Please wait a minute...
Acta Metall Sin  1994, Vol. 30 Issue (19): 314-317    DOI:
Current Issue | Archive | Adv Search |
PREPARATION OF IN-SITU TiC REINFORCED Al COMPOSITE BY CONTACT-REACTION
WANG Zidong;ZENGSongyan;LI Qingchun(Harbin Institute of Technology)Li Chunyu;WANG Shuncai;LIU Baicao(Beijing institute of Aeronautical Materials; Laboratory of Atomic Imaging of Solids; Insititute of Metal Research; Chinese Academy of Sciences; Shenyang)
Cite this article: 

WANG Zidong;ZENGSongyan;LI Qingchun(Harbin Institute of Technology)Li Chunyu;WANG Shuncai;LIU Baicao(Beijing institute of Aeronautical Materials; Laboratory of Atomic Imaging of Solids; Insititute of Metal Research; Chinese Academy of Sciences; Shenyang). PREPARATION OF IN-SITU TiC REINFORCED Al COMPOSITE BY CONTACT-REACTION. Acta Metall Sin, 1994, 30(19): 314-317.

Download:  PDF(269KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The TiC reinforced Al composite was prepared by in-situ contact-reaction.The TiC particles are sized down to nm, and free from lattice defect practically. No interaction between TiC and α-Al interfaces was found. The composite, thus, has a superior properties as comparison with that of pure Al.
Key words:  composite      in-situ reaction      Al     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1994/V30/I19/314

1BrupbacherJM,ChristodoulouL,NagleDC.USPat,4710348,19872WestwoodARC.MetallTrans.1988;19A:7493VyletalGM,VanAkenDC,AllisonJE.ScrMetallMater,1991;25:24054WestwoodARC.MetallTrans,1988;19B:1555马宗义,毕敬,吕毓雄,申红伟,高荫轩.金属学报,1992;28:B4196KuruvillaAK,PrasadKS,BhanuprasadVV,MahajanYR.ScrMetallMater,1990;24:8737王自东,李春玉,李庆春,张录山,于桂复.中国专利,申请号:93104814.1,1993
[1] ZHANG Leilei, CHEN Jingyang, TANG Xin, XIAO Chengbo, ZHANG Mingjun, YANG Qing. Evolution of Microstructures and Mechanical Properties of K439B Superalloy During Long-Term Aging at 800oC[J]. 金属学报, 2023, 59(9): 1253-1264.
[2] LU Nannan, GUO Yimo, YANG Shulin, LIANG Jingjing, ZHOU Yizhou, SUN Xiaofeng, LI Jinguo. Formation Mechanisms of Hot Cracks in Laser Additive Repairing Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1243-1252.
[3] FENG Qiang, LU Song, LI Wendao, ZHANG Xiaorui, LI Longfei, ZOU Min, ZHUANG Xiaoli. Recent Progress in Alloy Design and Creep Mechanism of γ'-Strengthened Co-Based Superalloys[J]. 金属学报, 2023, 59(9): 1125-1143.
[4] JIANG He, NAI Qiliang, XU Chao, ZHAO Xiao, YAO Zhihao, DONG Jianxin. Sensitive Temperature and Reason of Rapid Fatigue Crack Propagation in Nickel-Based Superalloy[J]. 金属学报, 2023, 59(9): 1190-1200.
[5] GONG Shengkai, LIU Yuan, GENG Lilun, RU Yi, ZHAO Wenyue, PEI Yanling, LI Shusuo. Advances in the Regulation and Interfacial Behavior of Coatings/Superalloys[J]. 金属学报, 2023, 59(9): 1097-1108.
[6] DU Jinhui, BI Zhongnan, QU Jinglong. Recent Development of Triple Melt GH4169 Alloy[J]. 金属学报, 2023, 59(9): 1159-1172.
[7] LI Jiarong, DONG Jianmin, HAN Mei, LIU Shizhong. Effects of Sand Blasting on Surface Integrity and High Cycle Fatigue Properties of DD6 Single Crystal Superalloy[J]. 金属学报, 2023, 59(9): 1201-1208.
[8] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
[9] MA Dexin, ZHAO Yunxing, XU Weitai, WANG Fu. Effect of Gravity on Directionally Solidified Structure of Superalloys[J]. 金属学报, 2023, 59(9): 1279-1290.
[10] CHEN Jia, GUO Min, YANG Min, LIU Lin, ZHANG Jun. Effects of W Concentration on Creep Microstructure and Property of Novel Co-Based Superalloys[J]. 金属学报, 2023, 59(9): 1209-1220.
[11] BI Zhongnan, QIN Hailong, LIU Pei, SHI Songyi, XIE Jinli, ZHANG Ji. Research Progress Regarding Quantitative Characterization and Control Technology of Residual Stress in Superalloy Forgings[J]. 金属学报, 2023, 59(9): 1144-1158.
[12] ZHENG Liang, ZHANG Qiang, LI Zhou, ZHANG Guoqing. Effects of Oxygen Increasing/Decreasing Processes on Surface Characteristics of Superalloy Powders and Properties of Their Bulk Alloy Counterparts: Powders Storage and Degassing[J]. 金属学报, 2023, 59(9): 1265-1278.
[13] ZHAO Peng, XIE Guang, DUAN Huichao, ZHANG Jian, DU Kui. Recrystallization During Thermo-Mechanical Fatigue of Two High-Generation Ni-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1221-1229.
[14] BAI Jiaming, LIU Jiantao, JIA Jian, ZHANG Yiwen. Creep Properties and Solute Atomic Segregation of High-W and High-Ta Type Powder Metallurgy Superalloy[J]. 金属学报, 2023, 59(9): 1230-1242.
[15] ZHANG Jian, WANG Li, XIE Guang, WANG Dong, SHEN Jian, LU Yuzhang, HUANG Yaqi, LI Yawei. Recent Progress in Research and Development of Nickel-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1109-1124.
No Suggested Reading articles found!