| THERMAL STABILITY OF Ti-24Al-11Nb-3V-1Mo ALLOY |
| ZHANG Bing;WAN Xiaojing;WANG Jianguo;ZHANG Ying Shanghai University of Technology |
|
Cite this article:
ZHANG Bing;WAN Xiaojing;WANG Jianguo;ZHANG Ying Shanghai University of Technology. THERMAL STABILITY OF Ti-24Al-11Nb-3V-1Mo ALLOY. Acta Metall Sin, 1993, 29(10): 23-27.
|
|
|
Abstract The thermal stability of Ti-24Al-11Nb-3V-1Mo alloy was studied after ex-posure at 650--750℃ for different time. The bending strength σ_(bb) and flexibility f decreasedwith increasing exposure temperature and exposure time in air, while only a little change ofσbb and f was noticed when samples exposed under vacuum in the same condition. This is dueto the formation of a brittle oxygen-enriched layer adjacent to the surface of material, inaddtion to the formation of TiO_2 on the surface after exposure in air. Thermal exposure of al-loy results in the change of microstructure, i.e., forming the "O" phase, which is not the ma-jor factor causing the degradation of mechnical properties.
|
|
Received: 18 October 1993
|
1 万晓景.钛科学与工程,第六届全国钛及钛合金学术交流会文集,原子能出版社,1987;V2:3 2 金属研究所,抚顺钢厂.金属学报,1976;12:172 3 Rowe R G. In: Wang S H, Liu C T, Pope P O, Stiegler J U eds. High Temperature Aluminide and Intermetallics, The Minerals and Materials Society, 1990 4 Kim Y W, Proes F H. In: Wang S H, Liu C T, Pope D P, Stiegler J O eds.,High Temperature Aluminide and Intermetallics, The Minerals and Materials Society, 1990 5 Wang Bin, Jia tiancong, Zou Dunxu, Ma Huiping, Zhong Zengyon. Mater Sci Eng, 1992; A153:422 6 葛志明.钛的二元相图,北京:国防工业出版社,1977 7 Angela Szaruga. Scr Met Mater, 1992; 26: 787 8 Rahmel A, Specer P J. Oxid Met, 1991; 35: 53 9 Luthra K L. Oxid Mat, 1991; 36: 475 10 万晓景,曹名洲,辛公春.金属学报,1979;15:563 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|