HIGH RESOLUTION STUDY OF TWINS IN Al_(20)Cu_2Mn_3 PHASE |
LI Chunzhi;WANG Shuncai;JIN Yan Institute of Aeronautical Materials; Beijing; Laboratory of Atomic Imaging of Solids; Institute of Metal Research; Academia Sinaica; Shenyang |
|
Cite this article:
LI Chunzhi;WANG Shuncai;JIN Yan Institute of Aeronautical Materials; Beijing; Laboratory of Atomic Imaging of Solids; Institute of Metal Research; Academia Sinaica; Shenyang. HIGH RESOLUTION STUDY OF TWINS IN Al_(20)Cu_2Mn_3 PHASE. Acta Metall Sin, 1992, 28(1): 1-5.
|
Abstract The dispersoid phase Al_(20)Cu_2Mn_3 in a 2024 Al alloy is commonly composed of twins. An observation of corresponding high resolution image shows that the twin boundary plane is a glide plane other than mirror one. Two neighbouring components of twins are not symmetry of reflection or rotation, but of glide reflection. The "diamond" glide plane is (101) and the glide vector is (1/4)(a--c). Components of twins in the phase take shape of prism with the longitudinal edge being parallel to [010] and side faces being {101} and {100}.
|
Received: 18 January 1992
|
1 Robinson K. Philos Mag, 1952; 43: 775 2 Li Chunzhi, Wang shuncai, Bian Weimin, Yan Minggao. In: Chai Junheng, Yao Junen eds. Proc 3rd Beijing Conf and Exib on Instrum Analysis, Beijing, October 27--30, 1989 Beijing: Ying Wai Printing Co. 1989: A27 3 Li Chunzhi, Wang Shuncai, Jin Yan, Hua Mingjian, Yan Minggao. In: Chen C Q, Starke E A Jr. eds. ALUMINUM ALLOYS' 90, Proc 2nd Int Conf on Aluminum Alloy, Beijing, October 9--13 1990, Beijing: International Academic Publisher, 1990: 504 4 王顺才,李春志,边为民.机械工程学报,1990;26(4) :16 |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|