANSFORMATION. Acta Metall Sin, 1991, 27(5): 14-20.
|
|
|
Abstract The inheritance phenomenon of precipitated V_4C_3 in martensitic transformation has been investigated by means of electron diffraction and matrix analysis. A crystallographic orientation relation among austenite, martensite and V_4C_3 carbide was found to be: (010)_A//(110)_M//(010)_(V_4C_3) [101]_A//[111]_M//[101]_(V_4C_3) The V_4C_3 first precipitated in austenite, and then was inherited to martensite. Although ertain orientation relation was kept between V_4C_3 and martensite, the interfacial structural analysis pointed out that the biphase interfacial energy is higher than that determined by Baker-Nutting relation, thus it is metastable. Because the V_4C_3 precipitated along the crystalline defects in austenite, they could be inherited to martensite.
|
|
Received: 18 May 1991
|
1 谢长生,何向山,崔崑.金属科学与工艺,1987;6(2) :48 2 Tekin E, Kelly P M. J Tron Steel Inst (London), 1965; 203: 715 3 Edington J W. Practical Electron Microscopy in Materials Science, Monograph IV: Typical Electron Microscope Investigations. London: Macmillan, 1976: 107 4 黄孝瑛.透射电子显微学,上海:上海科学技术出版社,1987:258 5 谢长生.华中工学院博士学位论文,1985 6 徐祖耀.金属材料热力学.北京:科学出版社,1981:242 7 Witcomb M J, Dahmer U, Westmacott K H. Acta Metall, 1983; 31: 743 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|