Please wait a minute...
Acta Metall Sin  2020, Vol. 56 Issue (10): 1335-1342    DOI: 10.11900/0412.1961.2020.00002
Current Issue | Archive | Adv Search |
Peritectic Solidification Characteristics and Mechanism of 15CrMoG Steel
LI Yaqiang1, LIU Jianhua1(), DENG Zhenqiang1, QIU Shengtao2, ZHANG Pei3, ZHENG Guiyun3
1 Institute of Engineering Technology, University of Science and Technology Beijing, Beijing 100083, China
2 National Engineering Research Center of Continuous Casting Technology, Central Iron and Steel Research Institute, Beijing 100081, China
3 Laiwu Branch of Shandong Iron and Steel Ltd. , Jinan 271104, China
Cite this article: 

LI Yaqiang, LIU Jianhua, DENG Zhenqiang, QIU Shengtao, ZHANG Pei, ZHENG Guiyun. Peritectic Solidification Characteristics and Mechanism of 15CrMoG Steel. Acta Metall Sin, 2020, 56(10): 1335-1342.

Download:  HTML  PDF(2256KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  

Cast defects of hypo-peritectic steel such as uneven growth of strand shell, crack formation and oscillation marks formation were found to occur frequently during continuous casting of steels. In industry, measures such as high-basicity casting powder, hot-top mold and reduction of mold cooling strength were usually used in the investigations, but a reasonable explanation for these measures has been lacking. In this work, solidification of 15CrMoG steel at different cooling rates were observed with an ultra high temperature confocal scanning laser microscope. The precipitation of the δ-phase was in a cellular manner when the cooling rates were 5 and 15 ℃/min, whereas it was in a dendrite manner when the cooling rate was increased to 100 ℃/min. Thermodynamic analysis of the peritectic phase nucleation showed that a concentration gradient existed at the L/δ interface during the solidication of initial δ phase which led to an increase in the Gibbs free energy barrier for the nucleation of the peritectic γ phase. As the cooling rate increased, the concentration gradient across the L/δ interface became steeper, resulting in an increase in the nucleation undercooling of the peritectic γ phase. This, in turn, decreased the temperature and increased the peritectic reaction rate. In addition, an increase in the cooling rate led to a change in the mode of peritectic transformation (δ→γ). A diffusion-controlled δ→γ transformation occurred due to the progression of planar and cellular interfaces at cooling rates of 5 and 15 ℃/min, respectively. However, a large δ→γ transformation, which was controlled by the interface process, occurred when the cooling rate was increased to 100 ℃/min. The difference in volume shrinkage of the different modes of peritectic transformation (δ→γ) led to a discussion of the control mechanism of continuous casting of hypo-peritectic steel.

Key words:  15CrMoG steel      cooling rate      peritectic reaction      peritectic transformation      continuous casting     
Received:  02 January 2020     
ZTFLH:  TF777  
Fund: National Natural Science Foundation of China(51874028)

URL: 

https://www.ams.org.cn/EN/10.11900/0412.1961.2020.00002     OR     https://www.ams.org.cn/EN/Y2020/V56/I10/1335

