| CELLULAR AUTOMATON SIMULATION STUDY ON NANOGRAIN GROWTH BASED ON THERMODYNAMIC FUNCTIONS OF NANOCRYSTALLINE |
| ;Xiaoyan SONG;; |
| 北京工业大学 |
|
Cite this article:
Xiaoyan SONG. CELLULAR AUTOMATON SIMULATION STUDY ON NANOGRAIN GROWTH BASED ON THERMODYNAMIC FUNCTIONS OF NANOCRYSTALLINE. Acta Metall Sin, 2008, 44(4): 495-500 .
|
|
|
Abstract Materials modeling and simulation have been widely used in studies on microstructure evolutions of conventional polycrystalline materials, but very few reports for uses in nanocrystalline materials. Based on our previous analytical model that describes the thermodynamic functions of nanograin boundaries (X.Song, J.Zhang, L.Li, et al, Acta Mater. 2006, 54(20), 5541-5550), the thermodynamic features of nanograin boundaries were introduced into the Cellular Automaton algorithm. With the hybrid model, the quantitative and visual simulations of nanograin growth have been carried out in this article. The simulation results show that the nanograin growth kinetics is different from the normal grain growth behavior in conventional polycrystalline materials. The nanograin growth exponent, n, is not a constant as in the polycrystalline metals which equals 2, but changes with the growing process, which has a range of 1.706.59. The excess free energy of the nanograin boundaries is the driving force for nanograin growth, which is closely related with the grain size. The simulation studies prove that the thermodynamic features of nanograin boundaries strongly affect the energy state of the nanocrystalline materials hence the nanograin growth kinetics, as a result of the nanoscale effect. It is considered by the authors that the simulations of nanograin growth should take into account the thermodynamic features of nanocrystalline materials.
|
|
Received: 02 August 2007
|
|
|
[1]Zhang L D,Mu J M.Nano Materials and Nano Structure. Beijing:Science Press,2001:5,61 (张立德,牟季美.纳米材料和纳米结构.北京:科学出版社,2001:5,61) [2]Wen Y H,Zhou F X,Liu Y W.Adv Mech,2001;31:47 (文玉华,周富信,刘曰武.力学进展,2001;31:47) [3]Raabe D,translated by Xiang J Z,Wu X H.Compu- tational Materials Science.Beijing:Chemical Industry Press,2002:8 (Raabe D著;项金钟,吴兴惠译.计算材料学.北京:化学工业出版社,2002:8) [4]Srolovitz D J,Grest G S,Anderson M P.Acta Metall,1985; 33:2233 [5]Song X Y,Liu G Q.Scr Mater,1998;38:1691 [6]Raabe D.Acta Mater,2000;48:1617 [7]Yu Q,Esche S K.Mater Lett,2003;57:4622 [8]Liu Z J,Shen Y G.Acta Mater,2004;52:729 [9]Fan D,Chen L Q.Acta Mater,1997;45:611 [10]Yoshihiro S,Yoshiyuki S,Hidehiro O.Comput Mater Sci, 2007;40:40 [11]Raabe D.Annu Rev Mater Res,2002;32:53 [12]Li Q,Li D Z,Qian B N.Acta Phys Sin,2004;53:3477 (李强,李殿中,钱百年.物理学报,2004;53:3477) [13]Raghavan S,Sahay S S.Mater Sci Eng,2007;A445-446: 203 [14]Song X Y,Gao J P,Zhang J X.Acta Phys Sin,2005;54: 1313 (宋晓艳,高金萍,张久兴.物理学报,2005;54,1313) [15]Song X Y,Yang K Y,Zhang J X.J Nanosci Nanotechnol, 2005;5:2155 [16]Song X Y,Li L M,Zhang J X,Yang K Y.Acta Mater, 2006;54:5541 [17]Neumann J V.Theory of Self-reproducing Automata.Ur- bana,Champaign:University of Illinois Press,1966:1 [18]Hesselbarth H W,Gobel I R.Acta Metall Mater,1991; 39:2135 [19]Fecht J H.Phys Rev Lett,1990;65:610 [20]Wagner M.Phys Rev,1992;45B:635 [21]Meng Q P,Rong Y H,Xu Z Y.Sci Chin,2002;32E:457 (孟庆平,戎永华,徐祖耀.中国科学,2002;32E:457) [22]Zhang Y J,Xie Y Q,Li W M.Chin J Nonferrous Met, 1996;6:114 (张迎九,谢佑卿,李为民.中国有色金属学报,1996;6:114) [23]Xu Z Y,Li L.Material Thermodynamics.3rd Edition, Beijing:Science Press,2005:30 (徐祖耀,李麟.材料热力学.第3版,北京:科学出版社,2005:30) [24]Ye D L,Hu J H.Applied Handbook of Thermodynamics Properties of Inorganic Substance.2nd Edition,Beijing: Metallurgical Industry Press,2002:278 (叶大伦,胡建华.实用无机物热力学数据手册.第2版,北京:冶金工业出版社,2002:278) |
| No Suggested Reading articles found! |
|
|