MICRODYNAMICAL MECHANISM OF DYNAMIC SOLIDIFICATION OF ALLOYS
JIAO Yuning;LIU Qingmin;YANG Yuansheng; HU Zhuangqi (Institute of Metal Research;Chinese Academy of Sciences;Shenyang)
Cite this article: 

JIAO Yuning;LIU Qingmin;YANG Yuansheng; HU Zhuangqi (Institute of Metal Research;Chinese Academy of Sciences;Shenyang). MICRODYNAMICAL MECHANISM OF DYNAMIC SOLIDIFICATION OF ALLOYS. Acta Metall Sin, 1994, 30(12): 540-544.

Download:  PDF(336KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  On the basis of the model of atomic cluster jump theory,a microdynamical model of crystal growth rate was developed under condition of the dynamic solidification.The classical continuous growth model seems to be only one of the special case.Theoretical analysis showed that the crystal growth rate is dependent on not only the nature of metal but also the supercooling,△T, and external force, F. Certain solidification behaviours of columnar crystals and columnar dendrites under fluid flow condition are explained by using of the model.JIAO Yuning, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110015
Key words:  dynamic solidification      microdynamics      continuous growth model     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1994/V30/I12/540

1FlemingsMC,AdamsCM,HuckeEE,TaylorHF.TransAFS,1956;54:6362焦育宁等.材料工程,1993;7:143刘山等.金属科学与工艺,1992,11(2):754MurakamiK,AiharaH,OkamotoT.ActaMetall,1984;32:9335何国等.93'全国相变学术会论文集,北京,1993:3486李庆春编.铸件形成理论.北京:机械工业出版社,19817胡汉起.金属凝固.北京:冶金工业出版社,19858王家忻,黄积荣,林建生.金属的凝固及其控制.北京:机械工业出版社,1977
No related articles found!
No Suggested Reading articles found!