Fig.1  Schematic of temperature control of experiments
Fig.2  In situ observations of δ precipitation and peritectic phase transformation at a cooling rate of 5 ℃/min (L—liquid phase)
(a, b) precipitation and growth of δ-ferrite (c, d) peritectic reaction (e, f) peritectic transformation
Fig.3  In situ observations of δ precipitation and peritectic phase transformation at the cooling rate of 15 ℃/min (a, b) precipitation and growth of δ-ferrite (c, d) peritectic reaction (e, f) peritectic transformation
Fig.4  In situ observations of δ precipitation and peritectic phase transformation at the cooling rate of 100 ℃/min
(a, b) precipitation and growth of δ-ferrite (c, d) peritectic reaction (e, f) peritectic transformation
Fig.5  Peritectic reactions at cooling rates of 5 ℃/min (a), 15 ℃/min (b) and 100 ℃/min (c)
Fig.6  Peritectic transformations at cooling rates of 5 ℃/min (a), 15 ℃/min (b) and 100 ℃/min (c)
Fig.7  Schematic of the concentration distribution at theL/δ interface
Fig.8  Carbon concentration distribution (a) and Gibbs free energies at cooling rates of 5 ℃/min (b), 15 ℃/min (c) and 100 ℃/min (d), respectively (T1, T2 and T3 are peritectic phase transformation temperatures at cooling rates of 5, 15 and 100 ℃/min, respectively. T0-line is the thermodynamic equivalence of δ and γ. Gδm, Gγmand GLm are Gibbs free energies of δ, γ and liquid, respectively. ΔGm is the thermodynamic driving force for the transformation of δ to γ. Cδ* is interfacial composition of δ. Cδe, Cγ/δe, Cγ/Leand CLe are the average compositions of δ,γ/δ interface, γ/L interface and liquid, respectively)
Color online
Fig.9  Migration distances of the L/δ and δ/γ interfaces as a function of the square root of time at the cooling rate of 5 ℃/min (t—time)
[1] Suzuki M, Yu C H, Sato H, et al. Origin of heat transfer anomaly and solidifying shell deformation of peritectic steels in continuous casting [J]. ISIJ Int., 1996, 36(suppl.): S171
[2] Jiang Z K, Su Z J, Xu C Q, et al. Abnormal mold level fluctuation during slab casting of peritectic steels [J]. J. Iron Steel Res. Int., 2020, 27: 160
doi: 10.1007/s42243-019-00299-7
[3] Saraswat R, Maijer D M, Lee P D, et al. The effect of mould flux properties on thermo-mechanical behaviour during billet continuous casting [J]. ISIJ Int., 2007, 47: 95
doi: 10.2355/isijinternational.47.95
[4] Xia G, Bernhard C, Ilie S, et al. A study about the influence of carbon content in the steel on the casting behavior [J]. Steel Res. Int., 2011, 82: 230
doi: 10.1002/srin.201000196
[5] Boettinger W J, Coriell S R, Greer A L, et al. Solidification microstructures: Recent developments, future directions [J]. Acta Mater., 2000, 48: 43
doi: 10.1016/S1359-6454(99)00287-6
[6] Shibata H, Arai Y, Suzuki M, et al. Kinetics of peritectic reaction and transformation in Fe-C alloys [J]. Metall. Mater. Trans., 2000, 31B: 981
[7] Griesser S, Bernhard C, Dippenaar R. Mechanism of the peritectic phase transition in Fe-C and Fe-Ni alloys under conditions close to chemical and thermal equilibrium [J]. ISIJ Int., 2014, 54: 466
doi: 10.2355/isijinternational.54.466
[8] Chuang Y K, Reinisch D, Schwerdtfeger K. Kinetics of the diffusion controlled peritectic reaction during solidification of iron-carbon-alloys [J]. Metall. Mater. Trans., 1975, 6A: 235
