| EFFECT OF Y ON PRECIPITATION AND MECHANICAL PROPERTIES OF Al-Li ALLOY |
| GUI Quanhong;JIANG Xiaojun;MA Luming;LIANG Guojun;XING Zhongshu;LI Yiyi Institute of Metal Research; Academia Sinica; Shenyang research assistant Institute of Metal Research ■demia ■ Shenyang 110015 |
|
Cite this article:
GUI Quanhong;JIANG Xiaojun;MA Luming;LIANG Guojun;XING Zhongshu;LI Yiyi Institute of Metal Research; Academia Sinica; Shenyang research assistant Institute of Metal Research ■demia ■ Shenyang 110015. EFFECT OF Y ON PRECIPITATION AND MECHANICAL PROPERTIES OF Al-Li ALLOY. Acta Metall Sin, 1993, 29(4): 19-24.
|
|
|
Abstract Effect of Y, containing 0.1 or 0.5 wt-%, on precipitation and tensile proper-ties of Al-Li-Cu-Mg-Zr alloy has been studied. An addition of Y may refine the grain size,promote the β′-phase precipitation, improve S′-phase distribution, and restrain the growthof δ′-phase. Tensile tests at room temperature indicate that 0.1 wt-% Y addition may in-crease the ductility but no more strength. However, 0.5 wt-%Y contained alloy exhibits high-er strength without reducing ductility.
|
|
Received: 18 April 1993
|
1 崔建忠,胡骏,马龙翔.材料科学进展,1991;5:147 2 陈铮,李明利,何明.金属学报,1991;27:A153 3 Mahalingan K, Mahauev V, Lindle G L, Sanders T H Jr. Scr Metall Mater. 1991; 25: 2181 4 Zhang Y, Zhao H, Gao G, Chen J, Yao D, Hu Z. In: Sanders T H Jr,. Starke E A Jr. eds, Aluminum-Lithium Alloys, Proc 5th Int Aluminum-Lithium Conf, Williamsburg Virginia, March 27--31, 1989, Brimingham: Materials and Component Engineeting, 1989: 539 5 萨维茨基EM著,白忠德译.稀土金属合金.北京:国防科学出版社,1975 6 Srivasan T S, Place A T. J Mater Sci, 1989; 24: 1546 |