Abstract On the basis of stress-strain analysis under cyclic loading, the mechanism, origin and cyclic number of micro-crack nucleation of duplex structure materials, saying ferrite plus martensite, have been experimentally studied and calculated.Both results are in fair mutual agreement. The morphology, distribution, size and relative quantities of the constitutional phase, especially strengthening phase, as well as the stress-strain distribution and variation in the micro-region are directly influential in the origin of micro-crack in duplex structure materials.
|
|
Received: 18 May 1991
|
1 Wan C M, Chou K C, Jahn M T, Kuo S M. J Mater Sci, 1981; 16: 2521--2527 2 Cai X L, Feng J, Owen W S. Metall Trans, 1985; 16A: 1405--1417 3 汪朝霞,西安交通大学硕士学位论文,1990 4 刘静华,柴东朗.西安交通大学学报,1989;23(Suppl.2) ;112-128$ |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|