Please wait a minute...
Acta Metall Sin  1995, Vol. 31 Issue (7): 304-308    DOI:
论文 Current Issue | Archive | Adv Search |
PSEUDO-COUPLED ZONE AND NUCLEATION OF Ni-Sn ALLOY UNDER DEEP UNDERCOOLING
LI Shunpu;ZHAO Deqian;CHEN Xichen(Institute of phesics;Chinese Academy of Sciences;Beijing 100080)(Manuscript received 1994-08-25)
Cite this article: 

LI Shunpu;ZHAO Deqian;CHEN Xichen(Institute of phesics;Chinese Academy of Sciences;Beijing 100080)(Manuscript received 1994-08-25). PSEUDO-COUPLED ZONE AND NUCLEATION OF Ni-Sn ALLOY UNDER DEEP UNDERCOOLING. Acta Metall Sin, 1995, 31(7): 304-308.

Download:  PDF(391KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  

The deep undercooling of the Ni-Sn alloy was achieved by means of the cyclic overheating to high temperature and rapid quenching in a mixed inorganic sail flux,so the pseudo-coupled zone of the alloy was obtained.Under deep undercooling,the nucleations of eutectic phases are both in dependent and heterogeneous.although the Ni3Sn phase is easy to grow nuclei.The inherent impurities in Ni-Sn alloy are favourable to nucleation of α-Ni phase.Correspondent.LI(Shunpu,Institute of physics,Chinese Academy of Sciences,Beijing 100080)

Key words:  :undercooling      eutectic alloy      pseudo-coupled zone      nucleation     
Received:  18 July 1995     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1995/V31/I7/304

1MerzGD.KattamisTZ.MetallTrans,1977:8A:295
2KattamisTZ,FlemingsMC.ModCast,1967;67:97
3PerepezkoJH,MaterSciEng,1984;65:125
4LacyLL,RathzTJ,RobisonMB.JApplPhys,1982;53:682
5MurtyY.KattamisTZ.JCrystGrowth.1974:22:219
6OjhaSN,AnantharamanTR,PamachandraraoP.JMaterSci,1982;17:2644
7JonesBL,WestonGM,SouthinRT.JCrystGrowth.1971:10:313
8MurtyY.KattaminsTZ,JCrystGrowth.1974:22:219
9ChuMGMetallTrans,1984:15A:1303
10TewariSNMetallTrans.1987:18A:525
11邢力谦,杨根仓,周尧和,郭振琪,材料科学进展,1991;5(1):16
12WuY,PicconeTJ,ShioharaY.MetallTrans1987;18A:915
13SmithellsCJ.MetalsReferenceBook.Lond0n:Butterworth&Ltd.1976:186

[1] ZHAO Yafeng, LIU Sujie, CHEN Yun, MA Hui, MA Guangcai, GUO Yi. Critical Inclusion Size and Void Growth in Dual-Phase Ferrite-Bainite Steel During Ductile Fracture[J]. 金属学报, 2023, 59(5): 611-622.
[2] ZHANG Lili, JI Zongwei, ZHAO Jiuzhou, HE Jie, JIANG Hongxiang. Key Factors Influencing Eutectic Si Modification in Al-Si Hypoeutectic Alloy by Trace La[J]. 金属学报, 2023, 59(11): 1541-1546.
[3] FENG Di, ZHU Tian, ZANG Qianhao, LEE Yunsoo, FAN Xi, ZHANG Hao. Solution Behavior of Spray-Formed Hypereutectic AlSiCuMg Alloy[J]. 金属学报, 2022, 58(9): 1129-1140.
[4] WU Caihong, FENG Di, ZANG Qianhao, FAN Shichun, ZHANG Hao, LEE Yunsoo. Microstructure Evolution and Recrystallization Behavior During Hot Deformation of Spray Formed AlSiCuMg Alloy[J]. 金属学报, 2022, 58(7): 932-942.
[5] LI Xifeng, LI Tianle, AN Dayong, WU Huiping, CHEN Jieshi, CHEN Jun. Research Progress of Titanium Alloys and Their Diffusion Bonding Fatigue Characteristics[J]. 金属学报, 2022, 58(4): 473-485.
[6] Juan DU, Xiaoxing CHENG, Tiannan YANG, Longqing CHEN, Frédéric Mompiou, Wenzheng ZHANG. In Situ TEM Study on the Sympathetic Nucleation of Austenite Precipitates[J]. 金属学报, 2019, 55(4): 511-520.
[7] Jianfeng ZHANG, Qing LAN, Qichi LE. Investigation on the Change of Thermoelectric Power of Al-Fe Hypoeutectic Alloy Melt Caused by AC Magnetic Field[J]. 金属学报, 2018, 54(7): 1042-1050.
[8] Shubo LI, Wenbo DU, Xudong WANG, Ke LIU, Zhaohui WANG. Effect of Zr Addition on the Grain Refinement Mechanism of Mg-Gd-Er Alloys[J]. 金属学报, 2018, 54(6): 911-917.
[9] Dandan FAN, Junfeng XU, Yanan ZHONG, Zengyun JIAN. Effect of Superheated Temperature and Cooling Rate on the Solidification of Undercooled Ti Melt[J]. 金属学报, 2018, 54(6): 844-850.
[10] Jincheng WANG, Can GUO, Qi ZHANG, Sai TANG, Junjie LI, Zhijun WANG. Recent Progresses in Modeling of Nucleation During Solidification on the Atomic Scale[J]. 金属学报, 2018, 54(2): 204-216.
[11] Tongmin WANG, Jingjing WEI, Xudong WANG, Man YAO. Progress and Application of Microstructure Simulation of Alloy Solidification[J]. 金属学报, 2018, 54(2): 193-203.
[12] Zongyuan ZOU, Xiaokui XU, Yinxiao LI, Chao WANG. Study on the Method of Improving the Toughness of CGHAZ for High Heat Input Welding Steels[J]. 金属学报, 2017, 53(8): 957-967.
[13] Jin WANG, Yuefei ZHANG, Jinyao MA, Jixue LI, Ze ZHANG. Microcrack Nucleation and Propagation Investigation ofInconel 740H Alloy Under In SituHigh Temperature Tensile Test[J]. 金属学报, 2017, 53(12): 1627-1635.
[14] Yong YANG,Zhaodong WANG,Tianrui LI,Tao JIA,Xiaolin LI,Guodong WANG. A Model for Precipitation-Temperature-Time Curve Calculation[J]. 金属学报, 2017, 53(1): 123-128.
[15] Liangshun LUO,Tong LIU,Yanning ZHANG,Yanqing SU,Jingjie GUO,Hengzhi FU. MICROSTRUCTURE EVOLUTION AND GROWTH BE-HAVIORS OF FACETED PHASE IN DIRECTIONALLY SOLIDIFIED Al-Y ALLOYS I. Microstructure Evolution of Directionally Solidified Al-15%Y Hypereutectic Alloy[J]. 金属学报, 2016, 52(7): 859-865.
No Suggested Reading articles found!