EXTENSION OF SOLID SOLUBILITY INDUCED BY MECHANICAL ALLOYING IN Fe-Cu SYSTEM
HUANG Jianyu;WU Yukun;HU Kuiyi;MENG Xiangmin Laboratory of Atomic Imaging of Solids and Laboratory of Rapidly Solidified Non-Equilibrium Alloys; Institute of Metal Research; Academia Sinica; Shenyang
Cite this article: 

HUANG Jianyu;WU Yukun;HU Kuiyi;MENG Xiangmin Laboratory of Atomic Imaging of Solids and Laboratory of Rapidly Solidified Non-Equilibrium Alloys; Institute of Metal Research; Academia Sinica; Shenyang. EXTENSION OF SOLID SOLUBILITY INDUCED BY MECHANICAL ALLOYING IN Fe-Cu SYSTEM. Acta Metall Sin, 1993, 29(2): 60-63.

Download:  PDF(732KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  At room temperature Fe and Cu form almost no solid solution in equilibriumphase diagram but X-ray diffraction and DTA show that the metastableFe_(1-x)Cu_x supersaturated solid solution can be obtained after 5 h of ball-milling of the mixedFe and Cu powders. The bcc phase is extended over the region with x≤0.10, while the fccphase with x≥0.30. For 0.10
Key words:  Fe-Cu system      mechanical alloying      supersaturated solid solution      martensite transformation     
Received:  18 February 1993     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1993/V29/I2/60

1 Klement W Jr. Trans AIME, 1965; 233: 1180
2 Sumiyama K, Yoshitake T, Nakamura Y. J Phys Soc Jpn, 1984; 53: 3160
3 杨元政,马学鸣,董远达.金属学报,1992;28:A399
4 Gaffet E, Louison C, Harmelin M, Faudot F. Mater Sci Eng, 1991: A134: 1380
5 Sumiyama K, Takemura K, Kataoka N, Nakamura Y. Jpn J Appl Phys, 1989; 28: 361
6 Easterling K E, Miekk-Oja H M. Acta Metall, 1967; 15: 1133
[1] WANG Shihong,LI Jian,GE Xin,CHAI Feng,LUO Xiaobing,YANG Caifu,SU Hang. Microstructural Evolution and Work Hardening Behavior of Fe-19Mn Alloy Containing Duplex Austenite and ε-Martensite[J]. 金属学报, 2020, 56(3): 311-320.
[2] Jintao SHI,Longgang HOU,Jinrong ZUO,Lin LU,Hua CUI,Jishan ZHANG. QUANTITATIVE ANALYSIS OF THE MARTENSITE TRANSFORMATION AND MICROSTRUCTURE CHARACTERIZATION DURING CRYOGENIC ROLLING OF A 304 AUSTENITIC STAINLESS STEEL[J]. 金属学报, 2016, 52(8): 945-955.
[3] Min ZHU, Zhongchen LU, Renzong HU, Liuzhang OUYANG. DIELECTRIC BARRIER DISCHARGE PLASMA ASSISTED BALL MILLING TECHNOLOGY AND ITS APPLICATIONS IN MATERIALS FABRICATION[J]. 金属学报, 2016, 52(10): 1239-1248.
[4] Cunyu WANG,Ying CHANG,Jie YANG,Kunmin ZHAO,Han DONG. THE COMBINED EFFECT OF HOT DEFORMATION PLUS QUENCHING AND PARTITIONING TREATMENT ON MARTENSITE TRANSFORMATION OF LOW CARBON ALLOYED STEEL[J]. 金属学报, 2015, 51(8): 913-919.
[5] HU Na, XUE Lihong, GU Jian, LI Heping, YAN Youwei. OPTIMIZATION OF GRADING ON MICROSTRUCTURE AND MECHANICAL PROPERTIES OF Al13Fe4/Al COM- POSITES IN SITU SYNTHESIZED BY MECHANICAL ALLOYING AND SPARK PLASMA SINTERING[J]. 金属学报, 2015, 51(2): 216-222.
[6] SHANG Hailong, LIU Wenqing, DONG Yujun, ZHANG Anming, MA Bingyang, LI Geyang. 3D ATOM PROBE CHARACTERIZATION OF MICRO-STRUCTURE OF TiBx/Al SUPERSATURATED SOLID SOLUTE COMPOSITE FILMS[J]. 金属学报, 2014, 50(4): 395-399.
[7] GU Jian, GU Sasa, XUE Lihong, WU Shusen, YAN Youwei. MICROSTRUCTURE EVOLUTION OF Al-Fe ALLOYS PREPARED BY MECHANICAL ALLOYING AND SPARK PLASMA SINTERING[J]. 金属学报, 2013, 29(4): 435-442.
[8] SHANG Hailong,SHEN Jie,YANG Duo,SUN Shiyang,LI Geyang. MICROSTRUCTURE AND MECHANICAL PROPERTIES OF Ti, C SOLID SOLUTION SUPERSATURATED Al-BASED COMPOSITE FILMS[J]. 金属学报, 2013, 49(3): 320-324.
[9] WANG Man, ZHOU Zhangjian, YAN Zhigang, YU Pengfei, SUN Hongying. TEM CHARACTERIZATION OF DISPERSOIDS AND MICROSTRUCTURE OF ODS-316 AUSTENITIC STEEL[J]. 金属学报, 2013, 49(2): 153-158.
[10] WEI Zhaozhao, MA Xiao, ZHANG Xinping. STUDY ON THE DISLOCATION STRUCTURE OF INTERPHASE INTERFACE AND MARTENSITE TRANSFORMATION CRYSTALLOGRAPHY IN Ni2 MnGa ALLOY[J]. 金属学报, 2013, 49(2): 187-198.
[11] LU Zheng, LU Chenyang, ZHANG Shouhui, XIE Rui, Liu Chunming. PREPARATION AND CHARACTERIZATION OF NANO-STRUCTURED 14Cr-ODS FERRITIC STEEL[J]. 金属学报, 2012, 48(6): 649-653.
[12] XU Mingzhou WANG Jianjun LIU Chunming. LOW TEMPERATURE DEFORMATION BEHAVIOR OF HIGH–NITROGEN NICKEL–FREE AUSTENITIC STAINLESS STEELS[J]. 金属学报, 2011, 47(10): 1335-1341.
[13] CHENG Xiaojuan WANG Hong KANG Guozheng DONG Yawei LIU Yujie. STUDY ON STRAIN--INDUCED MARTENSITE TRANSFORMATION OF 304 STAINLESS STEEL DURING RATCHETING DEFORMATION[J]. 金属学报, 2009, 45(7): 830-834.
[14] ZHANG Zhanling LIU Yongning YU Guang ZHU Jiewu HE Tao. MORPHOLOGY AND SUBSTRUCTURE OF JUJUBE--STONE--LIKE MARTENSITE IN ULTRAHIGH CARBON STEEL[J]. 金属学报, 2009, 45(3): 280-284.
[15] LIU Wei LI Zhibin WANG Xiang ZOU Hua WANG Lixin. EFFECT OF STRAIN RATE ON STRAIN INDUCED α'--MARTENSITE TRANSFORMATION AND MECHANICAL RESPONSE OF AUSTENITIC STAINLESS STEELS[J]. 金属学报, 2009, 45(3): 285-291.
No Suggested Reading articles found!