| Fracture features and deformation behaviors of electron beam weldment of a high-temperature titanium alloy Ti-60 at elevated temperature |
| CHEN Zhiyong; WANG Qingjiang; LIU Jianrong; LI Yulan; YANG Rui;LI Jinwei; LIU Fangjun |
|
Cite this article:
CHEN Zhiyong; WANG Qingjiang; LIU Jianrong; LI Yulan; YANG Rui; LI Jinwei; LIU Fangjun. Fracture features and deformation behaviors of electron beam weldment of a high-temperature titanium alloy Ti-60 at elevated temperature. Acta Metall Sin, 2008, 44(3): 263-271 .
|
|
|
|
|
Received: 28 September 2007
|
|
|
[1]Division of Titanium alloys of IMR.Unpublished Work for Ti-60 Alloys,Division of Titanium Alloys.Institute of Metal Research,Chinese Academy of Sciences,Shenyang, 2002 (Ti-60合金内部资料集.中国科学院金属研究所,沈阳,2002) [2]Liu J R.Ph.D.Dissertation,Institute of Metal Research, Chinese Academy of Sciences,Shenyang,2004. (刘建荣,中国科学院金属研究所博士学位论文,沈阳,2004) [3]BaeslackIII W A,Becker D W,Froes F H,J Met,1984; 36:46 [4]Barreda J L,Santamaria F,Azpiroz X,Irisarri A M, Varona J M.Vacuum,2001;62:143 [5]Murthy K K,Sundaresan S.Weld J,1997;76:81s [6]Murthy K K,Sundaresan S,Potluri N B.Eng Fract Mech, 1997;58:29 [7]Mohandas T,Banerjee D,Kutumbarao V V.Mater Sci Eng,1999;A269:217 [8]Oh J,Kim N J,Lee S,Lee E W.Mater Sci Eng,2003; A340:232 [9]Mohandas T,Banerjee D,Kutumbarao V V.Mater Sci Eng,1998;A254:147 [10]Burgers W G.Physica,1934;1:561 [11]Li G P.PhD Dissertation,Institute of Metal Research, Chinese Academy of Sciences,Shenyang,1995 (李阁平.中国科学院金属研究所博士学位论文,沈阳,1995) [12]Lei J F.PhD Dissertation,Institute of Metal Research, Chinese Academy of Sciences,Shenyang,1997 (雷家峰.中国科学院金属研究所博士学位论文,沈阳,1997) [13]Mohandus T,Banerjee D,Mahajan Y R,Kutumbarao V V.J Mater Sci,1996;31:3769 [14]Lin F S,Starke E A,Jr,Chakrabortty S B,Gysler A. Metall Trans,1984;15A:1229 [15]Andres C,Gysler A,Lütjering G.Z Metallkd,1997;88: 197 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|