[9] Fredriksson H, Stjerndahl J. Solidification of iron-base alloys [J]. Met. Sci., 1982, 16: 575
[10] Gao Z, Zhang X Z, Yao S F. Mechanism of crack formation during continuous casting of peritectic steel slabs [J]. J. Iron Steel Res., 2009, 21(10): 8
(高 仲, 张兴中, 姚书芳. 包晶钢铸坯裂纹形成机理的实验研究 [J]. 钢铁研究学报, 2009, 21(10): 8)
[11] de Andrés C G, Caballero F G, Capdevila C, et al. Application of dilatometric analysis to the study of solid-solid phase transformations in steels [J]. Mater. Charact., 2002, 48: 101
doi: 10.1016/S1044-5803(02)00259-0
[12] Guo J L, Wen G H, Pu D Z, et al. A novel approach for evaluating the contraction of hypo-peritectic steels during initial solidification by surface roughness [J]. Materials, 2018, 11: 571
doi: 10.3390/ma11040571
[13] Guo L J, Wen G H, Fu J J, et al. Influence of cooling rate on the contraction of peritectic transformation during solidification of peritectic steels [J]. Acta Metall. Sin., 2019, 55: 1311
doi: 10.11900/0412.1961.2018.00553
(郭军力, 文光华, 符姣姣等. 冷却速率对包晶钢凝固过程中包晶转变收缩的影响 [J]. 金属学报, 2019, 55: 1311)
doi: 10.11900/0412.1961.2018.00553
[14] Pu D Z, Wen G H, Fu D C, et al. Study of the effect of carbon on the contraction of hypo-peritectic steels during initial solidification by surface roughness [J]. Metals, 2018, 8: 982
doi: 10.3390/met8120982
[15] Saleem S, Vynnycky M, Fredriksson H. The influence of peritectic reaction/transformation on crack susceptibility in the continuous casting of steels [J]. Metall. Mater. Trans., 2017, 48B: 1625
[16] Phelan D, Reid M, Dippenaar R. Kinetics of the peritectic phase transformation: In-situ measurements and phase field modeling [J]. Metall. Mater. Trans., 2006, 37A: 985
[17] Matsuura K, Itoh Y, Narita T. A solid-liquid diffusion couple study of a peritectic reaction in iron-carbon system [J]. ISIJ Int., 1993, 33: 583
doi: 10.2355/isijinternational.33.583
[18] Griesser S, Reid M, Bernhard C, et al. Diffusional constrained crystal nucleation during peritectic phase transitions [J]. Acta Mater., 2014, 67: 335
doi: 10.1016/j.actamat.2013.12.018
[19] Griesser S, Bernhard C, Dippenaar R. Effect of nucleation undercooling on the kinetics and mechanism of the peritectic phase transition in steel [J]. Acta Mater., 2014, 81: 111
doi: 10.1016/j.actamat.2014.08.020
[20] Demirel Y. Nonequilibrium Thermodynamics: Transport and Rate Processes in Physical, Chemical and Biological Systems [M]. 2nd Ed., Amsterdam: Elsevier, 2007: 97
[21] Müller I. A History of Thermodynamics: The Doctrine of Energy and Entropy [M]. Berlin: Springer, 2007: 330
[22] Ueshima Y, Mizoguchi S, Matsumiya T, et al. Analysis of solute distribution in dendrites of carbon steel with δ/γ transformation during solidification [J]. Metall. Trans., 1986, 17B: 845
[23] Mittemeijer E J. Fundamentals of Materials Science: The Microstructure-Property Relationship Using Metals as Model Systems [M]. Berlin Heidelberg: Springer-Verlag, 2011: 139
[24] Jacot A, Sumida M, Kurz W. Solute trapping-free massive transformation at absolute stability [J]. Acta Mater., 2011, 59: 1716
doi: 10.1016/j.actamat.2010.11.038
[25] Liu Z C, Ren H P, Song Y Q, et al. Tutorial of Solid Metal Phase Transition [M]. Beijing: Metallurgical Industry Press, 2003: 181
