Please wait a minute...
Acta Metall Sin  1994, Vol. 30 Issue (12): 531-539    DOI:
Current Issue | Archive | Adv Search |
MICROSTRUCTURE AND PROPERTIES OF Au-Cu ALLOYS
XIE Youqing;ZHANG Hiaodong(Central South University of Technology; Changsha)
Cite this article: 

XIE Youqing;ZHANG Hiaodong(Central South University of Technology; Changsha). MICROSTRUCTURE AND PROPERTIES OF Au-Cu ALLOYS. Acta Metall Sin, 1994, 30(12): 531-539.

Download:  PDF(575KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  According to characteristic crystal theory of alloy phases established on the statistic thermodynamics and electronic theory of metals,a systematic analysis has been conducted on the Au-Cu system. The interaction equations of characteristic properties (energy and volume),electronic structures and their changing characters of characteristic atoms in the Au-Cu alloys have been determined. The theoretical values of heat of formation, mixing Gibbs free energy and lattice constant as a function of concentration are in good agreement with the experimental values.XIE Youqing, professor, Department of Materials Science and Engineering, Central South University of Technology, Changsha 410083
Key words:  Au-Cu alloy      electronic structure      atomic configuration      heat of formation      lattice constant     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1994/V30/I12/531

1HildebrandJH,ScottRL.TheSolubilityofNonelectrolytes.3rded,NewYork:VanNostrandReinhold,19502GuggenheimEA.Mixtures.Oxford:OxfordUniversityPress,19523LupisCHP,ElliottJF.ActaMetall,1967;15:2654谢佑卿.中国科学,A辑,1992;(8):8805谢佑卿,马柳莺,张晓东.科学通报,1992;16:15296谢佑卿,张晓东,赵礼颖,马秀林.中国科学,A辑,1993,(5):5457谢佑卿,张晓东,赵礼颖.中南矿冶学院学报(外文版),1992,4:4188谢佑卿,张晓东,马秀林,赵礼颖.中国有色金属学报,1992,2:519XieYQ.ActaMetallMater,1994(待发表)10谢佑卿,吕满珊,张晓东,赵礼颖.中国科学,A辑,1993;(8):875.11谢佑卿.中南矿冶学院学报.1993;(3):33212谢佑卿,马柳莺,张晓东,邹平,赵礼颖.中国科学,A辑,1993;(9):99913PearsonWB.HandbookofLatticeSpacingsandStructureofMetalsandAlloys,London:Pergamon.1958;41114GrayDE.AmericanInstituteofPhysicsHandbook.3rded,NewYork:McGraw-HillBookCompanyInc,1972,4:11915HultgrenR,DesaiPD,HawkinsDT,GleiserM,KellyeyKK.SelectedValuesofThermodynamicPropertiesofMetalsandAlloys,NewYork:Wiley,1963:45416谢佑卿,马柳莺.中南矿冶学院学报,1985;(1):117CahnRW.PhysicalMetallugy.Amsterdam:North-HollandPublishngCompany,1970:65
[1] HUANGFU Hao, WANG Zilong, LIU Yongli, MENG Fanshun, SONG Jiupeng, QI Yang. A First Principles Investigation of W1 - x Ir x Alloys: Structural, Electronic, Mechanical, and Thermal Properties[J]. 金属学报, 2022, 58(2): 231-240.
[2] WANG Shuo, WANG Junsheng. Structural Evolution and Stability of the δ′/θ′/δ′ Composite Precipitate in Al-Li Alloys: A First-Principles Study[J]. 金属学报, 2022, 58(10): 1325-1333.
[3] Liqun CHEN, Zhengchen QIU, Tao YU. Effect of Ru on the Electronic Structure of the [100](010) Edge Dislocation in NiAl[J]. 金属学报, 2019, 55(2): 223-228.
[4] MAO Pingli, YU Bo, LIU Zheng, WANG Feng, JU Yang. FIRST-PRINCIPLES CALCULATION OF ELECTRONIC STRUCTURE AND ELASTIC PROPERTY OF AB2 TYPE INTERMETALLICS IN Mg-Zn-Ca ALLOY[J]. 金属学报, 2013, 49(10): 1227-1233.
[5] WANG Youdao WU Erdong WANG Sucheng LI Wuhui. X-RAY DIFFRACTION ANALYSIS ON THE THICKNESS EFFECT OF γ/γ' LATTICE MISMATCHE IN NICKEL BASE SINGLE CRYSTAL SUPERALLOY DD10[J]. 金属学报, 2011, 47(11): 1418-1425.
[6] ZHOU Dianwu LIU Jinshui XU Shaohua PENG Ping. FIRST–PRINCIPLE CALCULATIONS OF STRUCTURAL STABILITIES AND ELASTIC PROPERTIES OF Al2Sr AND Mg2Sr PHASES[J]. 金属学报, 2011, 47(10): 1315-1320.
[7] ZHOU Dianwu XU Shaohua ZHANG Fuquan PENG Ping LIU Jinshui. FIRST-PRINCIPLES CALCULATIONS OF STRUCTURAL STABILITIES AND ELASTIC PROPERTIES OF AB2 TYPE INTERMETALLICS IN ZA62 MAGNESIUM ALLOY[J]. 金属学报, 2010, 46(1): 97-103.
[8] ZHANG Guoying ZHANG Hui FANG Geliang YANG Lina. ELECTRONIC STRUCTURE OF DIFFERENT REGIONS AND ANALYSIS OF STRESS CORROSION MECHANISM OF Al--Zn--Mg--Cu ALLOYS[J]. 金属学报, 2009, 45(6): 687-691.
[9] Dong Xing-Long; Jun-Peng Lei. Prediction of the primary intermetallic compound formed in Fe(Ni)-Sn nanoparticles system[J]. 金属学报, 2008, 44(8): 922-926 .
[10] LIANG Chu; XU Lingyan; YAO Chunxian; LAN Zhiqiang; LI Guangxu; GUO Jin. First-Principles Investigation on Effect of Co On Hydrogen Storage Properties of ZrMn2 Alloy[J]. 金属学报, 2008, 44(3): 351-356 .
[11] Liu Guili. The study on Ti alloys stress corrosion mechanicby recursion method[J]. 金属学报, 2007, 43(3): 249-253 .
[12] TAO Huijin; XIE Youqing; PENG Hongjian; YU Fangxin; LIU Ruifeng; LI Xiaobo. Temperature Dependence of tom States and Physical Properties of fcc-, metastable hcp- and bcc- Cu[J]. 金属学报, 2006, 42(6): 565-571 .
[13] JIAN Xiaoling. Investigations of Electronic Structures and Bond Characteristics of ZrMn2 Alloy and Its Hydride by First Principle[J]. 金属学报, 2006, 42(2): 123-128 .
[14] ZHANG Xiaozhong; ZHANG Lina; MA Yue; QI Junjie; YUAN Jun. Electronic Structure Characterization of Bonding of Grain Boundaries and Fracture Mode of Steels[J]. 金属学报, 2005, 41(6): 617-621 .
[15] DONG Jianmin; LI Hua; ZHANG Changwen; PAN Fengchun; WANG Yongjuan; ZHEN Peng. Electronic structure and magnetism of clusters Nin(n=2-6)[J]. 金属学报, 2005, 41(3): 242-244 .
No Suggested Reading articles found!