PSEUDO-COUPLED ZONE AND NUCLEATION OF Ni-Sn ALLOY UNDER DEEP UNDERCOOLING |
LI Shunpu;ZHAO Deqian;CHEN Xichen(Institute of phesics;Chinese Academy of Sciences;Beijing 100080)(Manuscript received 1994-08-25) |
|
Cite this article:
LI Shunpu;ZHAO Deqian;CHEN Xichen(Institute of phesics;Chinese Academy of Sciences;Beijing 100080)(Manuscript received 1994-08-25). PSEUDO-COUPLED ZONE AND NUCLEATION OF Ni-Sn ALLOY UNDER DEEP UNDERCOOLING. Acta Metall Sin, 1995, 31(7): 304-308.
|
Abstract The deep undercooling of the Ni-Sn alloy was achieved by means of the cyclic overheating to high temperature and rapid quenching in a mixed inorganic sail flux,so the pseudo-coupled zone of the alloy was obtained.Under deep undercooling,the nucleations of eutectic phases are both in dependent and heterogeneous.although the Ni3Sn phase is easy to grow nuclei.The inherent impurities in Ni-Sn alloy are favourable to nucleation of α-Ni phase.Correspondent.LI(Shunpu,Institute of physics,Chinese Academy of Sciences,Beijing 100080)
|
Received: 18 July 1995
|
1MerzGD.KattamisTZ.MetallTrans,1977:8A:295
2KattamisTZ,FlemingsMC.ModCast,1967;67:97
3PerepezkoJH,MaterSciEng,1984;65:125
4LacyLL,RathzTJ,RobisonMB.JApplPhys,1982;53:682
5MurtyY.KattamisTZ.JCrystGrowth.1974:22:219
6OjhaSN,AnantharamanTR,PamachandraraoP.JMaterSci,1982;17:2644
7JonesBL,WestonGM,SouthinRT.JCrystGrowth.1971:10:313
8MurtyY.KattaminsTZ,JCrystGrowth.1974:22:219
9ChuMGMetallTrans,1984:15A:1303
10TewariSNMetallTrans.1987:18A:525
11邢力谦,杨根仓,周尧和,郭振琪,材料科学进展,1991;5(1):16
12WuY,PicconeTJ,ShioharaY.MetallTrans1987;18A:915
13SmithellsCJ.MetalsReferenceBook.Lond0n:Butterworth&Ltd.1976:186 |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|