Effect of Re-Heat Rejuvenation Treatment on γ′ Microstructure of Directionally SolidifiedSuperalloy Damaged by Creep
Wenshu TANG(),Junfeng XIAO,Yongjun LI,Jiong ZHANG,Sifeng GAO,Qing NAN
1. Xi′an Thermal Power Research Institute Co., LTD., Xi′an 710054, China
Cite this article:
Wenshu TANG,Junfeng XIAO,Yongjun LI,Jiong ZHANG,Sifeng GAO,Qing NAN. Effect of Re-Heat Rejuvenation Treatment on γ′ Microstructure of Directionally SolidifiedSuperalloy Damaged by Creep. Acta Metall Sin, 2019, 55(5): 601-610.
As the core hot section components in gas turbine systems, the turbine blades are inevitably subjected to various microstructure creep damages after long time service, which seriously affect their service life. The hot isostatic pressing (HIP)-combined rejuvenation heat treatment process has been developed as a critical step in refurbishment of degraded blades with equiaxed structure, and there is a common view that HIP process has positive impact on healing creep cavities, however, the turbine blades in current gas turbine systems are widely made of directionally solidified superalloys with excellent resistance of creep voids due to the minimal number of oriented grain boundaries, which indicates that it is likely to use simple re-heat rejuvenation treatment consisting of solution and ageing treatments as a cheaper refurbishment method in recovering microctructures and properties of directionlly solidified superalloys. In this work, the interrupted creep test was conducted on directionlly solidified GTD111 superalloy to simulate the service damage of turbine blades. The effect of re-heat rejuvenation treatment on γ′ precipitates microstructure of creep degraded GTD111 superalloy and the evolution process of γ′ precipitates under different stages of re-heat rejuvenation treatment were investigated. The results show that solid solution treatment at the temperature range of 1180~1220 ℃ can effectively dissolve the coarsened and rafted primary γ′ precipitates and promote uniform precipitation of fine size secondary γ′ precipitates in the damaged alloy, meanwhile the size of secondary γ′ precipitates decreases with the increase of solution temperature and cooling rate. However, when the solid solution temperature increases to 1240 ℃, incipient melting in the interdendritic region ocurrs. High temperature ageing results in continued growth of the secondary γ′ precipitates and precipitation of tertiary γ′ precipitates. The size and cubic degree of the secondary γ′ precipitates increase with the increase of ageing temperature and soaking time. The tertiary γ′ precipitates continue to precipitate and grow during low temperature ageing process. The suitable re-heat rejuvenation parameters are 1220 ℃, 2 h, AC+1121 ℃, 2 h, AC+843 ℃, 24 h, AC. The rupture life of rejuvenated alloy under the condition of 750 ℃ and 843 MPa is up to 65 h, which is about 1.3 times of that of virgin alloy, due to its more volume fraction of duplex size γ′ precipitates after re-heat rejuvenation treatment.
