Acta Metall Sin  2009, Vol. 45 Issue (8): 919-923    DOI:
论文 Current Issue | Archive | Adv Search |
EFFECT OF AGING TIME ON ELECTROCHEMICAL CORROSION BEHAVIOR OF 2101 DUPLEX STAINLESS STEEL
HAN Dong 1; JIANG Yiming 1; DENG Bo 1; ZHANG Lihua 1; ZHANG Wei 2; LI Jin 1
1. Department of Material Science; Fudan University; Shanghai 200433
2. Institute of Stainless Steel; Baosteel Co.; Ltd; Shanghai 201900
Cite this article: 

HAN Dong JIANG Yiming DENG Bo ZHANG Lihua ZHANG Wei LI Jin. EFFECT OF AGING TIME ON ELECTROCHEMICAL CORROSION BEHAVIOR OF 2101 DUPLEX STAINLESS STEEL. Acta Metall Sin, 2009, 45(8): 919-923.

Download:  PDF(1146KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  

Duplex stainless steels (DSS) are extensively applied in many fields such as petroleum industry, petrochemistry, desalination service and paper–making industry. They are characterized by a two–phase structure, offering an attractive combination of corrosion resistance and mechanical properties. Their best general properties are obtained by keeping approximately equal volume fractions of austenite and ferrite but averting third harmful phases, such as σ, γ2, χ, carbide and nitride, to be precipitated. These harmful phases can be formed from ferrite when DSS are welded or worked at improper high temperatures. Recently, a kind of economical DSS 2101 of typical composition Fe– 21.4Cr–1.2Ni–5.7Mn–0.23N–0.31Mo was developed and shows a wide application potential due to its higher yield strength, better pitting corrosion resistance and lower cost than traditional 304 austenite steel. However, limited research has been dedicated to studying the microstructure and mechanical properties of DSS 2101. Especilly research n the nature of precipitations and their effects on mechanicl properties in DSS 101 ws stilacking in comparison to many researches on the recipitations in DSS 2205 and DSS 2507. In the present work, it aims at investigating how the precipitations can affect the corrosion resistance of DSS 2101. Pitting corrosion resistance of samples aged at 700 ℃ in 1 mol/L NaCl solution was evaluated by potentiodynamic polarization curve test. The electrochemical potentiokinetic reactivation (EPR) test was also used to evaluate the degree of sensitization to intergranular corrosion. Scanning electron microscopy (SEM) and optical microscopy (OM) were used to observe the surface morphology after electrochemical tests. The results demonstrate that both the resistance to pitting (Eb) and intergranular corrosion (Ra) decreases with aging time increasing. Pitting nucleates preferentially in the ferrite phase for the solution–annealed sample, while the initiation of pitting corrosion takes place around Cr2N, in the newly formed secondary austenite for the aged specimen. EPR tetconducted at room temperature are able to detect the sensitization to Ra due to Cr2N precipitation. With increasing aging time, more Cr2N particles are precipitated at phase interfaces and grain boundaries, causing a continuous decrease of resistance to intergranular corrosion.

Key words:  duplex stainless steel (DSS)      aging      pitting coosion      itergranular corroson      secondary austenite phase     
Received:  23 December 2008     
ZTFLH: 

TG172.8

 
Fund: 

Supported by National Natural Science Foundation of China (No.50871031), Chinese National Science and Technology Infrastructure Platforms Construction Project (No.2005DKA10400–Z13), Shanghai Science and Technology Development Funds (No.0725nm004) and Shanghai Leading Academic Discipline Project (No.B113)

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2009/V45/I8/919

[1] Westin E M, Brolun B, Hertzman S. Steel Res Int, 2008; 79: 473
[2] Olsson J, Snis M. Desalination, 2007; 205: 104
[3] Fu Y, Lin C J, Cai W D. Act Metall Sin, 2005; 41: 302
(付燕, 林昌健, 蔡文达. 金属学报, 2005; 41: 302)
[4] Chen T H, Wang K L, Yang J R. Mater Sci Eng, 2002; A338: 259
[5] Garfias–mesias L F, Sykes J M. Corros Sci, 1999; 41: 959
[6] Wang J, Uggowitzer P J, Magdowski R, Speidel M O. Scr Mater, 1999; 40: 123
[7] Merello R, Botana F J, Botella J, Maters M V, Marcos M. Corros Sci, 2003; 45: 909
[8] Zhang W, Jiang L Z, Hu J C, Song H M. Mater Charact, 2009; 60: 50
[9] Michael P, Oliver S, Thomas G. Mater Charact, 2007; 58: 65
[10] Henrik S, Rolf S. Mater Sci Eng, 2007; A444: 271
[11] Loljas M, Johansson P. Mater Technol, 2008; 79: 466
[12] Gui L F. Handbook of Materials Testing for Mechanical Engineering. Shenyang: Liaoning Science and Technology Publishing House, 2002: 175
(桂立丰. 机械工程材料测试手册, 沈阳: 辽宁科学技术出版社, 2002: 175)
[13] Zhang W, Jiang L Z, Hu J C, Song H M. Mater Sci Eng, 2008; A497:501
[14] Moayed M H, Newman R C. Corros Sci, 2006; 48: 1004
[15] Xiong H, Lin H X, Zhao G X. Nat Gas Oil, 2007; 25(5):33
(熊惠, 林红先, 赵国先. 天然气与石油, 2007; 25(5): 33)

