| MICROSTRUCTURE AND PROPERTIES OF Au-Cu ALLOYS |
| XIE Youqing;ZHANG Hiaodong(Central South University of Technology; Changsha) |
|
Cite this article:
XIE Youqing;ZHANG Hiaodong(Central South University of Technology; Changsha). MICROSTRUCTURE AND PROPERTIES OF Au-Cu ALLOYS. Acta Metall Sin, 1994, 30(12): 531-539.
|
|
|
Abstract According to characteristic crystal theory of alloy phases established on the statistic thermodynamics and electronic theory of metals,a systematic analysis has been conducted on the Au-Cu system. The interaction equations of characteristic properties (energy and volume),electronic structures and their changing characters of characteristic atoms in the Au-Cu alloys have been determined. The theoretical values of heat of formation, mixing Gibbs free energy and lattice constant as a function of concentration are in good agreement with the experimental values.XIE Youqing, professor, Department of Materials Science and Engineering, Central South University of Technology, Changsha 410083
|
|
|
| 1HildebrandJH,ScottRL.TheSolubilityofNonelectrolytes.3rded,NewYork:VanNostrandReinhold,19502GuggenheimEA.Mixtures.Oxford:OxfordUniversityPress,19523LupisCHP,ElliottJF.ActaMetall,1967;15:2654谢佑卿.中国科学,A辑,1992;(8):8805谢佑卿,马柳莺,张晓东.科学通报,1992;16:15296谢佑卿,张晓东,赵礼颖,马秀林.中国科学,A辑,1993,(5):5457谢佑卿,张晓东,赵礼颖.中南矿冶学院学报(外文版),1992,4:4188谢佑卿,张晓东,马秀林,赵礼颖.中国有色金属学报,1992,2:519XieYQ.ActaMetallMater,1994(待发表)10谢佑卿,吕满珊,张晓东,赵礼颖.中国科学,A辑,1993;(8):875.11谢佑卿.中南矿冶学院学报.1993;(3):33212谢佑卿,马柳莺,张晓东,邹平,赵礼颖.中国科学,A辑,1993;(9):99913PearsonWB.HandbookofLatticeSpacingsandStructureofMetalsandAlloys,London:Pergamon.1958;41114GrayDE.AmericanInstituteofPhysicsHandbook.3rded,NewYork:McGraw-HillBookCompanyInc,1972,4:11915HultgrenR,DesaiPD,HawkinsDT,GleiserM,KellyeyKK.SelectedValuesofThermodynamicPropertiesofMetalsandAlloys,NewYork:Wiley,1963:45416谢佑卿,马柳莺.中南矿冶学院学报,1985;(1):117CahnRW.PhysicalMetallugy.Amsterdam:North-HollandPublishngCompany,1970:65 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|