A YIELD MODEL OF POLYCRYSTALLINE METAL BASED ON NONLINEAR IRREVERSIBLE MULTIPLICATION PROCESS
HE Zongyan; HUANG Kezhi( Tsinghua University; Beijing 100084)
Cite this article: 

HE Zongyan; HUANG Kezhi( Tsinghua University; Beijing 100084). A YIELD MODEL OF POLYCRYSTALLINE METAL BASED ON NONLINEAR IRREVERSIBLE MULTIPLICATION PROCESS. Acta Metall Sin, 1995, 31(3): 97-104.

Download:  PDF(449KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  On the assumption that plastically deformed grains multiply irreversibly during tensile deformation, a yield model of polycrystalline metal and explicit relationships between stress σ and deformation time t were proposed. When t is small enough, the yield stresses can be formulated approximately. According to the different values of the ratio of initially deformed grains, tension rate, grain diameter and other parameters. several typical yield modes can be described. some phenomena can be explained quantitatively, which are in better agreement with Hall-Petch formula and the experiments.
Key words:  polycrystal      yield      dislocation     
Received:  18 March 1995     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1995/V31/I3/97

1周邦新.金属学报,1983;19:A312FujitaH.MiyazakiS.ActaMetall1978:26:12733哈宽富.金属力学性质的微观理论.北京:科学出版社,1991:4164PetchNJ.JIronSteelInst1953:174:255CottrellAH.TransAIME.1958:212:1926JamesLiTransAIME.1963:227:2397HallEO.ProcRoySoc,1951:B64:4748BaldwinJrWMActaMetall.1955:3:1869JohnstonWGJApplPhys.1962;33:271610NahnGT.ActaMetall,1962;10:72711赖祖涵.金属的晶体缺陷与力学性质,北京:冶金工业出版社,1988:19312PetchNJActaMetall1964;12:59
[1] HAN Weizhong, LU Yan, ZHANG Yuheng. Mechanism of Ductile-to-Brittle Transition in Body-Centered-Cubic Metals:A Brief Review[J]. 金属学报, 2023, 59(3): 335-348.
[2] HAN Dong, ZHANG Yanjie, LI Xiaowu. Effect of Short-Range Ordering on the Tension-Tension Fatigue Deformation Behavior and Damage Mechanisms of Cu-Mn Alloys with High Stacking Fault Energies[J]. 金属学报, 2022, 58(9): 1208-1220.
[3] TIAN Ni, SHI Xu, LIU Wei, LIU Chuncheng, ZHAO Gang, ZUO Liang. Effect of Pre-Tension on the Fatigue Fracture of Under-Aged 7N01 Aluminum Alloy Plate[J]. 金属学报, 2022, 58(6): 760-770.
[4] ZHENG Shijian, YAN Zhe, KONG Xiangfei, ZHANG Ruifeng. Interface Modifications on Strength and Plasticity of Nanolayered Metallic Composites[J]. 金属学报, 2022, 58(6): 709-725.
[5] GAO Chuan, DENG Yunlai, WANG Fengquan, GUO Xiaobin. Effect of Creep Aging on Mechanical Properties of Under-Aged 7075 Aluminum Alloy[J]. 金属学报, 2022, 58(6): 746-759.
[6] SHEN Guohui, HU Bin, YANG Zhanbing, LUO Haiwen. Influence of Tempering Temperature on Mechanical Properties and Microstructures of High-Al-Contained Medium Mn Steel Having δ-Ferrite[J]. 金属学报, 2022, 58(2): 165-174.
[7] WU Xiaolei, ZHU Yuntian. Heterostructured Metallic Materials: Plastic Deformation and Strain Hardening[J]. 金属学报, 2022, 58(11): 1349-1359.
[8] LAN Liangyun, KONG Xiangwei, QIU Chunlin, DU Linxiu. A Review of Recent Advance on Hydrogen Embrittlement Phenomenon Based on Multiscale Mechanical Experiments[J]. 金属学报, 2021, 57(7): 845-859.
[9] AN Xudong, ZHU Te, WANG Qianqian, SONG Yamin, LIU Jinyang, ZHANG Peng, ZHANG Zhaokuan, WAN Mingpan, CAO Xingzhong. Interaction Mechanism of Dislocation and Hydrogen in Austenitic 316 Stainless Steel[J]. 金属学报, 2021, 57(7): 913-920.
[10] SHI Zengmin, LIANG Jingyu, LI Jian, WANG Maoqiu, FANG Zifan. In Situ Analysis of Plastic Deformation of Lath Martensite During Tensile Process[J]. 金属学报, 2021, 57(5): 595-604.
[11] LIANG Jinjie, GAO Ning, LI Yuhong. Interaction Between Interstitial Dislocation Loop and Micro-Crack in bcc Iron Investigated by Molecular Dynamics Method[J]. 金属学报, 2020, 56(9): 1286-1294.
[12] LI Meilin, LI Saiyi. Motion Characteristics of <c+a> Edge Dislocation on the Second-Order Pyramidal Plane in Magnesium Simulated by Molecular Dynamics[J]. 金属学报, 2020, 56(5): 795-800.
[13] LI Yuancai, JIANG Wugui, ZHOU Yu. Effect of Nanopores on Tensile Properties of Single Crystal/Polycrystalline Nickel Composites[J]. 金属学报, 2020, 56(5): 776-784.
[14] LI Yizhuang,HUANG Mingxin. A Method to Calculate the Dislocation Density of a TWIP Steel Based on Neutron Diffraction and Synchrotron X-Ray Diffraction[J]. 金属学报, 2020, 56(4): 487-493.
[15] LIU Yang,WANG Lei,SONG Xiu,LIANG Taosha. Microstructure and High-Temperature Deformation Behavior of Dissimilar Superalloy Welded Joint of DD407/IN718[J]. 金属学报, 2019, 55(9): 1221-1230.
No Suggested Reading articles found!