| FEATURE OF SERRATED YIELDING IN HIGH STRENGTH Al-Zn-Mg-Cu ALLOY |
| QIAN Kuangwu;LI Xiaoqi;ZHANG Haoguo Fuzhou University |
|
Cite this article:
QIAN Kuangwu;LI Xiaoqi;ZHANG Haoguo Fuzhou University. FEATURE OF SERRATED YIELDING IN HIGH STRENGTH Al-Zn-Mg-Cu ALLOY. Acta Metall Sin, 1991, 27(5): 77-78.
|
|
|
Abstract The temperature dependence of critical strain for serrated yielding was found inhigh strength Al-Zn-Mg-Cu alloy. It divides into two temperature regions. Their temperaturecoefficients of critical strain will be negative and positive respectively.
|
|