Microstructure and Mechanical Properties of Monel K-500 Alloy in Synergetic Modulation of Directional Solidification and Thermal Processing
YANG Minghui, LI Xingwu, SUN Chonghao, RUAN Ying()
School of Physical Science and Technology, Northwestern Polytechnical University, Xi'an 710072, China
Cite this article:
YANG Minghui, LI Xingwu, SUN Chonghao, RUAN Ying. Microstructure and Mechanical Properties of Monel K-500 Alloy in Synergetic Modulation of Directional Solidification and Thermal Processing. Acta Metall Sin, 2025, 61(4): 561-571.
Monel K-500 alloy is a Ni-based alloy that is widely used in marine environments and chemical industries because of its exceptional corrosion resistance and mechanical properties. The synergetic modulation of directional solidification and thermal processing (DS-TP) technique combines DS and in situ heat treatment in a single experiment, thus eliminating the influence of environmental changes and avoiding aging effect. To investigate the effect of the DS-TP technique on the mechanical properties of the alloy, samples were prepared using DS alone and the DS-TP technique at different growth rates. Subsequently, the microstructures and mechanical properties of the samples were analyzed. In the DS experiments, an Al2O3 ceramic crucible (diameter: 10 mm) containing the alloy sample was heated using a graphite heater and an electromagnetic induction coil. As the sample was superheated to 200 K, it was immersed in the Ga-In-Sn liquid at a certain pulling rate. In the DS-TP experiments, the directionally solidified sample was in situ annealed at 1223 K for 1 h and then immersed into the liquid. Subsequently, the sample was subjected to an aging process at 923 K for 5 h. The microstructure of the directionally solidified Monel K-500 alloy showed columnar γ grains with pronounced <001> texture. When the growth rate decreased, the temperature gradient at the solid-liquid interface during directional solidification increased. Lower growth rates led to a coarser microstructure, lesser microsegregation of Cu, and fewer transverse grain boundaries. As the growth rate decreased from 100 μm/s to 5 μm/s, the yield strength, tensile strength, and elongation increased from 248 MPa, 421 MPa, and 63.4% to 288 MPa, 487 MPa, and 69.9%, respectively. Unlike the case of the directionally solidified alloys, the nanoscale γʹ hardening phase precipitated in the DS-TP-treated alloys and the degree of microsegregation decreased. Further, the yield strength and tensile strength increased from 368 and 640 MPa, respectively, to 386 and 686 MPa, respectively, as the growth rate decreased from 100 μm/s to 5 μm/s. The distribution of intergranular cracks in the fractography was similar to that of large-angle grain boundaries in the region closing the fracture. With the growth rate decreasing, intragranular cracks gradually appeared, and the number of intergranular cracks decreased. Moreover, grain deviation from the preferred growth orientation increased the dislocation density and decreased the elongation. Grain refinement promoted the homogeneous distribution of dislocations and caused a slight increase in the elongation. At a growth rate of 5 μm/s, the tensile strength and yield strength of the DS-TP-treated alloy increased by 34% and 41%, respectively.
Fund: National Natural Science Foundation of China(52073232, 52225406, 52088101);Science Fund for Scientific and Technological Innovation Team of Shaanxi Province(2021TD-14)
Corresponding Authors:
RUAN Ying, professor, Tel: (029)88431669, E-mail: ruany@nwpu.edu.cn
Fig.1 Experimental schematics of directional solidification (DS) (a) and synergetic modulation of directional solidification and thermal processing (DS-TP) (b) of Monel K-500 alloys (T—temperature of sample, t—time of experiment, TL—melting tempereture, TP1—holding temperature; insets are the schematics of the movement of samples during DS and DS-TP, respectively)
Fig.2 Schematics of sampling positions for EBSD analyses (a) and specimen dimensions of Monel K-500 alloy (b) (Red surfaces are the regions of EBSD observation)
