| SIZE EFFECTS ON THE STRENGTH OF METALS |
HUANG Xiaoxu( ) |
| Danish-Chinese Center for Nanometals, Department of Wind Energy, Technical University of Denmark, DK-4000 Roskilde, Denmark |
|
Cite this article:
HUANG Xiaoxu. SIZE EFFECTS ON THE STRENGTH OF METALS. Acta Metall Sin, 2014, 50(2): 137-140.
|
|
|
Abstract The grain size effect and the specimen size effect on the strength of metals are briefly reviewed with respect to their history and current status of research. It is revealed that the fundamental strengthening mechanisms responsible for these two types of size effect are to increase the resistance to dislocation motion and to dislocation generation, respectively. It is shown that both strengthening mechanisms take place in some nanostructured metals, which leads to a suggestion to use these two mechanisms for optimizing the strength and ductility of nanostructured metals. This suggestion is verified by some results obtained in nanostructured pure aluminum.
|
|
Received: 08 January 2014
|
|
|
| Fund: Supported by Danish National Research Foundation (No.DNRF86-5) and National Natural Science Foundation of China ( No.51261130091) |
| [1] |
Hall E O. Proc Phys Soc, 1951; 64B: 747
|
| [2] |
Petch N J. J Iron Steel Inst, 1953; 174: 25
|
| [3] |
Armstrong R W, Codd I, Douthwaite R M, Petch N J. Philos Mag, 1962; 7: 45
|
| [4] |
Takaki S. Mater Sci Forum, 2010; 654-656: 11
|
| [5] |
Eshelby J D, Frank F C, Nabarro F R N. Philos Mag, 1951; 42: 351
|
| [6] |
Li J C M. Trans TMS-AIME, 1963; 227: 239
|
| [7] |
Conrad H, Jung K. Mater Sci Eng, 2005; A391: 272
|
| [8] |
Dunstan D J, Bushby A J. Inter J Plast, 2014; 53: 56
|
| [9] |
Schiøtz J, Jacobsen K W. Science, 2003; 301: 1357
|
| [10] |
Kamikawa N, Huang X, Tsuji N, Hansen N. Acta Mater, 2009; 57: 4198
|
| [11] |
Hansen N. Acta Metall, 1977; 25: 863
|
| [12] |
Brenner S S. J Appl Phys, 1956; 27: 1484
|
| [13] |
Brenner S S. J Appl Phys, 1957; 28: 1023
|
| [14] |
Uchic M D, Shade P A, Dimiduk D M. Annu Rev Mater Res, 2009; 39: 361
|
| [15] |
Sudharshan Phani P, Johanns K E, George E P, Pharr G M. Acta Mater, 2013; 61: 2489
|
| [16] |
Johanns K E, Sedlmayr A, Sudharshan Phani P, Mönig R, Kraft O, George E P, Pharr G M. J Mater Res, 2012; 27: 508
|
| [17] |
Dehm G. Prog Mater Sci, 2009; 54: 664
|
| [18] |
Shan Z W, Mishra R K, Asif S A S, Warren O L, Minor A M. Nat Mater, 2008; 7: 115
|
| [19] |
Sudharshan Phani P, Johanns K E, Duscher G, Gali A, George E P, Pharr G M. Acta Mater, 2011; 59: 2172
|
| [20] |
Dunstan D J, Bushby A J. Int J Plast, 2013; 40: 152
|
| [21] |
Huang X, Tsuji N, Hansn N. Science, 2006; 312: 249
|
| [22] |
Huang X, Kamikawa N, Hansen N. Mater Sci Eng, 2008; A483-484 : 102
|
| [23] |
Huang X, Kamikawa N, Hansen N. J Mater Sci, 2008; 43: 7397
|
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|