| Research and Application Progress of SiCp-Reinforced Aluminum-Based Composite Brake Discs for Rail Transit Vehicles |
TAN Dong1, WU Liukun2, FU Kangxi1, XIA Shaohua1, LI Chong2( ), CUI Lei2, LIU Yongchang2, ZAN Yuning3 |
1 CRRC Qishuyan Institute Co. Ltd., Changzhou 213011, China 2 State Key Laboratory of High Performance Roll Materials and Composite Forming, School of Materials Science and Engineering, Tianjin University, Tianjin 300350, China 3 Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China |
|
Cite this article:
TAN Dong, WU Liukun, FU Kangxi, XIA Shaohua, LI Chong, CUI Lei, LIU Yongchang, ZAN Yuning. Research and Application Progress of SiCp-Reinforced Aluminum-Based Composite Brake Discs for Rail Transit Vehicles. Acta Metall Sin, 2026, 62(7): 1163-1174.
|
|
|
Abstract Driven by the “dual-carbon” strategy, the lightweighting of rail transit equipment has become a dominant industry trend. Among the key components, the brake disc—critical to the braking system—faces particularly stringent weight-reduction requirements. SiCp-reinforced aluminum-based composites (SiCp/Al), known for their low density, high thermal conductivity, and superior wear resistance, are now regarded as the prime candidate to replace conventional cast-iron discs. In recent years, SiCp/Al brake discs have been implemented in urban rail transit vehicles operating at 120 km/h. However, their high-temperature stability remains a technical challenge, and no breakthroughs have been achieved for operation on suburban railways at speed ≥ 140 km/h. This study systematically reviews the research progress and engineering applications of SiCp/Al brake discs in rail transit, focusing on its fabrication methods, core performance, in-service behavior, and evaluation standards. Future development directions are discussed to guide technological innovation and the industrial deployment of advanced rail transit equipment.
|
|
Received: 16 December 2025
|
|
|
| Fund: National Key Research and Development Program of China(2023YFB3710602);National Nat-ural Science Foundation of China(U24A2026) |
Corresponding Authors:
LI Chong, professor, Tel: 13021398676, E-mail: lichongme@tju.edu.cn
|
| [1] |
Wang W L, Wu J H, Zhang G D. The tribological and wear behavior of aluminum matrix composites [J]. Acta Metall. Sin., 1998, 34: 1178
|
|
王文龙, 吴军华, 张国定. 铝基复合材料的摩擦磨损性能 [J]. 金属学报, 1998, 34: 1178
|
| [2] |
Xu H Y, Huang L J, Geng L, et al. Effects of Cu content on the wear properties of Al2O3·SiO2sf/Al-Cu composites [J]. Acta Metall. Sin., 2013, 49: 1131
doi: 10.3724/SP.J.1037.2013.00001
|
|
许虹宇, 黄陆军, 耿 林 等. Cu含量对Al2O3·SiO2sf/Al-Cu复合材料耐磨性能的影响 [J]. 金属学报, 2013, 49: 1131
doi: 10.3724/SP.J.1037.2013.00001
|
| [3] |
Liu C X, Luo R, Xie Y, et al. Research progress on particle reinforced aluminum matrix composites for brake discs in rail transit [J]. Mod. Urban Transit, 2022, (7): 11
|
|
刘春轩, 罗 任, 谢 屹 等. 轨道交通制动盘用颗粒增强铝基复合材料研究及进展 [J]. 现代城市轨道交通, 2022, (7): 11
|
| [4] |
Zhang R, Zhu S Z, Liu Z Y, et al. Influence of aging temperatures on precipitation behaviors of SiC/Al-Zn-Mg-Cu composites [J]. Acta Metall. Sin., 2024, 60: 1043
|
|
张 冉, 朱士泽, 刘振宇 等. 时效温度对SiC/Al-Zn-Mg-Cu复合材料时效析出行为的影响 [J]. 金属学报, 2024, 60: 1043
|
| [5] |
Ramanathan A, Krishnan P K, Muraliraja R. A review on the production of metal matrix composites through stir casting—Furnace design, properties, challenges, and research opportunities [J]. J. Manuf. Process., 2019, 42: 213