Fig.3 Microstructures (a-c) and locally high magnified images (d-f) of directionally solidified Monel K-500 alloy at growth rates (V) of 5 μm/s (a, d), 50 μm/s (b, e), and 100 μm/s (c, f), and primary dendrite trunk spacing (λ1) and secondary dendrite arm spacing (λ2) (g) (Q—quenching region, D—directional solidified region)
Fig.4 Crystal orientation distributions of γ phase in Monel K-500 alloys processed by DS (a-c) and DS-TP (d-f) at growth rates of 5 μm/s (a, d), 50 μm/s (b, e), and 100 μm/s (c, f) (SD—solidification direction, ND—normal direction, TD—transverse direction; red cubes are the unit cells of corresponding grain)
Fig.5 Element distributions of dendrite interface in Monel K-500 alloy processed by DS (a-c) and DS-TP (d-f) at growth rates of 5 μm/s (a, d), 50 μm/s (b, e), and 100 μm/s (c, f)
Fig.6 TEM analyses of Monel K-500 alloys processed by DS (a-c) and DS-TP (d-f) at growth rate of 5 μm/s (Insets in Fig.6e show the fast Fourier transform (FFT) patterns) (a, d) bright field (BF) and dark field (DF) images (b, e) high-resolution TEM (HRTEM) images (c, f) selected area electron diffraction (SAED) patterns
Fig.7 Tensile performances of Monel K-500 alloys processed by DS and DS-TP (a) stress-strain curves (b) yield strength (σs) (c) ultimate tensile strength (σb) (d) elongation (δ)
Fig.8 Grain orientation distributions (a1-c1), and low (a2-c2) and high (a3-c3) magnified SEM images of Monel K-500 alloys processed by DS-TP at growth rates of 5 μm/s (a1-a3), 50 μm/s (b1-b3), and 100 μm/s (c1-c3)
Fig.9 Kernel average misorientation (KAM) distributions and pole figure (insets) in regions I (a1-c1), II (a2-c2), and III (a3-c3) in Fig.2a of the tensile specimen of Monel K-500 alloys processed by DS-TP at growth rates of 5 μm/s (a1-a3), 50 μm/s (b1-b3), and 100 μm/s (c1-c3) (The dotted circles in Figs.9b1-b3 show the projection of grain A on the pole figure)
Fig.10 Grain orientation distributions of longitudinal fracture section (Arrows show the grain boundaries formed during plastic deformation) (a1-c1) and misorientation distributions (a2-c2) of Monel K-500 alloys processed by synergetic modulation at growth rates of 5 μm/s (a1, a2), 50 μm/s (b1, b2), and 100 μm/s (c1, c2) (Insets show the misorientation distributions of Monel K-500 alloys before fracture)
1
Chen J, Wang J Z, Yan F Y, et al. Effect of applied potential on the tribocorrosion behaviors of Monel K500 alloy in artificial seawater [J]. Tribol. Int., 2015, 81: 1
2
Gouda V K, Selim I Z, Khedr A A, et al. Pitting corrosion behaviour of Monel-400 alloy in chloride solutions [J]. J. Mater. Sci. Technol., 1999, 15: 208
3
Hu Q F, Liu Y C, Zhang T, et al. Corrosion failure analysis on the copper alloy flange by experimental and numerical simulation [J]. Eng. Fail. Anal., 2020, 109: 104276
4
Kannan A R, Kumar S M, Pramod R, et al. Microstructure and corrosion resistance of Ni-Cu alloy fabricated through wire arc additive manufacturing [J]. Mater. Lett., 2022, 308: 131262
5
Dey G K, Mukhopadhyay P. Precipitation in the Ni Cu-base alloy Monel K-500 [J]. Mater. Sci. Eng., 1986, 84: 177
6
Zhi Y Q, Zhang M C, Tang R Q, et al. Precipitation of strengthening phase in 718Plus alloy during early aging [J]. Chin. J. Nonferrous Met., 2023, 33: 55
Chen Z, Wang C C, Tang C, et al. Microstructure and mechanical properties of a Monel K-500 alloy fabricated by directed energy deposition [J]. Mater. Sci. Eng., 2022, A857: 144113
8
Harris Z D, Burns J T. The effect of isothermal heat treatment on hydrogen environment-assisted cracking susceptibility in Monel K-500 [J]. Mater. Sci. Eng., 2019, A764: 138249
9
Shoemaker L E, Smith G D. A century of Monel metal: 1906-2006 [J]. JOM, 2006, 58(9): 22
10
Es-Said O S, Zakharia K, Zakharia Z, et al. Failure analysis of K-Monel 500 (Ni-Cu-Al alloy) bolts [J]. Eng. Fail. Anal., 2000, 7: 323
11
Nayan N, Singh G, Souza P M, et al. Hot workability and microstructure control in Monel®400 (Ni-30Cu) alloy: An approach using processing map, constitutive equation and deformation modeling [J]. Mater. Sci. Eng., 2021, A825: 141855
12
Kim K M, Hurley P, Duarte J P. High-resolution prediction of quenching behavior using machine learning based on optical fiber temperature measurement [J]. Int. J. Heat Mass Transfer, 2022, 184: 122338
