| Research Progress on Controlled Solidificationand Its Applications |
Guang CHEN1( ), Gong ZHENG1, Zhixiang QI1, Jinpeng ZHANG1, Pei LI1, Jialin CHENG2, Zhongwu ZHANG3 |
1 Engineering Research Center of Materials Behavior and Design, Ministry of Education, MIIT Key Laboratory of Advanced Metallic and Intermetallic Materials Technology,Nanjing University of Science and Technology, Nanjing 210094, China 2 School of Materials Engineering, Nanjing Institute of Technology, Nanjing 211167, China 3 Key Laboratory of Superlight Materials and Surface Technology, Ministry of Education, Harbin Engineering University, Harbin 150001, China |
|
Cite this article:
Guang CHEN, Gong ZHENG, Zhixiang QI, Jinpeng ZHANG, Pei LI, Jialin CHENG, Zhongwu ZHANG. Research Progress on Controlled Solidificationand Its Applications. Acta Metall Sin, 2018, 54(5): 669-681.
|
|
|
Abstract This paper reviews the study of our group on controlled solidification and its applications in recent 20 years, including melt heat treatment before solidification, semi-solid processing between liquidus and solidus, rapid progressive solidification of nonequilibrium materials, semi-solid progressive solidification, and directional heat treatment in solid phase transformation. Furthermore, a new technique of material preparation is proposed with the combination of directional solidification and directional heat treatment. In addition, an outlook of controlled solidification technology and its applications are provided.
|
|
Received: 20 December 2017
|
|
|
| Fund: Supported by National Natural Science Foundation of China (Nos.51731006, 51771093 and 51571117), China Postdoctoral Science Foundation (No.2017M620212) and National Postdoctoral Program for Innovative Talents (No.BX201700120) |
| [1] | Kermanpur A, Varahraam N, Engilehei E, et al.Directional solidification of Ni base superalloy IN738LC to improve creep properties[J]. Mater. Sci. Technol., 2000, 16: 579 | | [2] | Versnyder F I, Shank M E.The development of columnar grain and single crystal high temperature materials through directional solidification[J]. Mater. Sci. Eng., 1970, 6: 213 | | [3] | Versnyder F L, Barlow R B, Sink L W, et al.Directional solidification in the precision casting of gas-turbine parts[J]. Modern Cast, 1967, 52: 68 | | [4] | Erickson J S, Owczarski W A, Curran P W.Process speeds up directional solidification[J]. Met. Prog., 1971, 99: 58 | | [5] | Giamei A F, Tschinkel J G.Liquid metal cooling: A new solidification technique[J]. Metall. Trans., 1976, 7A: 1427 | | [6] | Chen G, Li J G, Fu H Z.Advanced unidirectional solidification processing[J]. Mater. Rev., 1999, 13(5): 5(陈光, 李建国, 傅恒志. 先进定向凝固技术[J]. 材料导报, 1999, 13(5): 5) | | [7] | Lux B, Haour G, Mollard F.Dynamic undercooling of superalloys[J]. Metall, 1981, 35: 1235 | | [8] | Li J S.On electromagnetic shaping directional solidification of stainless steel [D]. Xi'an: Northwestern Polytechnical University, 1998(李金山. 钢的电磁约束成形定向凝固研究 [D]. 西安: 西北工业大学, 1998) | | [9] | Gill S C, Zimmermann M, Kurz W.Laser resolidification of the Al-Al2Cu eutectic: The coupled zone[J]. Acta Metall. Mater., 1992, 40: 2895 | | [10] | Koohpayeh S M, Fort D, Abell J S.The optical floating zone technique: A review of experimental procedures with special reference to oxides[J]. Prog. Cryst. Growth Charact. Mater., 2008, 54: 121 | | [11] | Su Y Q, Guo J Z, Liu C, et al.Progress in theory and technology on directional solidification[J]. Spec. Cast. Nonferrous Alloys, 2006, 26: 25(苏彦庆, 郭景哲, 刘畅等. 定向凝固技术与理论研究的进展[J]. 特种铸造及有色合金, 2006, 26: 25) | | [12] | Chen G, Fu H Z.Advanced Materials Fabricated by Nonequilibrium Solidification [M]. Beijing: Science Press, 2004: 14(陈光, 傅恒志. 非平衡凝固新型金属材料 [M]. 