(刘宗昌, 任慧平, 宋义全等. 金属固态相变教程 [M]. 北京: 冶金工业出版社, 2003: 181)
[1] WANG Fa, JIANG He, DONG Jianxin. Evolution Behavior of Complex Precipitation Phases in Highly Alloyed GH4151 Superalloy[J]. 金属学报, 2023, 59(6): 787-796.
[2] ZHANG Yuexin, WANG Jujin, YANG Wen, ZHANG Lifeng. Effect of Cooling Rate on the Evolution of Nonmetallic Inclusions in a Pipeline Steel[J]. 金属学报, 2023, 59(12): 1603-1612.
[3] PENG Zhiqiang, LIU Qian, GUO Dongwei, ZENG Zihang, CAO Jianghai, HOU Zibing. Independent Change Law of Mold Heat Transfer in Continuous Casting Based on Big Data Mining[J]. 金属学报, 2023, 59(10): 1389-1400.
[4] LI Shanshan, CHEN Yun, GONG Tongzhao, CHEN Xingqiu, FU Paixian, LI Dianzhong. Effect of Cooling Rate on the Precipitation Mechanism of Primary Carbide During Solidification in High Carbon-Chromium Bearing Steel[J]. 金属学报, 2022, 58(8): 1024-1034.
[5] GUO Dongwei, GUO Kunhui, ZHANG Fuli, ZHANG Fei, CAO Jianghai, HOU Zibing. A New Method for CET Position Determination of Continuous Casting Billet Based on the Variation Characteristics of Secondary Dendrite Arm Spacing[J]. 金属学报, 2022, 58(6): 827-836.
[6] LIU Zhongqiu, LI Baokuan, XIAO Lijun, GAN Yong. Modeling Progress of High-Temperature Melt Multiphase Flow in Continuous Casting Mold[J]. 金属学报, 2022, 58(10): 1236-1252.
[7] ZHU Yuping, Naicheng SHENG, XIE Jun, WANG Zhenjiang, XUN Shuling, YU Jinjiang, LI Jinguo, YANG Lin, HOU Guichen, ZHOU Yizhou, SUN Xiaofeng. Precipitation Behavior of W-Rich Phases in a High W-Containing Ni-Based Superalloys K416B[J]. 金属学报, 2021, 57(2): 215-223.
[8] GUO Zhongao, PENG Zhiqiang, LIU Qian, HOU Zibing. Nonuniformity of Carbon Element Distribution of Large Area in High Carbon Steel Continuous Casting Billet[J]. 金属学报, 2021, 57(12): 1595-1606.
[9] TANG Haiyan, LIU Jinwen, WANG Kaimin, XIAO Hong, LI Aiwu, ZHANG Jiaquan. Progress and Perspective of Functioned Continuous Casting Tundish Through Heating and Temperature Control[J]. 金属学报, 2021, 57(10): 1229-1245.
[10] CAI Laiqiang, WANG Xudong, YAO Man, LIU Yu. Meshless Method for Non-Uniform Heat Transfer/Solidification Behavior of Continuous Casting Round Billet[J]. 金属学报, 2020, 56(8): 1165-1174.
[11] REN Zhongming,LEI Zuosheng,LI Chuanjun,XUAN Weidong,ZHONG Yunbo,LI Xi. New Study and Development on Electromagnetic Field Technology in Metallurgical Processes[J]. 金属学报, 2020, 56(4): 583-600.
[12] WANG Xi,LIU Renci,CAO Ruxin,JIA Qing,CUI Yuyou,YANG Rui. Effect of Cooling Rate on Boride and Room Temperature Tensile Properties of β-Solidifying γ-TiAl Alloys[J]. 金属学报, 2020, 56(2): 203-211.
[13] Chunlei WU,Dewei LI,Xiaowei ZHU,Qiang WANG. Influence of Electromagnetic Swirling Flow in Nozzle on Solidification Structure and Macrosegregation of Continuous Casting Square Billet[J]. 金属学报, 2019, 55(7): 875-884.
[14] GUO Junli, WEN Guanghua, FU Jiaojiao, TANG Ping, HOU Zibing, GU Shaopeng. Influence of Cooling Rate on the Contraction of Peritectic Transformation During Solidification of Peritectic Steels[J]. 金属学报, 2019, 55(10): 1311-1318.
[15] Zibing HOU, Rui XU, Yi CHANG, Jianghai CAO, Guanghua WEN, Ping TANG. Time-Series Fluctuation Characteristics of Segregation Carbon Element Distribution Along Casting Direction in High Carbon Continuous Casting Billet[J]. 金属学报, 2018, 54(6): 851-858.