13
He Z B, Chen B Y, Zhou B W, et al. Effect of TiC precipitation on the corrosion behavior of Monel K500 alloy in 3.5 wt.% NaCl solution [J]. Corros. Sci., 2023, 211: 110886
14
Arjmand M, Abbasi S M, Taheri A K, et al. Hot workability of cast and wrought Ni-42Cu alloy through hot tensile and compression tests [J]. Trans. Nonferrous Met. Soc. China, 2016, 26: 1589
15
Ebrahimi G R, Momeni A, Ezatpour H R, et al. Dynamic recrystallization in Monel400 Ni-Cu alloy: Mechanism and role of twinning [J]. Mater. Sci. Eng., 2019, A744: 376
16
Marenych O O, Ding D, Pan Z, et al. Effect of chemical composition on microstructure, strength and wear resistance of wire deposited Ni-Cu alloys [J]. Addit. Manuf., 2018, 24: 30
17
Li X W, Ruan Y, Sun C H, et al. Distinct difference between peri-eutectic and eutectic growth in ternary Fe-Ni-Ti alloy [J]. Scr. Mater., 2023, 226: 115193
18
Li J, Ding R, Guo Q Y, et al. Effect of solution cooling rate on microstructure evolution and mechanical properties of Ni-based superalloy ATI 718Plus [J]. Mater. Sci. Eng., 2021, A812: 141113
19
Hofmeister M, Klein L, Miran H, et al. Corrosion behaviour of stainless steels and a single crystal superalloy in a ternary LiCl-KCl-CsCl molten salt [J]. Corros. Sci., 2015, 90: 46
20
Liu K L, Wang J S, Yang Y H, et al. An integrated microporosity model of 3D X-ray micro-tomography and directional solidification simulations for Ni-based single crystal superalloys [J]. Comput. Mater. Sci., 2021, 188: 110172
21
Gündüz M, Kaya H, Çadırlı E, et al. Effect of solidification processing parameters on the cellular spacings in the Al-0.1wt% Ti and Al-0.5wt% Ti alloys [J]. J. Alloys Compd., 2007, 439: 114
22
Li J Z, Li J G. Effects of solidification rate and temperature gradient on microstructure and crystal orientation of Co32Ni40Al28 alloys [J]. Mater. Lett., 2012, 68: 40
23
Xu Y K, Li C L, Huang Z H, et al. Microstructure and mechanical properties of CoCrCuFeNiTi0.8 high-entropy alloy prepared by directional solidification [J]. Chin. J. Nonferrous Met., 2021, 31: 1494
Liu T, Tao J, Cai X Y, et al. Effect of growth rate on microstructure evolution in directionally solidified Ti-47Al alloy [J]. Heliyon, 2022, 8: e08704
25
Yang X, Chen R R, Liu T, et al. Formation of dendrites and strengthening mechanism of dual-phase Ni36Co30Fe11Cr11Al6Ti6 HEA by directional solidification [J]. J. Alloys Compd., 2023, 948: 169806
26
Liu G H, Li X Z, Su Y Q, et al. Microstructure, microsegregation pattern and the formation of B2 phase in directionally solidified Ti-46Al-8Nb alloy [J]. J. Alloys Compd., 2012, 541: 275
27
Vaidya M, Pradeep K G, Murty B S, et al. Bulk tracer diffusion in CoCrFeNi and CoCrFeMnNi high entropy alloys [J]. Acta Mater., 2018, 146: 211
28
Lü M T, Li J L, Sun J D, et al. Design of cuboidal γ/γ' coherent microstructure and its stability in low-density Co-Ni-Al-Mo-Cr-Ti/Nb/Ta superalloys [J]. Acta Phys. Sin., 2022, 71: 118102
Gao Z M, Jie W Q, Liu Y Q, et al. Formation mechanism and coupling prediction of microporosity and inverse segregation: A review [J]. Acta Metall. Sin., 2018, 54: 717
doi: 10.11900/0412.1961.2017.00501
Gupta R, Sharma V, Prasad M J N V, et al. Orientation anisotropy and strain localization during elevated temperature tensile deformation of single crystal and bi-crystal Ni-based GTD444 superalloy [J]. Mater. Sci. Eng., 2023, A880: 145310
31
Sun H, Lin X P, Zhou B, et al. Microstructures and tensile deformation behavior of directionally solidified Mg-xGd-0.5Y alloys [J]. Acta Metall. Sin., 2020, 56: 340
Martin N, Hor A, Copin E, et al. Correlation between microstructure heterogeneity and multi-scale mechanical behavior of hybrid LPBF-DED Inconel 625 [J]. J. Mater. Process. Technol., 2022, 303: 117542
33
Chandra S, Samal M K, Kumar N N, et al. Atomistically informed crystal plasticity analysis of deformation behavior of alloy 690 including grain boundary effects [J]. Materialia, 2021, 16: 101053
34
Bibhanshu N, Gussev M N, Massey C P, et al. Investigation of deformation mechanisms in an advanced FeCrAl alloy using in-situ SEM-EBSD testing [J]. Mater. Sci. Eng., 2022, A832: 142373