北京: 科学出版社, 2004: 14) | | [13] | Вертман А А, Самарин А М. Методы исследования свойств металлических расплавов [М]. Москва: Наука, 1969: 197 | | [14] | Chen G, Cai Y W, Li J G, et al.Research and application of melt heat treatment[J]. J. Hebei Univ. Sci. Technol., 1998, 19(1): 6(陈光, 蔡英文, 李建国等. 熔体热处理研究及其应用[J]. 河北科技大学学报, 1998, 19(1): 6) | | [15] | Chen G, Yu J W, Sun Y C, et al.Influence of melt thermal history on the unidirectional solidification interface stability of Al-4.65% Cu alloy[J]. Chin. J. Mater. Res., 1999, 13: 497(陈光, 俞建威, 孙彦臣等. 熔体热历史对Al-Cu合金定向凝固界面稳定性的影响[J]. 材料研究学报, 1999, 13: 497) | | [16] | Chen G, Yu J W, Fu H Z.Influence of the melt heat history on the solid/liquid interface morphology evolution in unidirectional solidification[J]. J. Mater. Sci. Lett., 1999, 18: 1571 | | [17] | Chen G, Yu J W, Xie F Q, et al.Influence of melt superheat history on morphology of unidirectional directionally solidified solid/liquid interface in nickel-base superalloys[J]. Acta Metall. Sin., 2001, 37: 488(陈光, 俞建威, 谢发勤等. 熔体过热历史对Ni基高温合金定向凝固界面形态的影响[J]. 金属学报, 2001, 37: 488) | | [18] | Geng X G, Chen G, Fu H Z.The effect of melt superheat on interface morphological stability during directional solidification[J]. Acta Metall. Sin., 2002, 38: 225(耿兴国, 陈光, 傅恒志. 熔体过热对定向凝固界面形态稳定性的影响[J]. 金属学报, 2002, 38: 225) | | [19] | Geng X G, Chen G, Fu H Z.Hysteresis effect on some physical properties of melt superheat[J]. Mater. Sci. Eng., 2002, 20: 549(耿兴国, 陈光, 傅恒志. 过热合金熔体的几种物性滞后效应[J]. 材料科学与工程, 2002, 20: 549) | | [20] | Tiller W A, Jackson K A, Rutter J W, et al.The redistribution of solute atoms during the solidification of metals[J]. Acta Metall., 1953, 1: 428 | | [21] | Yang G, Kou H C, Yang J R, et al.Microstructure control of Ti-45Al-8.5Nb-(W, B, Y) alloy during the solidification process[J]. Acta Mater., 2016, 112: 121 | | [22] | Yang G, Kou H C, Liu Y, et al.Response of the solidification microstructure of a high Nb containing TiAl alloy to an isothermal high-temperature heat treatment[J]. Intermetallics, 2015, 63: 1 | | [23] | Yang G, Kou H C, Wang J, et al.Effect of melt treatment on the grain sizes of Ti-48Al-2Cr-2Nb Alloy[J]. Spec. Cast. Nonferrous Alloys, 2014, 34: 243(杨光, 寇宏超, 王军等. 熔体处理对Ti-48Al-2Cr-2Nb合金凝固组织的影响[J]. 特种铸造及有色合金, 2014, 34: 243) | | [24] | Sun G Y, Chen G, Liu C T, et al.Innovative processing and property improvement of metallic glass based composites[J]. Scr. Mater., 2006, 55: 375 | | [25] | Sun G Y, Chen G, Chen G L.Comparison of microstructures and properties of Zr-based bulk metallic glass composites with dendritic and spherical bcc phase precipitates[J]. Intermetallics, 2007, 15: 632 | | [26] | Hofmann D C, Suh J Y, Wiest A, et al.Designing metallic glass matrix composites with high toughness and tensile ductility[J]. Nature, 2008, 451: 1085 | | [27] | Hofmann D C, Suh J Y, Wiest A, et al.Development of tough, low-density titanium-based bulk metallic glass matrix composites with tensile ductility[J]. Proc. Natl. Acad. Sci. USA, 2008, 105: 20136 | | [28] | Inoue A, Kong F L, Zhu S L, et al.Production methods and properties of engineering glassy alloys and composites[J]. Intermetallics, 2015, 58: 20 | | [29] | Suryanarayana C, Inoue A.Bulk Metallic Glasses [M]. Boca Raton: CRC Press, 2010: 441 | | [30] | Cheng J L. Chen G, Xu F, et al.Correlation of the microstructure and mechanical properties of Zr-based in-situ bulk metallic glass matrix composites[J]. Intermetallics, 2010, 18: 2425 | | [31] | Zhang X L, Chen G, Du Y L.Synthesis of plastic Mg-based bulk metallic glass matrix composites by the Bridgman solidification[J]. Metall. Mater. Trans., 2012, 43A: 2604 | | [32] | Zhang X L, Sun G Y. Chen G.Improving the strength and the toughness of Mg-based bulk metallic glass by Bridgman solidification[J]. Mater. Sci. Eng., 2013, A564: 158 | | [33] | Chen G, Zhang X L, Liu C T.High strength and plastic strain of Mg-based bulk metallic glass composite containing in situ formed intermetallic phases[J]. Scr. Mater., 2013, 68: 150 | | [34] | Cheng J L.Phase selection, oxygen and mechanical behavior of Zr based bulk metallic glass composites [D]. Nanjing: Nanjing University of Science and Technology, 2012(成家林. 