Please wait a minute...
Acta Metall Sin  2008, Vol. 44 Issue (9): 1090-1094     DOI:
Research Articles Current Issue | Archive | Adv Search |
Effects of humidity on domain switching in BaTiO3 single crystals under sustained electric field
;;;;
北京科技大学
Cite this article: 

. Effects of humidity on domain switching in BaTiO3 single crystals under sustained electric field. Acta Metall Sin, 2008, 44(9): 1090-1094 .

Download:  PDF(4300KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Effects of humidity on domain switching behaviors in BaTiO3 single crystals under electric field were investigated by polarized light microscopy (PLM). It was found that the humidity has different effect on different domain configurations. The low humidity has no effect on both a-b domain configuration and b-c domain configuration under fields. However, the high humidity can promote b domain switch to c domain under electric fields. The effects were explained by different adsorption of polar H2O molecules on different domain areas in humidity conditions.
Key words:  Domain switching      Humidity      BaTiO3 single crystals      sustained external field      
Received:  14 January 2008     
ZTFLH:  N073  
  N079  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2008/V44/I9/1090

[1]Weitzing H,Schneider G A,Steffens J,Hammer M,Hoff- mann M J.J Eur Ceram Soc,1999;19:1333
[2]Lynch C S.Acta Mater,1996;44:4137
[3]Njiwa A B K,Lupascu D C,Rodel J.Acta Mater,2004; 52:4919
[4]Wang F,Su Y J,He J Y,Qiao L J,Chu W Y.Scr Mater, 2006;54:201
[5]Shang J K,Tan X.Acta Mater,2001;49:2993
[6]Jiang Y J,Fang D N,Li F X.Appl Phys Left,2007;90: 222907
[7]Tan X L,Xu Z K,Shang J K.Mater Sci Eng,2001;A314: 157
[8]Hackemann S,Pfeiffer W.J Eur Ceram Soc,2003;23:141
[9]Wang Y,Chu W Y,Gao K W,Su Y J,Qiao L J.Appl Phys Lett,2003;82:1583
[10]Su Y J,Wang Y,Chu W Y,Gao K W,Qiao L J.Acta Mater,2004;52:3753
[11]Zhao X W,Chu W Y,Su Y J,Li J X,Gao K W,Qiao L J.Acta Metall Sin,2006;42:13 (赵显武,褚武扬,宿彦京,李金许,高克玮,乔利杰.金属学报,2006;42:13)
[12]Merz W J.Phys Rev,1954;95:690
[13]Little E A.Phys Rev,1955;98:978
[14]Munoz Saldana J,Schneider G A,Eng L M.Surf Sci, 2001;480:L402
[15]Hirth J P.Metall Trans,1980;11A:861
[16]Chu W Y,Qiao L J,Chen Q Z,Gao K W.Fracture and Environmental Fracture.Beijing:Science Press,2000:36 (褚武扬,乔利杰,陈奇志,高克玮.断裂与环境断裂.北京:科学出版社,2000:36)
[1] Dongyu HE,Yuxin LIU. PFM Study of the 90° Step-by-Step Domain Switching and the Temperature Effect in 0.8PbTiO3-0.2Bi(Mg0.5Ti0.5)O3 Ferroelectric Thin Film[J]. 金属学报, 2019, 55(3): 325-331.
[2] JIANG Bing XING Xianran GUO Zhimeng. CRACK PROPAGATION AND DOMAIN SWITCHING IN BaTiO3 SINGLE CRYSTALS UNDER EXTERNAL FIELD[J]. 金属学报, 2011, 47(5): 605-610.
[3] ZHAO Xianwu CHU Wuyang QIAO Lijie. DOMAIN SWITCHING AND THE CHANGE IN INDENTATION CRACKS FOR BaTiO3 SINGLE CRYSTAL UNDER THE ELECTRIC FIELD PERPENDICULAR TO THE POLARIZATION[J]. 金属学报, 2010, 46(3): 340-345.
[4] ZHAO Xianwu CHU Wuyang QIAO Lijie. SUB–CRITICAL CRACK GROWTH IN AIR AND DOMAIN SWITCHING FOR BaTiO3 SINGLE CRYSTAL UNDER CONSTANT DEFLECTION[J]. 金属学报, 2010, 46(2): 167-171.
[5] ;. THREE DIMENSIONS PHASE FIELD SIMULATION OF MECHATRONIC COUPLE FOR FERROELECTRIC MATERIALS[J]. 金属学报, 2008, 44(8): 927-932 .
[6] ZHANG Sa; CHENG Xuan; ZHANG Ying. In Situ Raman Spectroscopy Observation for Domain Switching of Ferroelectric Ceramics[J]. 金属学报, 2005, 41(6): 663-668 .
[7] WANG Ruimin; CHU Wuyang; SU Yanjing; GAO Kewei; QIAO Lijie. Domain switching and indentation crack propagating in BaTiO3 single crystal induced by etching[J]. 金属学报, 2005, 41(3): 297-301 .
No Suggested Reading articles found!