EFFECT OF Cr ADDITION ON TRANSFORMATION AND CYCLIC DEFORMATION CHARACTERISTICS OF Ti-Ni SHAPE MEMORY ALLOY |
YANG Jun1), HE Zhirong1), WANG Fang2), WANG Yongshan1) |
1) School of Materials Science and Engineering, Shaanxi University of Technology, Hanzhong 723003
2) Library, Shaanxi University of Technology, Hanzhong 723003 |
|
Cite this article:
YANG Jun HE Zhirong WANG Fang WANG Yongshan. EFFECT OF Cr ADDITION ON TRANSFORMATION AND CYCLIC DEFORMATION CHARACTERISTICS OF Ti-Ni SHAPE MEMORY ALLOY. Acta Metall Sin, 2011, 47(2): 157-162.
|
Abstract The effect of Cr addition on the transformation and the cyclic deformation characteristics in 550℃ annealed Ti-50.8Ni shape memory alloy (SMA) were investigated by differential scanning calorimetry (DSC) and tensile test. The B2→R→M/M→B2 type reversiable transformation occurred in Ti-50.8Ni alloy upon cooling/heating. After the addition of 0.3%Cr in Ti-50.8Ni alloy, the transformation type for Ti-50.8Ni-0.3Cr alloy was B2→R→M/M→R→B2, and the transformation temperatures decreased significantly. At room temperature, the phase composition was parent phase B2 for both Ti-50.8Ni and Ti-50.8Ni-0.3Cr alloys, while the former showed shape memory effect; the latter showed superelasticity. With increasing cyclic deformation number n, Ti-50.8Ni alloy evolved from shape memory effect to linear superelasticity, and its stress inducing martensitic critical stress and the accumulation residual strain increased rapidly; while Ti-50.8Ni-0.3Cr alloy evolved from incomplete superelastic to complete superelastic, and the stress-strain curve shape was stable. With increasing n, the superelastic residual strain εr decreased and the superelastic strain recovery ratio ηs of Ti-50.8Ni alloy increased, while the εr and ηs in Ti-50.8Ni-0.3Cr alloy kept at lower and higher values, respectively. The superelastic of Ti-50.8-0.3Cr alloy was stable.
|
Received: 10 August 2010
|
Fund: Supported by Natural Science Foundation of Shaanxi Province (No.2009JM6010) and Special Scientific Research Program Founded by Shaanxi Provincial Education Department (No.09JK375) |
[1] Otsuka K, Wayman C M. Shape Memory Materials. Cambridge: Cambridge University Press, 1998: 220[2] He Z R, Wang F, Zhou J E. Heat Treat Met, 2006; 31(9): 17(贺志荣, 王芳, 周敬恩. 金属热处理, 2006; 31(9): 17)[3] Kim J I, Miyazaki S. Metall Mater Trans, 2005; 36A: 3301[4] He Z R, Wang F. Acta Metall Sin, 2010; 46: 329(贺志荣, 王 芳. 金属学报, 2010; 46: 329)[5] He Z R, Wang F, Wang Y S, Xia P J, Yang B. Acta Metall Sin, 2007; 43: 1293(贺志荣, 王芳, 王永善, 夏鹏举, 杨波. 金属学报, 2007; 43: 1293)[6] Liu A L, Sui J H, Lei Y C, Cai W, Gao Z Y, Zhao L C. J Mater Sci, 2007; 42: 5791[7] Adharapurapu R R, Vecchio K S. Exp Mech, 2007; 47: 365[8] Soga Y, Doi H, Yoneyama T. Mater Med, 2000; 11: 695[9] Chen F. Mech Eng, 2009; 10: 21(陈芳. 机械工程师, 2009; 10: 21)[10] Shang Z J, Wang Z M, Yin G S, Zheng B Y. Rare Met Mater Eng, 2009; 38: 460(商泽进, 王忠民, 尹冠生, 郑碧玉. 稀有金属材料与工程, 2009; 38: 460)[11] Zhang X P, Liu H Y, Yuan B, Zhang Y P. Mater Sci Eng, 2008; A481: 170[12] Carl P F, Alicia M O, Jeffrey T, Ken G, Hans J M. Metall Mater Trans, 2004; 35A: 2013[13] Cho G B, Kim Y H, Hur S G, Yu C A, Nam T H. Met Mater Int, 2006; 12: 181[14] He Z R, Wang F. Acta Metall Sin, 2008; 44: 23(贺志荣, 王芳. 金属学报, 2008; 44: 23)[15] Tahara M, Kim H Y, Hosoda H, Miyazaki S. Acta Mater, 2009; 57: 2461[16] Miyazaki S, Imai T, Igo Y, Otsuka K. Metall Trans, 1986; 17A: 115[17] Eucken S, Duering T W. Acta Metall, 1989; 37: 2245[18] Zhao L C, Cai W, Zheng Y F. Shape Memory Effect and Superelasticity in Alloys. Beijing: National Defense Industry Press, 2002: 121(赵连城, 蔡伟, 郑玉峰. 合金的形状记忆效应与超弹性. 北京:国防工业出版社, 2002: 121) |