锆基块体金属玻璃复合材料相选择、氧含量与力学行为研究 [D]. 南京: 南京理工大学, 2012) | | [35] | Chen G, Cheng J L, Liu C T.Large-sized Zr-based bulk-metallic-glass composite with enhanced tensile properties[J]. Intermetallics, 2012, 28: 25 | | [36] | Chang K M.Tensile and impact properties of directionally solidified Fe-40Al intermetallic[J]. Metall. Mater. Trans., 1990, 21A: 3027 | | [37] | Bei H, George E P.Microstructures and mechanical properties of a directionally solidified NiAl-Mo eutectic alloy[J]. Acta Mater., 2005, 53: 69 | | [38] | Johnson D R, Masuda Y, Inui H, et al.Alignment of the TiAl/Ti3Al lamellar microstructure in TiAl alloys by growth from a seed material[J]. Acta Mater., 1997, 45: 2523 | | [39] | Bewlay B P, Lipsitt H A, Jackson M R, et al. Solidification processing of high temperature intermetallic eutectic-based alloys [J]. Mater. Sci. Eng., 1995, A192-193: 534 | | [40] | Wang Q S, Shen Y, Pan B Y, et al.Strong interplay between stripe spin fluctuations, nematicity and superconductivity in FeSe[J]. Nat. Mater., 2016, 15: 159 | | [41] | Liu Y, Li Z C, Liu W P, et al.KxFe2-ySe2 single crystals: Floating-zone growth, transport and structural properties[J]. Supercond. Sci. Technol., 2012, 25: 075001 | | [42] | Motoyama E M, Yu G, Vishik I M, et al.Spin correlations in the electron-doped high-transition-temperature superconductor Nd2-xCexCuO4±δ[J]. Nature, 2007, 445: 186 | | [43] | Jang D H, Lee W J, Sohn E, et al.Single crystal growth and optical properties of a transparent perovskite oxide LaInO3[J]. J. Appl. Phys., 2017, 121: 125109 | | [44] | Phelan W A, Koohpayeh S M, Cottingham P, et al.On the chemistry and physical properties of flux and floating zone grown SmB6 single crystals[J]. Sci. Rep., 2016, 6: 20860 | | [45] | Hatnean M C, Lees M R, Paul D M K, et al . Large, high quality single-crystals of the new Topological Kondo Insulator, SmB6[J]. Sci. Rep., 2013, 3: 3071 | | [46] | Jain A, Krautloher M, Porras J, et al.Higgs mode and its decay in a two dimensional antiferromagnet[J]. Nat. Phys., 2017, 13: 633 | | [47] | Sutter D, Fatuzzo C G, Moser S, et al.Hallmarks of Hunds coupling in the Mott insulator Ca2RuO4[J]. Nat. Commun., 2017, 8: 15176 | | [48] | Cao S X, Zhao H Z, Kang B J, et al.Temperature induced spin switching in SmFeO3 single crystal[J]. Sci. Rep., 2014, 4: 5960 | | [49] | Shen Y, Li Y D, Wo H L, et al.Evidence for a spinon Fermi surface in a triangular-lattice quantum-spin-liquid candidate[J]. Nature, 2016, 540: 559 | | [50] | Ren Y, Palstra T T M, Khomskii D I, et al. Temperature-induced magnetization reversal in a YVO3 single crystal[J]. Nature, 1998, 396: 441 | | [51] | Oh Y S, Luo X, Huang F T, et al.Experimental demonstration of hybrid improper ferroelectricity and the presence of abundant charged walls in (Ca, Sr)3Ti2O7 crystals[J]. Nat. Mater., 2015, 14: 407 | | [52] | Viskadourakis Z, Sunku S S, Mukherjee S, et al.Ferroelectricity in underdoped La-based cuprates[J]. Sci. Rep., 2015, 5: 15268 | | [53] | Baloch M M, Bhadeshia H K D H. Directional recrystallization in Inconel MA 6000 nickel base oxide dispersion strengthened superalloy[J]. Mater. Sci. Technol., 1990, 6: 1236 | | [54] | Da C Andrade E N. Preparation of single crystal wires of metals of high melting point[J]. Proc. R. Soc.: