|
|
|
| Measurement of creep rate sensitivity of microcastings at room temperature by using nanoindentation |
|
Cite this article:
. Measurement of creep rate sensitivity of microcastings at room temperature by using nanoindentation. Acta Metall Sin, 2008, 44(3): 272-276 .
[1]Mayo M J,Nix W D.Acta Metall,1988;36:2183 [2]Mayo M J,Siegel R W,Narayanasamy A,Nix W D.J Mater Res,1990;5:1073 [3]Mayo M J,Siegel R W,Liao Y X,Nix W D.J Mater Res, 1992;7:973 [4]Raman V,Berriche R.J Mater Res,1992;7:627 [5]Lucas B N,Oliver W C.Metall Mater Trans,1999;30 A: 601 [6]Chen J,Wang W,Lu L,Lu K.Acta Metall Sin,2001;37: 1179 (陈吉,汪伟,卢磊,卢何.金属学报,2001;37:1179) [7]Baumeister G,Mueller K,Ruprecht R,Hausselt J.Mi- crosyst Technol,2002;8:105 [8]Baumeister G,Ruprecht R,Hausselt J.Microsyst Technol, 2004;10:261 [9]Chung S,Park S,Lee L,Jeong H,Cho D.Microsyst Tech- nol,2005;11:424 [10]Noguchi H,Abe S.J Jpn Soc Precision Eng,2003;69: 125 (野口裕之,安部新一.精密工学会志,2003;69:125) [11]Li B S,Ren M X,Fu H Z.Foundry,2007;56:673 (李邦盛,任明星,傅恒志.铸造,2007;56:673) [12]Atkins A G,Silverio A,Tabor D.J Inst Met,1966;94: 369 [13]Wang F J,Qian Y Y,Ma X.Acta Metall Sin,2005;41: 775 (王凤江,钱乙余,马鑫.金属学报,2005;41:775) [14]Wang F,Xu K W.Acta Metall Sin,2004;40:1032 (王飞,徐可为.金属学报,2004;40:1032) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|