Please wait a minute...
Acta Metall Sin  1991, Vol. 27 Issue (5): 73-76    DOI:
Current Issue | Archive | Adv Search |
INTERGRANULAR EMBRITTLEMENT IN PLASMA CARBURIZED LAYER
XIA Lifang;MA Xinxin Harbin Institute of Technology
Cite this article: 

XIA Lifang;MA Xinxin Harbin Institute of Technology. INTERGRANULAR EMBRITTLEMENT IN PLASMA CARBURIZED LAYER. Acta Metall Sin, 1991, 27(5): 73-76.

Download:  PDF(1072KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The principal reason of the intergranular embrittlement in plasma carburized lay-er on 20Cr2Ni4A steel, analyzed by TEM and Auger spectra, was revealed to be due to the segregation of S, P and other impurities along prior austenite grain boundaries. The retained austenite in the layer is unrelated to the intergranular fracture caused in the region. However,the segregation of impurities may be eliminated by reheating and quenching.
Key words:  carburizing      plasma carburizing      embrittlement      impurities segregation     
Received:  18 May 1991     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1991/V27/I5/73

1 Krauss G. Metall Trans, 1978; 9A: 1527
2 Xia Lifang. Lu Yuyan. Advances in Surface Treatment, Vol.Ⅱ. Pergamon Press, 1986: 195
3 Honeycombe R W K著,傅俊岩等译.钢的显微组织和性能.北京:冶金工业出版社,1985:218
[1] WU Xinqiang, RONG Lijian, TAN Jibo, CHEN Shenghu, HU Xiaofeng, ZHANG Yangpeng, ZHANG Ziyu. Research Advance on Liquid Lead-Bismuth Eutectic Corrosion Resistant Si Enhanced Ferritic/Martensitic and Austenitic Stainless Steels[J]. 金属学报, 2023, 59(4): 502-512.
[2] XIAO Na, HUI Weijun, ZHANG Yongjian, ZHAO Xiaoli. Hydrogen Embrittlement Behavior of a Vacuum-Carburized Gear Steel[J]. 金属学报, 2021, 57(8): 977-988.
[3] LAN Liangyun, KONG Xiangwei, QIU Chunlin, DU Linxiu. A Review of Recent Advance on Hydrogen Embrittlement Phenomenon Based on Multiscale Mechanical Experiments[J]. 金属学报, 2021, 57(7): 845-859.
[4] LI Jinxu,WANG Wei,ZHOU Yao,LIU Shenguang,FU Hao,WANG Zheng,KAN Bo. A Review of Research Status of Hydrogen Embrittlement for Automotive Advanced High-Strength Steels[J]. 金属学报, 2020, 56(4): 444-458.
[5] LIU Zhenbao,LIANG Jianxiong,SU Jie,WANG Xiaohui,SUN Yongqing,WANG Changjun,YANG Zhiyong. Research and Application Progress in Ultra-HighStrength Stainless Steel[J]. 金属学报, 2020, 56(4): 549-557.
[6] Futao DONG,Fei XUE,Yaqiang TIAN,Liansheng CHEN,Linxiu DU,Xianghua LIU. Effect of Annealing Temperature on Microstructure, Properties and Hydrogen Embrittlement of TWIP Steel[J]. 金属学报, 2019, 55(6): 792-800.
[7] Xiaoli ZHAO, Yongjian ZHANG, Chengwei SHAO, Weijun HUI, Han DONG. Hydrogen Embrittlement of Intercritically AnnealedCold-Rolled 0.1C-5Mn Steel[J]. 金属学报, 2018, 54(7): 1031-1041.
[8] Tianci ZHANG, Haitao WANG, Zhengcao LI, Henk SCHUT, Zhengming ZHANG, Ming HE, Yuliang SUN. Positron Annihilation Investigation of Embrittlement Behavior in Chinese RPV Steels after Fe-Ion Irradiation[J]. 金属学报, 2018, 54(4): 512-518.
[9] Jun SUN, Suzhi LI, Xiangdong DING, Ju LI. Hydrogenated Vacancy: Basic Properties and Its Influence on Mechanical Behaviors of Metals[J]. 金属学报, 2018, 54(11): 1683-1692.
[10] Xu YANG, Bo LIAO, Jian LIU, Wei YAN, Yiyin SHAN, Furen XIAO, Ke YANG. Embrittlement Phenomenon of China Low Activation Martensitic Steel in Liquid Pb-Bi[J]. 金属学报, 2017, 53(5): 513-523.
[11] Yongqiang WANG,Bin YANG,Na LI,Suhua LIN,Li SUN. EMBRITTLEMENT OF σ PHASE IN STAINLESS STEEL FOR PRIMARY COOLANT PIPES OF NUCLEAR POWER PLANT[J]. 金属学报, 2016, 52(1): 17-24.
[12] Zhifang PENG,Wen REN,Chao YANG,Fangyu CHEN,Hongguo LIU,Fangfang PENG,Qingsong MEI. RELATIONSHIP BETWEEN THE EVOLUTION OF PHASE PARAMETERS OF GRAIN BOUNDARY M23C6 AND EMBRITTLEMENT OF HR3C SUPER-HEATER TUBES IN SERVICE[J]. 金属学报, 2015, 51(11): 1325-1332.
[13] Yongwei SUN,Jizhi CHEN,Jun LIU. STUDY ON HYDROGEN EMBRITTLEMENT SUSCEPTIBILITY OF 1000 MPa GRADE 0Cr16Ni5Mo STEEL[J]. 金属学报, 2015, 51(11): 1315-1324.
[14] PENG Yichao, ZHANG Maicang, DU Chenyang, DONG Jianxin. HIGH TEMPERATURE VACUUM CARBURIZATION BEHAVIORS AND PHASE EVOLUTION MECHANISMS OF Cr35Ni45Nb ALLOY UNDER SERVICE CONDITION[J]. 金属学报, 2015, 51(1): 11-20.
[15] WANG Yanfei, GONG Jianming, RONG Dongsong, GAO Feng. MEASUREMENT AND CALCULATION OF CARBON CONCENTRATION AND DIFFUSION-INDUCED STRESS IN STAINLESS STEEL AFTER LOW TEMPERATURE GAS CARBURIZING[J]. 金属学报, 2014, 50(4): 409-414.
No Suggested Reading articles found!