[1] ZHANG Leilei, CHEN Jingyang, TANG Xin, XIAO Chengbo, ZHANG Mingjun, YANG Qing. Evolution of Microstructures and Mechanical Properties of K439B Superalloy During Long-Term Aging at 800oC[J]. 金属学报, 2023, 59(9): 1253-1264.
[2] LIANG Kai, YAO Zhihao, XIE Xishan, YAO Kaijun, DONG Jianxin. Correlation Between Microstructure and Properties of New Heat-Resistant Alloy SP2215[J]. 金属学报, 2023, 59(6): 797-811.
[3] LIU Manping, XUE Zhoulei, PENG Zhen, CHEN Yulin, DING Lipeng, JIA Zhihong. Effect of Post-Aging on Microstructure and Mechanical Properties of an Ultrafine-Grained 6061 Aluminum Alloy[J]. 金属学报, 2023, 59(5): 657-667.
[4] WANG Bin, NIU Mengchao, WANG Wei, JIANG Tao, LUAN Junhua, YANG Ke. Microstructure and Strength-Toughness of a Cu-Contained Maraging Stainless Steel[J]. 金属学报, 2023, 59(5): 636-646.
[5] WANG Changsheng, FU Huadong, ZHANG Hongtao, XIE Jianxin. Effect of Cold-Rolling Deformation on Microstructure, Properties, and Precipitation Behavior of High-Performance Cu-Ni-Si Alloys[J]. 金属学报, 2023, 59(5): 585-598.
[6] MA Guonan, ZHU Shize, WANG Dong, XIAO Bolv, MA Zongyi. Aging Behaviors and Mechanical Properties of SiC/Al-Zn-Mg-Cu Composites[J]. 金属学报, 2023, 59(12): 1655-1664.
[7] GONG Xiangpeng, WU Cuilan, LUO Shifang, SHEN Ruohan, YAN Jun. Effect of Natural Aging on Artificial Aging of an Al-2.95Cu-1.55Li-0.57Mg-0.18Zr Alloy at 160oC[J]. 金属学报, 2023, 59(11): 1428-1438.
[8] GENG Yaoxiang, TANG Hao, XU Junhua, ZHANG Zhijie, YU Lihua, JU Hongbo, JIANG Le, JIAN Jianglin. Formability and Mechanical Properties of High-Strength Al-(Mn, Mg)-(Sc, Zr) Alloy Produced by Selective Laser Melting[J]. 金属学报, 2022, 58(8): 1044-1054.
[9] GAO Chuan, DENG Yunlai, WANG Fengquan, GUO Xiaobin. Effect of Creep Aging on Mechanical Properties of Under-Aged 7075 Aluminum Alloy[J]. 金属学报, 2022, 58(6): 746-759.
[10] REN Ping, CHEN Xingpin, WANG Cunyu, YU Feng, CAO Wenquan. Effects of Pre-Strain and Two-Step Aging on Microstructure and Mechanical Properties of Fe-30Mn-11Al-1.2C Austenitic Low-Density Steel[J]. 金属学报, 2022, 58(6): 771-780.
[11] CHEN Shenghu, RONG Lijian. Oxide Scale Formation on Ultrafine-Grained Ferritic-Martensitic Steel During Pre-Oxidation and Its Effect on the Corrosion Performance in Stagnant Liquid Pb-Bi Eutectic[J]. 金属学报, 2021, 57(8): 989-999.
[12] ZHOU Hongyu, RAN Minrui, LI Yaqiang, ZHANG Weidong, LIU Junyou, ZHENG Wenyue. Effect of Diamond Particle Size on the Thermal Properties of Diamond/Al Composites for Packaging Substrate[J]. 金属学报, 2021, 57(7): 937-947.
[13] ZHU Shize, WANG Dong, WANG Quanzhao, XIAO Bolv, MA Zongyi. Influence of Cu Content on the Negative Effect of Natural Aging in SiC/Al-Mg-Si-Cu Composites[J]. 金属学报, 2021, 57(7): 928-936.
[14] CHEN Junzhou, LV Liangxing, ZHEN Liang, DAI Shenglong. Precipitation Strengthening Model of AA 7055 Aluminium Alloy[J]. 金属学报, 2021, 57(3): 353-362.
[15] ZHANG Le,WANG Wei,M. Babar Shahzad,SHAN Yiyin,YANG Ke. Fabrication and Properties of Novel Multi-LayeredMetal Composites[J]. 金属学报, 2020, 56(3): 351-360.
No Suggested Reading articles found!