doi: 10.1016/j.jmapro.2019.04.017
|
| [6] |
Chen Z P, Chen W P, Liu F F. Research progress on casting Al matrix composites [J]. Cast. Equip. Technol., 2020, (1): 42
|
|
陈志平, 陈维平, 刘方方. 铸造铝基复合材料的研究进展 [J]. 铸造设备与工艺, 2020, (1): 42
|
| [7] |
Hashim J, Looney L, Hashmi M S J. Metal matrix composites: Production by the stir casting method [J]. J. Mater. Process. Technol., 1999, 92-93: 1
doi: 10.1016/S0924-0136(99)00118-1
|
| [8] |
Zhang Z L. Investigation on semi-solid stir casting technology of SiCp/A357 composite [D]. Beijing: University of Science and Technology Beijing, 2017
|
|
张桢林. SiCp/A357复合材料半固态搅拌铸造工艺研究 [D]. 北京: 北京科技大学, 2017
|
| [9] |
Pan L W, Lin W J, Tang J F, et al. Preparation methods and research status of particles-reinforced aluminum matrix composites [J]. Mater. Rev., 2016, 30(suppl.1) : 511
|
|
潘利文, 林维捐, 唐景凡 等. 颗粒增强铝基复合材料制备方法及研究现状 [J]. 材料导报, 2016, 30(): 511
|
| [10] |
Pan L K, Han J M, Zhang Y X, et al. Microstructure and properties of derived material for high content SiCp/A356 composites [J]. Chin. J. Nonferrous Met., 2016, 26: 2078
|
|
潘利科, 韩建民, 张颖骁 等. 高含量SiCp/A356复合材料衍生材料的组织与性能 [J]. 中国有色金属学报, 2016, 26: 2078
|
| [11] |
Zhang Z L, Zhang Z F, Xu J, et al. Properties of SiCp/A357 composites fabricated by double-deck mechanical stirring casting [J]. Spec. Cast. Nonferrous Alloys, 2017, 37: 598
|
|
张桢林, 张志峰, 徐 骏 等. 双级机械搅拌铸造SiCp/A357复合材料的工艺及性能 [J]. 特种铸造及有色合金, 2017, 37: 598
|
| [12] |
Zhang Z L, Xu J, Xiang J, et al. Application of electromagnetic stirring suction casting in aluminum matrix composite brake disc [J]. Spec. Cast. Nonferrous Alloys, 2022, 42: 171
|
|
张桢林, 徐 骏, 向 俊 等. 电磁搅拌吸铸技术及其在铝陶制动盘铸造中的应用 [J]. 特种铸造及有色合金, 2022, 42: 171
doi: 10.15980/j.tzzz.2022.02.008
|
| [13] |
Tong W B. Study on structure and forming process of aluminum matrix composites axial brake disc for urban rail [D]. Beijing: Beijing Jiaotong University, 2019
|
|
童卫兵. 城轨铝基复合材料轴装制动盘结构与成型工艺研究 [D]. 北京: 北京交通大学, 2019
|
| [14] |
Zhao H Q, Yang Z Y, Zhang X F, et al. Casting process design and defect prediction of SiCp/A356 brake disc [J]. Foundry Technol., 2019, 40: 671
|
|
赵海芹, 杨智勇, 张雄飞 等. SiCp/A356制动盘铸造成形工艺设计和缺陷预测 [J]. 铸造技术, 2019, 40: 671
|
| [15] |
Qin Q, Hua J J. Preparation of powder metallurgy submicron SiC particle reinforced Al based composites and mechanical properties [J]. Spec. Cast. Nonferrous Alloys, 2017, 37: 411
|
|
覃 群, 华建杰. 粉末冶金制备SiCp增强Al基复合材料及其性能 [J]. 特种铸造及有色合金, 2017, 37: 411
|
| [16] |
Cao L X, Zhang X Y, Huo S H, et al. Progress of study on powder metallurgical aluminum-based composite brake disc for urban rail transit [J]. Roll. Stock, 2024, 62(6): 87
|
|
曹柳絮, 张晓泳, 霍树海 等. 城市轨道交通粉末冶金铝基复合材料制动盘研究进展 [J]. 铁道车辆, 2024, 62(6): 87
|
| [17] |
Fu K X, Tan D, Zhang S Q, et al. Friction and wear behavior of SiCp/Al brake disk sliding against semimetallic brake pad under the braking condition of urban rail vehicles [J]. Tribol. Trans., 2024, 67: 875
doi: 10.1080/10402004.2024.2389933
|
| [18] |
Tan D, Xia S H, Yob A, et al. Evaluation of the wear resistance of aluminium-based hybrid composite brake discs under relevant city rail environments [J]. Mater. Des., 2022, 215: 110504
doi: 10.1016/j.matdes.2022.110504
|
| [19] |
Viswanatha B M, Kumar M P, Basavarajappa S, et al. Effect of ageing on dry sliding wear behaviour of Al-MMC for disc brake [J]. Tribol. Ind., 2014, 36: 40