Fig.1 Re-heat rejuvenation process curve of damaged GTD111 alloy (AC—air cooling)
Fig.2 Full-life creep curve and interrupted creep curve of virgin GTD111 alloy under the condition of 980 ℃ and 190 MPa (I, II and III indicate the primary, secondary and tertiary stages of the creep, respectively. “○”indicates the interrupted point on the creep curve)
Fig.3 Cross sectional OM (a, c) and SEM (b, d) images of virgin (a, b) and damaged (c, d) GTD111 alloy
Fig.4 Interdendritic microstructures of creep damaged GTD111 alloy after holding 2 h at different solution temperatures(a) 1240 ℃ (b) 1220 ℃ (c) 1200 ℃ (d) 1180 ℃
Fig.5 γ′ precipitates microstructures in dendritic core of creep damaged GTD111 alloy under different solution conditions(a) 1220 ℃, 2 h, AC (b) 1200 ℃, 2 h, AC (c) 1180 ℃, 2 h, AC (d) 1150 ℃, 2 h, AC(e) 1220 ℃, 1 h, AC (f) 1220 ℃, 3 h, AC (g) 1220 ℃, 4 h, AC (h) 1220 ℃, 2 h, FC (furnace cooling)
Fig.6 γ′ precipitates microstructures in dendritic core of creep damaged GTD111 alloy under different high temperature ageing conditions(a) 1220 ℃, 2 h, AC+1140 ℃, 2 h, AC (b) 1220 ℃, 2 h, AC+1121 ℃, 2 h, AC(c) 1220 ℃, 2 h, AC+1100 ℃, 2 h, AC (d) 1220 ℃, 2 h, AC+1050 ℃, 2 h, AC(e) 1220 ℃, 2 h, AC+1121 ℃, 1 h, AC (f) 1220 ℃, 2 h, AC+1121 ℃, 4 h, AC
Fig.7 γ′ precipitates microstructures in dendritic core of creep damaged GTD111 alloy under different low temperature ageing conditions(a) 1220 ℃, 2 h, AC+1121 ℃, 2 h, AC+790 ℃, 24 h, AC (b) 1220 ℃, 2 h, AC+1121 ℃, 2 h, AC+843 ℃, 24 h, AC(c) 1220 ℃, 2 h, AC+1121 ℃, 2 h, AC+910 ℃, 24 h, AC (d) 1220 ℃, 2 h, AC+1121 ℃, 2 h, AC+843 ℃, 48 h, AC
Fig.8 Comparation of γ′ microstucture characteristics for virgin, damaged and rejuvenated GTD111 alloys
Fig.9 Comparation graph of stress rupture properties under the condition of 750 ℃ and 843 MPa for virgin, damaged and rejuvenated GTD111 alloys
Fig.10 Schematic for γ′ phase morphology evolution of creep damaged alloy during re-heat rejuvenation treatment process
[1]
ZhangJ, LouL H, LiH. Material and processing technology of directionally solidified blade in heavy duty industrial gas turbines[J].Mater. China, 2013, 32: 12
LiH, LouL H, ShiX J, et al. γ′coarsening and creep rupture property of DZ411(DSM11) superalloy [A]. High Temperature structure Material for Power and Energy: the Proceedings of 11th China's Superalloy[C]. Beijing: Metallurgical Industry Press, 2012: 392
LeeB K, SongW Y, HanT K, et al. Change of microstructures of directionally solidified Ni base superalloy GTD-111 at high temperature[J]. Solid State Phenom., 2006, 118: 65
[5]
TawancyH M, Al-HadhramiL M. Comparative performance of turbine blades used in power generation: Damage vs. microstructure and superalloy composition selected for the application[J]. Eng. Fail. Anal., 2014, 46: 76
[6]
HosseiniS S, NateghS, EkramiA A. Microstructural evolution in damaged IN738LC alloy during various steps of rejuvenation heat treatments[J]. J. Alloys Compd., 2012, 512: 340
[7]
LvovaE, NorsworthyD. Influence of service-induced microstructural changes on the aging kinetics of rejuvenated Ni-based superalloy gas turbine blades[J]. J. Mater. Eng. Perform., 2001, 10: 299
[8]
JamesA. Review of rejuvenation process for nickel base superalloys[J]. Mater. Sci. Technol., 2001, 17: 481
[9]
LiburdiJ, LowdenP, NagyD, et al. Practical experience with the development of superalloy rejuvenation[A]. ASME Turbo Expo 2009: Power for Land, Sea, and Air[C]. Orlando: International Gas Turbine Institute, 2009, 4: 819
[10]
WangyaoP, HomkrajaiW, KrongtongV, et al. OM study of effect of HIP and heat treatments on microstructural restoration in cast nickel based superalloy, IN-738[J]. J. Met. Mater. Miner., 2017, 17: 87
