					Cite this article:
						|  |  
    					|  |  
    					| COMPONENT SELECTION AND TECHNOLOGICAL OPTIMIZATION OF THICK WALL 1Cr13 TUBE USED AS CONTROL POLES IN NUCLEAR POWER STATION DRIVING MACHINES |  
						| DU Xiangyuan, SU Guoyue |  
						| Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016 |  
						|  |  
					
			      DU Xiangyuan SU Guoyue. COMPONENT SELECTION AND TECHNOLOGICAL OPTIMIZATION OF THICK WALL 1Cr13 TUBE USED AS CONTROL POLES IN NUCLEAR POWER STATION DRIVING MACHINES. Acta Metall Sin, 2011, 47(9): 1155-1158.	
				 
					
						| 
								
									|  
          
          
            
              
				
												  
													
													    |  |  
														| Abstract  The control poles for driving machine in the built and building nuclear power station are made of thick wall 1Cr13 tubes which all depend on overseas importation. With the fast development of domestic nuclear power stations and the need with coming export, as one of the key parts of driving machines, the 1Cr13 tubes used as control poles should be finished in our country. By optimizing the contents of C, Ni, Cr, H, O and N etc., and adjusting the technology of cold rolling, the cracking problem of 1Cr13 tube as control poles during machining is avoided and favorable surface quality is also obtained. The mechanical properties of  finished tubes reach the technical request after proper heat--treatment. |  
															| Received:  06 April 2011 |  
            
									            
									               
																												  
															| [1] Lu S Y, Zhang T K, Kang X F, Yang C Q, Wang X. Stainless Steel, Beijing: Atomic Energy Press, 1995: 23(陆世英, 张廷凯, 康喜范, 杨长强, 王熙. 不锈钢. 北京: 原子能出版社, 1995: 23)[2] Cui Z Q. Metal and Heat Treatment. Beijing: Mechanical Industry Press, 1988: 285(崔忠圻. 金属学与热处理. 北京: 机械工业出版社, 1988: 285)[3] Barid J D. Met Mater, 1971; 4: 1[4] Bao J. Spec Steel Technol, 2006; 11(2): 20(鲍进. 特钢技术, 2006; 11(2): 20)[5] Li H S. Spec Steel Technol, 2006; 12(4): 25(李海生. 特钢技术, 2006; 12(4): 25)[6] Zhang Y T. Manual for Heat Treatment Technician. Beijing: Mechanical Industry Press, 2005: 89(张玉庭. 热处理技师手册. 北京: 机械工业出版社, 2005: 89)[7] Woodfine B C. J Iron Steel Inst, 1953; 173: 229 |  
             
								                
															
																| 
																																																																									
																				| No Suggested Reading articles found! |  |  
             
												
											    	
											        	|  | Viewed |  
											        	|  |  |  
												        |  | Full text 
 | 
 
 |  
												        |  |  |  
												        |  | Abstract 
 | 
 |  
												        |  |  |  
												        |  | Cited |  |  
												        |  |  |  |  
													    |  | Shared |  |  
													    |  |  |  |  
													    |  | Discussed |  |  |  |  |