A study of intragranular slip and grain boundary sliding in fcc Pd
Cite this article: 

. A study of intragranular slip and grain boundary sliding in fcc Pd. Acta Metall Sin, 2008, 44(3): 257-262 .

Download:  PDF(786KB) 
Export:  BibTeX | EndNote (RIS)      
Key words:       
Received:  23 November 2007     
ZTFLH:  TG111  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2008/V44/I3/257

[1]Schiotz J,Di Tolla F D,Jacobsen K W.Nature,1998; 391:561
[2]Schiotz J,Jacobsen K W.Science,2003;301:1357
[3]Van Swygenhoven H.Phys Rev,2001;64B:224105
[4]Yamakov V,Wolf D,Phillpot S R,Mukherjee A K,Gleiter H.Natur Mater,2004;3:43
[5]Zelin M G,Mukherjee A K.Acta Mater,1995;43:2359
[6]Van Swygenhoven H,Derlet P M,Froseth A G.Nat Mater, 2004;3:399
[7]Froseth A G,Van Swygenhoven H,Derlet P M.Acta Mater,2004;52:2259
[8]Van Swygenhoven H,Derlet P M,Hasnaoui A.Phys Rev, 2002;66B:024101
[9]Van Swygenhoven H.Science,2002;296:66
[10]Chen M,Ma E,Hemker K J,Sheng H,Wang Y,Cheng X.Science,2003;300:1275
[11]Lu L,Shen Y,Chen X,Qian L,Lu K.Science,2004;304: 422
[12]Wang Y C,Li J H,Ye H Q.Philos Mag,1996;73A:213
[13]Foiles S M,Baskes M I,Daw M S.Phys Rev,1986;33B: 7983
[14]Wang Y C,Ye H Q.Philos Mag,1997;75A:261
[15]Sutton A P,Vitek V.Philos Trans R Soc,1983;309A:1
[16]Pond R C,Vitek V.Proc R Soc London,1977;357A:453
[1] WANG Luning, LIU Lijun, YAN Yu, YANG Kun, LU Lili. Influences of Protein Adsorption on the in vitro Corrosion of Biomedical Metals[J]. 金属学报, 2021, 57(1): 1-15.
[2] TUNG Feng'en;WANG Yuming Institute of Materials Science; Jilin University; Changchun. X-RAY ANALYSIS OF WORK-HARDENING PROCESS FOR POLYCRYSTALLINE а-BRASS DURING UNIAXIAL TENSILE TEST[J]. 金属学报, 1989, 25(2): 82-84.
[3] WANG Jinliang, WANG Chenchong, HUANG Minghao, HU Jun, XU Wei. The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation[J]. 金属学报, 2021, 57(5): 575-585.
[4] DU Hegui;LIU Xin Northeast University of Technology; Shenyang. KINETICS OF CARBON COMBUSTION IN PLASMA AIR[J]. 金属学报, 1989, 25(2): 85-88.
[5] . [J]. 金属学报, 2001, 37(1): 42-46 .
[6] . [J]. 金属学报, 1999, 35(3): 320-324 .
[7] . [J]. 金属学报, 2000, 36(1): 72-76 .
[8] . [J]. 金属学报, 1999, 35(3): 330-333 .
[9] . [J]. 金属学报, 1999, 35(3): 334-336 .
[10] . [J]. 金属学报, 2000, 36(6): 647-650 .
[11] . [J]. 金属学报, 2000, 36(6): 655-658 .
[12] No Author. ACTA METALLURGLCA SLNLCA Volume 28 Series A 1992 SUBJECT INDEX[J]. 金属学报, 1992, 28(12): 63-90.
[13] . [J]. 金属学报, 2000, 36(7): 780-784 .
[14] No Author. ACTA METALLURGICA SINICA(JINSHU XUEBAO) Volume 28 1992 AUTHOR INDEX[J]. 金属学报, 1992, 28(12): 71-94.
[15] Хань Яо-вэнь Инсмцмум мемаддов АН КНР;Г.н.Ойкс Московскц цнсмцмум смадц. НЗУЧЕНИЕ ПРОЦЕССОВ ДЕСУЛЬФУРАЦИИ ХНДКОΓО МЕТАЛЛА В ВАКУУМЕ[J]. 金属学报, 1963, 6(2): 98-110.
No Suggested Reading articles found!