Please wait a minute...
Acta Metall Sin  1994, Vol. 30 Issue (1): 44-48    DOI:
Current Issue | Archive | Adv Search |
HIGH TEMPERATURE OXIDATION BEHAVIOR OF DS Ni_3Al-Mo BASE ALLOY
YE Changjiang;LI Tiefan;SHEN.Jianian;MAO Xiaoyu;(Corrosion Science Lab.;Institute of Corrosion and Protection of Metals; Chinese Academy of Sciences;Shenyang 110015)(Manuscript received 23 August; 1993;in revised form 26 October;1993)
Cite this article: 

YE Changjiang;LI Tiefan;SHEN.Jianian;MAO Xiaoyu;(Corrosion Science Lab.;Institute of Corrosion and Protection of Metals; Chinese Academy of Sciences;Shenyang 110015)(Manuscript received 23 August; 1993;in revised form 26 October;1993). HIGH TEMPERATURE OXIDATION BEHAVIOR OF DS Ni_3Al-Mo BASE ALLOY. Acta Metall Sin, 1994, 30(1): 44-48.

Download:  PDF(357KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A study of oxidation kinetics of DS Ni3Al-Mo base alloy(IC-6) have been carried out in thermobalance at 1273 and 1373 K in air for 300 h.The structure and composition of the oxide were examined by EPMA and XPD analyses.The oxide oxidation of IC-6 alloy can be described as a system in which both oxygen inward diffusion of oxidation of IC-6alloy:is in good agreement with experimental data.The volatilization rate constant of MoO3 was calculated qualitatively,as Ks=3.27×10-4mg/cm2·s at 1273 and 1373K respectively.Correspondent:YE Changjiang,(Institute of Corrosion and Protection of Metals,Chinese Academy of Sciences,Shenyang 110015)
Key words:  DS Ni_3Al-Mo alloy      high temperature oxidation      parabolic rate constant      volatilization rate coustant     
Received:  18 January 1994     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1994/V30/I1/44

1韩雅芳,李孙华.金属间化合物,北京:机械工业出版社,1992:702TanignchiS,ShibataT,TsuruokaH,OxidMet,1986;26:13孙超,郭建亭,李辉,管恒荣.中国腐蚀与防护学报,1990;10:1714KubaschewskiO,HopkinsBE,OxidationofMetalsandAlloys,London,1962:2455KuenzlyJD,DouglassDL,OxldMet,1974;8:1396BrennerSS,J.ElectrochemSoc,1955;102:77T著,马志春译,耐热扩散涂层,北京:国防工业出版社,1988:2638SimnadM,SplinersA,JMetals,1955;7:10119TedmonCS,JElectrochemSoc.1966;113:766
[1] XU Wenguo, HAO Wenjiang, LI Yingju, ZHAO Qingbin, LU Bingyu, GUO Heyi, LIU Tianyu, FENG Xiaohui, YANG Yuansheng. Effects of Trace Aluminum and Titanium on High Temper-ature Oxidation Behavior of Inconel 690 Alloy[J]. 金属学报, 2023, 59(12): 1547-1558.
[2] XIE Leipeng, SUN Wenyao, CHEN Minghui, WANG Jinlong, WANG Fuhui. Effects of Processing on Microstructures and Properties of FGH4097 Superalloy[J]. 金属学报, 2022, 58(8): 992-1002.
[3] YANG Liang, LV Haotian, WAN Chunlei, GONG Qianming, CHEN Hao, ZHANG Chi, YANG Zhigang. Review: Mechanism of Reactive Element Effect—Oxide Pegging[J]. 金属学报, 2021, 57(2): 182-190.
[4] Mingyu ZHAO,Huijuan ZHEN,Zhihong DONG,Xiuying YANG,Xiao PENG. Preparation and Performance of a Novel Wear-Resistant and High Temperature Oxidation-Resistant NiCrAlSiC Composite Coating[J]. 金属学报, 2019, 55(7): 902-910.
[5] GAO Bo, WANG Lei, SONG Xiu, LIU Yang, YANG Shuyu, CHIBA Akihiko. Effect of Pre-Oxidation on High Temperature Oxidation and Corrosion Behavior of Co-Al-W-Based Superalloy[J]. 金属学报, 2019, 55(10): 1273-1281.
[6] Yin BAI, Zhengdong LIU, Jianxin XIE, Hansheng BAO, Zhengzong CHEN. Effect of Pre-Oxidation Treatment on the Behavior of High Temperature Oxidation in Steam of G115 Steel[J]. 金属学报, 2018, 54(6): 895-904.
[7] Yuxiang ZENG,Xiping GUO,Yanqiang QIAO,Zhongyi NIE. EFFECT OF Zr ADDITION ON MICROSTRUCTURE AND OXIDATION RESISTANCE OF Nb-Ti-Si BASE ULTRAHIGH-TEMPERATURE ALLOYS[J]. 金属学报, 2015, 51(9): 1049-1058.
[8] Haigen ZHAO,Shusuo LI,Yanling PEI,Shengkai GONG,Huibin XU. MICROSTRUCTURE AND MECHANICAL PROPERTIES OF Ni3Al-BASED SINGLE CRYSTSAL ALLOY IC21[J]. 金属学报, 2015, 51(10): 1279-1287.
[9] ZHOU Xiaowei SHEN Yifu GU Dongdong. MICROSTRUCTURE AND HIGH TEMPERATURE OXIDATION RESISTANCE OF NANOCRYSTALLINE Ni–CeO2 COMPOSITE COATINGS DEPOSITED BY DOUBLE–PULSED ELECTRO DEPOSITION[J]. 金属学报, 2012, 48(8): 957-964.
[10] YU Daqian, LU Xuyang, MA Jun, JIANG Sumeng, LIU Shanchuan, GONG Jun, SUN Chao. STUDY OF OXIDATION BEHAVIOR OF THE GRADIENT NiCrAlY COATING AT 1000 AND 1100 ℃[J]. 金属学报, 2012, 48(6): 759-768.
[11] SONG Peng LU Jiansheng ZHANG Defeng LU Jianguo LI Dejiang. EFFECT OF La AND Hf DOPANT ON THE HIGH TEMPERATURE OXIDATION OF CoNiCrAl ALLOYS[J]. 金属学报, 2011, 47(6): 655-662.
[12] PENG Xin JIANG Sumeng DUAN Xuhai GONG Jun SUN Chao. HIGH TEMPERATURE OXIDATION BEHAVIOR OF A (MCrAlY+AlSiY) COMPOSITE COATING[J]. 金属学报, 2009, 45(3): 378-384.
[13] Xinqing Zhao. THE EFFECT OF Nb ON THE OXIDATION BEHAVIOR OF TiNiAl ALLOYS[J]. 金属学报, 2006, 42(8): 820-826 .
[14] ZHANG Xuejun; WU Weitao; NIU Yan. Effect Of Silver Addition On Surface Morphology Of Al2O3 Scales During Oxidation Of β-NiAl[J]. 金属学报, 2005, 41(4): 369-374 .
[15] GUO Minghu; WANG Qimin; KE Peiling; CUI Yuyou; GONG Jun; SUN Chao; WEN Lishi. Effect of Ni-Al coating on high temperature oxidation behaviors of Ti-22Al-26Nb alloy[J]. 金属学报, 2005, 41(3): 312-316 .
No Suggested Reading articles found!