Abstract A new model, called A-model, was developed based on the hypothesis of polyhedral grains. The probability functions and the method to calculate 3-dimensional grain size distribution functions using the A-model are given. The theoretical analysis and experimental test have demonstrated that the A-model reduces the systematical error radically and gives much better results.
|
Received: 18 August 1992
|
1 Rhines F N, Craig K R, Rousse D A. Metall Trans, 1976; 7A: 1729-1734 2 Rhines F N, Patterson B R. Metall Trans, 1982; 13A: 985-993 3 Exner H E. Int Metall Rev, 1972; 17: 25-42 4 Wicksell S D. Biometrika, 1925; 17: 84-99 5 Scheil E. Z Anorg Chem, 1931; 201: 259-264 6 Scheil E. Z Metallk, 1935; 27: 199-209 7 Exner H E. Z Metallk, 1966; 57: 755-763 8 Saltykov S A. Stereometric Metallography. 2nd ed., Moscow: Metallurgizdat, 1958 9 Bockstiegel G. Z Metallk, 1966; 57: 647-652 10 DeHoff R T, Liu Guoquan. Metall Trans, 1985; 16A: 2007-2011q |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|