| Modelling structural changes of a molten Cu55 cluster on cooling by molecular dynamics |
| zhang lin;;; |
| 东北大学 |
|
Cite this article:
zhang lin. Modelling structural changes of a molten Cu55 cluster on cooling by molecular dynamics. Acta Metall Sin, 2008, 44(10): 1161-1166 .
|
|
|
Abstract Structural changes of a molten Cu cluster containing 55 atoms on cooling have been investigated by employing molecular-dynamics simulations. Through microstructure analysis on pair distribution functions and atom density functions, the simulations show that the structural changes involve in three stages owing to the continuous interchange positions among atoms. In the beginning of the changes, a three-shells structure is formed in this cluster. Then, atoms in this cluster distribute in four shells, and meantime thirteen atoms in the inner part of this cluster form an icosahedron. Finally, the icosahedral structure including fifty-five atoms of this cluster is constructed. In this modeling, the shells are determined by atom density functions.
|
|
Received: 23 January 2008
|
|
|
[1]Ercolessi F,Andreoni W,Tosatti E.Phys Rev Lett,1991; 66:911 [2]Li T X,Ji Y L,Yu S W,Wang G H.Solid State Commun, 2000;116:547 [3]Zhang Z,Hu W Y,Xiao S F.Phys Rev,2006;73B:125443 [4]Liu H B,Ascencio J A,Alvarez M P,Yacaman M J.Surf Sci,2001;491:88 [5]Xu S N,Zhang L,Zhang C B,Qi Y.Acta Metall Sin,2007; 43:379 (徐送宁,张林,张彩碚,祁阳.金属学报,2007;43:379) [6]Lee Y J,Maeng J Y,Lee E K,Kim B,Kim S,Han K K. J Comput Chem,2000;21:380 [7]Chushak Y G,Bartell L S.J Phys Chem,2001;105B: 11605 [8]Valkealahti S,Manninen M.Phys Rev,1992;45B:9459 [9]Zhang L,Zhang C B,Qi Y.Chin Phys,2007;16:77 [10]Yang Q W,Zhu R Z,Wen Y H.Acta Phys Sin,2005;54: 89 (杨全文,朱如曾,文玉华.物理学报,2005:54:89) [11]Zhang L,Zhang C B,Qi Y.Phys Lett,2008;372A:2874 [12]Yildirim E K,Guven(?)Z B.Modell Simul Mater Sci Eng, 2006;14:947 [13]Nam H S,Hwang N M,Yu B D,Yoon J K.Phys Rev Lett, 2002;89:275502 [14]Ikeshoji T,Koga K.Phys Rev,2001;63E:031101 [15]Yang Q W,Zhu R Z.Acta Phys Sin,2005;54:4245 (杨全文,朱如曾.物理学报,2005;54:4245) [16]Qi W H,Wang M P,Li Z,Xie D.Chin J Nonferrous Met- als,2005;15:1854 (齐卫宏,汪明朴,李周,谢丹.中国有色金属学报,2005;15:1854) [17]Rosu M F,Pleiter F,Niesen L.Phys Rev,2001;63B: 165425 [18]Haberland H,Issendorff B V.Phys Rev Lett,1996;76: 1445 [19]Flelicke A,Kirilyuk A,Ratsch C,Behler J,Scheffler M, Von Helden G,Ferrando G.Phys Rev Lett,2004;93: 023401 [20]Chen S,Sommers J M.J Phys Chem,2001;105B:816 [21]Baumberger F,Greber T,Osterwalder J.Phys Rev,2000; 62B:15431 [22]Martin D S,Maunder A,Weightman P.Phys Rev,2001; 63B:155403 [23]Boisvert G,Lewis L J.Phys Rev,1997;56B:7643 [24]Trushin O S,Salo P,Al-Nissila T.Phys Rev,2000;62B: 1611 [25]Sprague J A,Montalenti F,Uberuaga B P,Kress J D, Voter A F.Phys Rev,2002;66B:205415 [26]Jacob T,Anton J,Sarpe-Tudoran C,Sepp W D,Fricke B,Bastu(?)T.Surf Sci,2003;536:45 [27]Frantz J,Rusanen M,Nordlund K,Koponen I T.J Phys: Condens Matter,2004;16:2995 [28]Darby S,Mortimer-Jones T V,Johnston R L,Roberts C. J Chem Phys,2002;116:1536 [29]Mei J,Davenport J W,Fernado G W.Phys Rev,1991; 43B:4653 [30]Liu J,Zhao J Z,Hu Z Q.Acta Metall Sin,2005;41:219 (刘俊,赵九洲,胡壮麒.金属学报,2005;41:219) [31]Zhang L,Wang S Q,Ye H Q.Chin Phys,2006;15:610 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|