|
| [20] |
Hong S J, Kim H M, Huh D, et al. Effect of clustering on the mechanical properties of SiC particulate-reinforced aluminum alloy 2024 metal matrix composites [J]. Mater. Sci. Eng., 2003, A347: 198
|
| [21] |
Wang R, Zhang C. Research on friction and wear properties of aluminum matrix composites for brake discs with SiCp/A357 contents [J]. China Rail., 2023, (2): 74
|
|
王 瑞, 张 臣. 制动盘用SiCp/A357铝基复合材料摩擦磨损性能研究 [J]. 中国铁路, 2023, (2): 74
|
| [22] |
Tan D, Fu K X, Zhang S Q, et al. Friction and wear behavior of different volume fraction SiCp/Al composites by stir casting combined with friction stir processing [J]. Mater. Mech. Eng., 2024, 48(9): 59
|
|
谭 东, 付康习, 张士琦 等. 搅拌铸造结合搅拌摩擦加工制备不同体积分数SiCp/Al复合材料的摩擦磨损行为 [J]. 机械工程材料, 2024, 48(9): 59
|
| [23] |
Lee T, Lee J, Lee D, et al. Effects of particle size and surface modification of SiC on the wear behavior of high volume fraction Al/SiCp composites [J]. J. Alloys Compd., 2020, 831: 154647
doi: 10.1016/j.jallcom.2020.154647
|
| [24] |
Ye C T, Jia L N, Qi Y, et al. Strengthening effects of Mg-Si precipitates on wear resistance of SiCp/Al-Si-Mg composites [J]. Wear, 2025, 564-565: 205716
doi: 10.1016/j.wear.2024.205716
|
| [25] |
Du A D, Lattanzi L, Jarfors A E W, et al. Role of matrix alloy, reinforcement size and fraction in the sliding wear behaviour of Al-SiCp MMCs against brake pad material [J]. Wear, 2023, 530-531: 204969
doi: 10.1016/j.wear.2023.204969
|
| [26] |
Lattanzi L, Awe S A. Thermophysical properties of Al-based metal matrix composites suitable for automotive brake discs [J]. J. Alloys Metall. Syst., 2024, 5: 100059
|
| [27] |
Rong Z Z. Study on high temperature mechanical properties of nano-Al2O3/6061 aluminum matrix composites [D]. Zhengzhou: Zhengzhou University of Aeronautics, 2023
|
|
荣智峥. 纳米氧化铝颗粒增强6061铝基复合材料的高温力学性能研究 [D]. 郑州: 郑州航空工业管理学院, 2023
|
| [28] |
Lyu Y, Wahlström J, Tu M, et al. A friction, wear and emission tribometer study of non-asbestos organic pins sliding against AlSiC MMC discs [J]. Tribol. Ind., 2018, 40: 274
doi: 10.24874/ti
|
| [29] |
Yang Z Y, Zang J J, Fang D L, et al. Thermal fatigue crack propagation mechanism of SiCp/A356 composites for urban rail train brake disc [J]. J. Mater. Eng., 2022, 50(7): 165
|
|
杨智勇, 臧家俊, 方丹琳 等. 城轨列车制动盘SiCp/A356复合材料热疲劳裂纹扩展机理 [J]. 材料工程, 2022, 50(7): 165
doi: 10.11868/j.issn.1001-4381.2021.000521
|
| [30] |
Chen A L, Arai Y, Tsuchida E. An experimental study on effect of thermal cycling on monotonic and cyclic response of cast aluminium alloy-SiC particulate composites [J]. Composites, 2005, 36B: 319
|
| [31] |
Pal S, Bhanuprasad V V, Mitra R. Damage evaluation in discontinuously reinforced aluminum matrix composites subjected to thermal cycling [J]. Mater. Sci. Eng., 2008, A489: 11
|
| [32] |
Nam T H, Requena G, Degischer P. Thermal expansion behaviour of aluminum matrix composites with densely packed SiC particles [J]. Composites, 2008, 39A: 856
|
| [33] |
Requena G, Yubero D C, Corrochano J, et al. Stress relaxation during thermal cycling of particle reinforced aluminium matrix composites [J]. Composites, 2012, 43A: 1981
|
| [34] |
Song P L, Yang Z Y, Zang J J, et al. Effects of thermal cycling treatment on load bearing and friction behavior of SiCp/A356 composites [J]. Eng. Fail. Anal., 2024, 156: 107828
doi: 10.1016/j.engfailanal.2023.107828