Mathemat., Phys. Eng. Sci., 1937, 163A: 16 | | [55] | Chou T S, Bhadeshia H K D H. Recrystallization temperatures in mechanically alloyed oxide-dispersion-strengthened MA956 and MA957 steels[J]. Mater. Sci. Eng., 1994, A189: 229 | | [56] | Miodownik M A, Wilkinson A J, Martin J W.On the secondary recrystallisation of MA754[J]. Acta Mater., 1998, 46: 2809 | | [57] | Sha W, Bhadeshia H K D H. Modelling of recrystallisation in mechanically alloyed materials[J]. Mater. Sci. Eng., 1997, A233: 91 | | [58] | Baker I, Li J.Directional annealing of cold-rolled copper single crystals[J]. Acta Mater., 2002, 50: 805 | | [59] | Li J, Baker I.An EBSP study of directionally recrystallized cold-rolled nickel[J]. Mater. Sci. Eng., 2005, A392: 8 | | [60] | Li J, Johns S L, Iliescu B M, et al.The effect of hot zone velocity and temperature gradient on the directional recrystallization of polycrystalline nickel[J]. Acta Mater., 2002, 50: 4491 | | [61] | Humphreys F J.A unified theory of recovery, recrystallization and grain growth, based on the stability and growth of cellular microstructures—I. The basic model[J]. Acta Mater., 1997, 45: 4231 | | [62] | Greaves M S, Base P S, Roberts W T, et al.Directional recrystallization in nickel based high temperature alloy[J]. Mater. Sci. Technol., 1996, 12: 730 | | [63] | Bhadeshia H K D H. Recrystallisation of practical mechanically alloyed iron-based and nickel-base superalloys[J]. Mater. Sci. Eng., 1997, A223: 64 | | [64] | Evens P J, Martin J W, Little E A.Secondary recrystallization of MA957 oxide dispersion strengthened by ferritic superalloy[J]. Mater. Sci. Technol., 1992, 8: 531 | | [65] | Godfrey A W, Martin J W.The effect of directional recrystallization on the low cycle fatigue response of a powder metallurgy nickel-based superalloy at elevated temperatures[J]. Mater. Sci. Eng., 1997, A222: 91 | | [66] | Duhl D N, Thompson R R.Directional structures for advanced aircraft turbine blades[J]. J. Aircraft., 1977, 14: 521 | | [67] | Cairns R L, Curwick L R, Benjamin J S.Grain growth in dispersion strengthened superalloys by moving zone heat treatments[J]. Metall. Trans., 1975, 6A: 179 | | [68] | Gessinger E H.Mechanical alloying of In-738[J]. Metall. Trans., 1976, 7A: 1203 | | [69] | Gater C A, Martin J W.Grain reorientation during zone annealing of MA6000[J]. Mater. Sci. Technol., 1996, 12: 613 | | [70] | Miodownik M A, Martin J W, Little E A.Secondary recrystallization of two oxide dispersion strengthened ferritic superalloys: MA 956 and MA 957[J]. Mater. Sci. Technol., 1994, 10: 102 | | [71] | Sha W, Bhadeshia H K D H. Directional recrystallization in mechanically alloyed oxide dispersion-strengthened metals by annealing in a moving temperature gradient[J]. J. Mater. Sci., 1995, 30: 1439 | | [72] | Marsh J M. Martin J W.Micromechanisms of texture development during zone annealing of MA 6000 extrusions[J]. Mater. Sci. Technol., 1991, 7: 183 | | [73] | Mujahid M, Martin J W.The effect of oxide particle coherency on Zener pinning in ODS superalloys[J]. J. Mater. Sci., 1994, 13: 153 | | [74] | Capdevila C, Chen Y L, Jones A R, et al.Grain boundary mobility in Fe-base oxide dispersion strengthened PM2000 alloy[J]. ISI Int., 2003, 43: 777 | | [75] | Watanabe T, Fujii H, Oikawa H, et al.Grain boundaries in rapidly solidified and annealed Fe-6.5 mass% Si polycrystalline ribbons with high ductility[J]. Acta Metall., 1989, 37: 941 | | [76] | Tsujimoto T, Matsui T, Suzuki T, et al.Evolution of high aspect ratio grains in a TiAl-based alloy by directional grain growth[J]. Intermetallics, 2001, 9: 97 | | [77] | Zhang Z W, Chen G, Chen G L.Dynamics and mechanism of columnar grain growth of pure iron under directional