STRUCTURE AND PROPERTY OF DIRECTIONALLY SOLIDIFIED EUTECTIC Bi/MnBi ALLOY
FU Xuli;LI Jun;WANG Wu;YANG Yongqing;SHU Guangji Southeast University; Nanjing Correspondent lecturer; Department of Materials Science and Engineering; Southeast University; Nanjing 210018
Cite this article:
FU Xuli;LI Jun;WANG Wu;YANG Yongqing;SHU Guangji Southeast University; Nanjing Correspondent lecturer; Department of Materials Science and Engineering; Southeast University; Nanjing 210018. STRUCTURE AND PROPERTY OF DIRECTIONALLY SOLIDIFIED EUTECTIC Bi/MnBi ALLOY. Acta Metall Sin, 1992, 28(6): 85-89.
Abstract Eutectic Bi / MnBi magnetic alloy was prepared by directional solidification.When the growth rate, R>2 cm / h, the MnBi fibre spacing, λ, distributed homogeneously inBi matrix, follows λ~2R=constant. The thermal gradient, G_L, does not influence λ. The mag-netic property, B_r of Bi / MnBi alloy decreases with the increase of R and increases with theincrease of G_L
1 Pirich R G, Metall Trans, 1984; 15A: 2139 2 Savas M A, Smith R W, J Crystal Growth, 1986; 76: 880 3 Notis M R, Shah D M, Young S P, Graham CD, ITEEE Trans Magn, 1979; 3 (2) : 957 4 Chen T. J Appl Phys, 1974; 45: 2358 5 杨永清.东南大学硕士学位论文,1990 6 Kurz W, Fisher D J. Fundamentals of Solidification Trans Tech publications, 1984 7 Flemings M C. Solidification Processing. New York: McGraw-Hill, 1974 8 Toloui B, Hellawell A. Acta Metall, 1976; 24: 565 9 Ravishankar P S, Wilcox W R, Laron D J. Acta Metall, 1980; 28: 1583