|
| [35] |
Pan L K, Han J M, Yang Z Y, et al. Thermal fatigue crack behavior of SiCp/A356 composites prepared by stirring casting [J]. Results Phys., 2017, 7: 927
doi: 10.1016/j.rinp.2017.02.010
|
| [36] |
Zhou K L, Cai W B, Chi M R, et al. Dynamic performance analysis of aluminum matrix composite brake disc for linear metro vehicle [J]. Electr. Drive Locomot., 2021, (1): 53
|
|
周开磊, 蔡吴斌, 池茂儒 等. 直线电机地铁车辆铝基复合材料制动盘动力学性能分析 [J]. 机车电传动, 2021, (1): 53
|
| [37] |
Gou Q B, Zhang N, Meng F H, et al. Development and experimental study of new brake friction pairs for standard metro train [J]. Electr. Drive Locomot., 2022, (2): 67
|
|
苟青炳, 张 宁, 孟繁辉 等. 标准地铁车辆用新型制动摩擦副设计与试验研究 [J]. 机车电传动, 2022, (2): 67
|
| [38] |
Zhao F. Application of aluminum matrix composite brake disc on subway vehicles [J]. Machinery, 2023, 50(10): 33
|
|
赵 锋. 铝基复合材料制动盘在地铁车辆上的应用研究 [J]. 机械, 2023, 50(10): 33
|
| [39] |
Cao J H, Liang H, Xue J, et al. Research on brake disc lightweight technology based on improving train running quality [J]. Mod. Urban Transit, 2019, (11): 47
|
|
曹建行, 梁 洪, 薛 江 等. 基于提高列车运行品质的制动盘轻量化技术研究 [J]. 现代城市轨道交通, 2019, (11): 47
|
| [40] |
Zhao N Q, Liu X H, Pu B W. Progress on multi-dimensional carbon nanomaterials reinforced aluminum matrix composites: A review [J]. Acta Metall. Sin., 2019, 55: 1
doi: 10.11900/0412.1961.2018.00456
|
|
赵乃勤, 刘兴海, 蒲博闻. 多维度碳纳米相增强铝基复合材料研究进展 [J]. 金属学报, 2019, 55: 1
doi: 10.11900/0412.1961.2018.00456
|
| [41] |
Zhang X X, Zheng Z, Gao Y, et al. Progress in high throughput fabrication and characterization of metal matrix composites [J]. Acta Metall. Sin., 2019, 55: 109
doi: 10.11900/0412.1961.2018.00307
|
|
张学习, 郑 忠, 高 莹 等. 金属基复合材料高通量制备及表征技术研究进展 [J]. 金属学报, 2019, 55: 109
doi: 10.11900/0412.1961.2018.00307
|
| [42] |
Bi S, Li Z C, Sun H X, et al. Microstructure and mechanical properties of carbon nanotubes-reinforced 7055Al composites fabricated by high-energy ball milling and powder metallurgy processing [J]. Acta Metall. Sin., 2021, 57: 71
doi: 10.11900/0412.1961.2020.00238
|
|
毕 胜, 李泽琛, 孙海霞 等. 高能球磨结合粉末冶金法制备碳纳米管增强7055Al复合材料的微观组织和力学性能 [J]. 金属学报, 2021, 51: 71
|
| [43] |
Zhou L, Zhang M Y, Yang X S, et al. Simulation of thermal expansion coefficient of configurational GNPs/2009Al composites [J]. Acta Metall. Sin., 2024, 60: 977
doi: 10.11900/0412.1961.2022.00333
|
|
周 丽, 张明远, 杨欣盛 等. 构型化石墨烯纳米片/2009Al复合材料热膨胀系数模拟 [J]. 金属学报, 2024, 60: 977
|
| [44] |
Kukutschová J, Roubíček V, Malachová K, et al. Wear mechanism in automotive brake materials, wear debris and its potential environmental impact [J]. Wear, 2009, 267: 807
doi: 10.1016/j.wear.2009.01.034
|
| [45] |
Yuan Z W, Tian C, Zhang D Q, et al. Development and testing of pad for brake disc of aluminum matrix composites [J]. J. Tongji Univ. (Nat. Sci. Ed.), 2019, 47: 201
|
|
袁泽旺, 田 春, 张定权 等. 铝基复合制动盘闸片开发及试验 [J]. 同济大学学报(自然科学版), 2019, 47: 201
|
| [46] |
Gao H M, Wang G S, Yang H S, et al. Application and development of organic friction materials in rail transit field [J]. Rail Transit Mater., 2024, 3(1): 32
|
|
高红梅, 汪贵松, 杨火顺 等. 合成摩擦材料在轨道交通领域的应用与发展 [J]. 轨道交通材料, 2024, 3(1): 32
|
| [47] |
Li S C. Performance research of organic composite friction materials matching Al-MMC brake discs [D]. Nanning: Guangxi University for Nationalities, 2024
|
|
李尚谌. 匹配铝基制动盘的有机复合摩擦材料性能研究 [D]. 南宁: 广西民族大学, 2024
|
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|