annealing[J]. Acta Mater., 2007, 55: 5988 | | [78] | Zhang Z W, Chen G L, Chen G.Microstructural evolution of commercial pure iron during directional annealing[J]. Mater. Sci. Eng., 2006, A422: 241 | | [79] | Zhang Z W, Chen G L, Chen G.The effect of drawing velocity and phase transformation on the structure of directionally annealed iron[J]. Mater. Sci. Eng., 2006, A434: 58 | | [80] | Zhang Z W, Chen G L, Chen G. The effect of crystallographic texture on columnar grain growth in commercial pure iron during directional annealing [J]. Mater. Sci. Eng., 2006, A435-436: 573 | | [81] | Ruo Z R, Liu Y, Deng Q Q, et al.Phase field study of the formation of columnar-grain structure during directional annealing[J]. Guangxi Phys., 2013, 34(1): 9(罗志荣, 刘瑶, 邓芊芊等. 相场方法研究定向退火条件下柱状晶粒的形成过程[J]. 广西物理, 2013, 34(1): 9) | | [82] | Ruo Z R, Gao Y J, Deng Q Q, et al.Phase field simulation of formation and continuous propagation of columnar grain structure during directional annealing[J]. Chin. J. Nonferrous Met., 2014, 24: 1778(罗志荣, 高英俊, 邓芊芊等. 定向退火条件下柱状晶形成及连续扩展的相场模拟[J]. 中国有色金属学报, 2014, 24: 1778) | | [83] | Zhang Z W, Chen G, Bei H B, et al.Directional recrystallization and microstructures of an Fe-6.5wt%Si alloy[J]. J. Mater. Res., 2009, 24: 2654 | | [84] | Zhang Z W, Chen G, Bei H, et al.Improvement of magnetic properties of Fe-6.5wt%Si by directional recrystallization[J]. Appl. Phys. Lett., 2008, 93: 191908 | | [85] | Bertram A, Olschewski J.Anisotropic creep modelling of the single crystal superalloy SRR99[J]. Comput. Mater. Sci., 1996, 5: 12 | | [86] | Burgers W G.On the process of transition of the cubic-body-centered modification into the hexagonal-close-packed modification of zirconium[J]. Physica, 1934, 1: 561 | | [87] | Chen G, Peng Y B, Zheng G, et al.Polysynthetic twinned TiAl single crystals for high-temperature applications[J]. Nat. Mater., 2016, 15: 876 | | [88] | Bewlay B P, Weimer M, Kelley T, et al.The science, technology, and implementation of TiAl alloys in commercial aircraft engines [A]. Materials Research Society Symposium Proceedings [C]. Pittsburgh: Materials Research Society Press, 2013: 49 | | [89] | Pollock T M.Alloy design for aircraft engines[J]. Nat. Mater., 2016, 15: 809 | | [90] | Inui H, Oh M H, Nakamura A, et al.Room-temperature tensile deformation of polysynthetically twinned (PST) crystals of TiAl[J]. Acta Metall. Mater., 1992, 40: 3095 | | [91] | Yamaguchi M, Inui H, Ito K.High-temperature structural intermetallics[J]. Acta Mater., 2000, 48: 307 | | [92] | Kim M C, Oh M H, Lee J H, et al. Composition and growth rate effects in directionally solidified TiAl alloys [J]. Mater. Sci. Eng., 1997, A239-240: 570 | | [93] | Jung I S, Kim M C, Lee J H, et al.High temperature phase equilibria near Ti-50 at% Al composition in Ti-Al system studied by directional solidification[J]. Intermetallics, 1999, 7: 1247 | | [94] | Jung I S, Jang H S, Oh M H, et al. Microstructure control of TiAl alloys containing β stabilizers by directional solidification [J]. Mater. Sci. Eng., 2002, A329-331: 13 | | [95] | Lapin J, Gabalcová Z, Pelachová T.Effect of Y2O3 crucible on contamination of directionally solidified intermetallic Ti-46Al-8Nb alloy[J]. Intermetallics, 2011, 19: 396 | | [96] | Lapin J, Ondrú? L, Nazmy M.Directional solidification of intermetallic Ti-46Al-2W-0.5 Si alloy in alumina moulds[J]. Intermetallics, 2002, 10: 1019 | | [97] | Lapin J, Gabalcová Z.Solidification behaviour of TiAl-based alloys studied by directional solidification technique[J]. Intermetallics, 2011, 19: 797 | | [98] | Schütze M.High-temperature alloys: Single-crystal performance boost[J]. Nat. Mater., 2016, 15: 823 |
|
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|