[11]
ZhouY, ZhangZ, ZhaoZ H, et al. Effects of HIP temperature on the microstructural evolution and property restoration of a Ni-based superalloy[J]. J. Mater. Eng. Perform., 2013, 22: 215
[12]
WangyaoP, PolsilapaS, NisaratanapornE. The application of hot isostatic pressing process to rejuvenate serviced cast superalloy turbine blades[J]. Acta Metall. Slov., 2005, 11: 196
[13]
LindblomY. Refurbishing superalloy components for gas turbines[J]. Mater. Sci. Technol., 1985, 1: 636
[14]
BaldanA. Rejuvenation procedures to recover creep properties of nickel-base superalloys by heat treatment and hot isostatic pressing techniques[J]. J. Mater. Sci., 1991, 26: 3409
[15]
KimH I, ParkH S, KooJ M, et al. Microstructural investigation of GTD 111DS materials in the heat treatment conditions[J]. J. Mech. Sci. Technol., 2012, 26: 2019
[16]
GuoH M, ZhaoY S, ZhengS, et al. Effect of hot-isostatic pressing on microstructure and mechanical properties of second generation single crystal superalloy DD6[J]. J.Mater. Eng., 2016, 44(10): 60
RuttertB, BürgerD, RonceryL M, et al. Rejuvenation of creep resistance of a Ni-base single-crystal superalloy by hot isostatic pressing[J]. Mater. Des., 2017, 134: 418
[18]
McleanM, TiplerH R. Assessment of damage accumulation and propertiy regeneration by hot isostatic pressing and heat treatment of laboratory-tested and service exposed IN738LC[A]. Proceedings of Superalloys[C]. London: AIME, 1984: 73
[19]
PalJ, SrinivasanD, ChengE. Effect of rejuvenation heat treatment and aging on the microstructure evolution in Rene N5 single crystal Ni base superalloy blades [A]. Superalloys 2016: Proceedings of the 13th International Symposium on Superalloys[C]. Pennsylvania: TMS, 2016: 285
[20]
YaoZ, DegnanC C, JepsonM A E, et al. Effect of rejuvenation heat treatments on gamma prime distributions in a Ni based superalloy for power plant applications[J]. Mater. Sci. Tech., 2013, 29: 775
[21]
KuipersJ, WiensK, RuggieroB. Rejuvenation heat treatment of single crystal gas turbine blades [A]. ASME Turbo Expo 2017: Turbomachinery Technical Conference and Exposition[C]. Charlotte: International Gas Turbine Institute, 2017, 6: 1
[22]
CheruvuN S, SwaminathanV P, KinneyC D. Recovery of microstructure and mechanical properties of service run GTD-111 DS buckets [A]. ASME 1999 International Gas Turbine and Aeroengine Congress and Exhibition[C]. Indianapolis, Indiana: International Gas Turbine Institute, 1999, 4: 1
[23]
YooK B, LeeH S. The microstructure and mechanical properties of Ni-based superalloy after service exposure in gas turbine[J]. Mater. Sci. Forum, 2010, 654-656: 2523
[24]
LeeH S, KimD H, KimD S, et al. Microstructural changes by heat treatment for single crystal superalloy exposed at high temperature[J]. J. Alloys Compd., 2013, 561: 135
[25]
SemiatinS L, KrambR C, TurnerR E, et al. Analysis of the homogenization of a nickel-base superalloy[J]. Scr. Mater., 2004, 51: 491
[26]
NingL K, ZhengZ, JinT, et al. Effect of heat treatments on the microstructure and property of a new nickel base single crystal superalloy[J].Acta Metall. Sin., 2014, 50: 1011
BaldanA. Review progress in ostwald ripening theories and their applications to nickel-base superalloys Part I: Ostwald ripening theories[J]. J. Mater. Sci., 2002, 37: 2171
[30]
KusabirakiK, NagahamaH, WangL, et al. The growth of γ′ precipitates in nickel-base superalloys[J].Tetsu Hagané, 1990, 76: 1341
ZHANG Hongwei; CHEN Rongzhang (Beijing Institute of Aeronautical Materials;Beijing 100095)(Manuscript received 1996-03-29; in revised form 1996-08-01. THIN-WALL EFFECT OF A DIRECTIONALLY SOLIDIFIED SUPERALLOY[J]. 金属学报, 1997, 33(4): 370-374.