Abstract  The effect of rare earth oxide (La2O3) contents on direct laser sintering of WC-10Co particulate reinforced Cu matrix composites was investigated. It shows that using an optimal La2O3 content of 1.0% can refine the laser sintered structure, homogenize the dispersion of reinforcing particulates and improve the particulate/matrix bonding coherence, leading to a high densification of 96.3% theoretical density and a high microhardness of HV0.1403.1. However, an excessive addition of La2O3 above 1.5% results in a decrease in the laser sintering ability. The metallurgical mechanisms of rare earth element in laser sintering of particulate reinforced metal matrix composites were discussed.
Key words:  direct metal laser sintering      metal matrix composites      WC-Co      
Received:  10 January 2007     
ZTFLH:  TG14,TG665  

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2007/V43/I9/968

[1]Simchi A.Mater Sci Eng,2006;A428:148
[2]Zhu H H,Fuh J Y H,Lu L.Rapid Prototyp J,2005;11: 74
[3]Gu D D,Shen Y F,Yang J L,Wang Y.Mater Sci Technol, 2006;22:1449
[4]Gu D D,Shen Y F.J Mater Process Technol,2007;182: 564
[5]Simchi A,Petzoldt F,Pohl H.J Mater Process Technol, 2003;141:319
[6]Das S,PuPating T P,Danyo G,Brown L E,Beaman J J, Bourell D L.Mater Des,2000;21:63
[7]Pintsuk G,Br(?)nings S E,D(?)ring J E,Linke J,Staid I, Xue L.Fusion Eng Des,2003;66-68:237
[8]Wang H M.Acta Aeronaut Astronaut Sin,2002;23:473 (王华明.航空学报,2002;23:473)
[9]Breval E,Cheng J P,Agrawal D K,Gigl P,Dennis M, Roy R,Papworth A J.Mater Sci Frog,2005;A391:285
[10]Gu D D,Shen Y F.Powder Metall,2006;49:258
[11]Cal Q K,He C L,Zhao M J,Bi J,Liu C S.Acta Metall Sin,2003;39:865 (才庆魁,贺春林,赵明久,毕敬,刘常升.金属学报,2003;39:865)
[12]Zhao M J,Liu Y,Bi J.Acta Metall Sin,2003;39:221 (赵明久,刘越,毕敬.金属学报,2003;39:221)
[13]Gui M C,Han J M,Li P Y.Mater Sci Technol,2004;20: 765
[14]Maeda K,Childs T H C.J Mater Process Technol,2004; 149:609
[15]Zhong M L,Liu W J.Acta Metall Sin,2002;38:495 (钟敏霖,刘文今.金属学报,2002;38:495)
[16]Wu P,Zhou C C,Tang X N.Acta Metall Sin,2002;38: 1257 (吴萍,周昌炽,唐西南.金属学报,2002;38:1257)
[17]Yang S,Liu W J,Zhong M L,Wang Z J,Kokawa H.J Mater Sci,2005;40:2751
[18]Gu D D,Shen Y F.Mater Lett,2006;60:3664
[19]Gu D D,Shen Y F.Mater Sci Eng,2006;A435-436:54
[20]Gu D D,Shen Y F.J Alloys Compd,2007;431:112
[21]Zheng W C,Li S S,Tang B,Zeng D B.Acta Metall Sin, 2006;42:835 (郑伟超,李双寿,汤彬,曾大本.金属学报,2006;42:835)
[22]Wu G H,Ma C J,Wang Y S,Zhu Y P,Ding W J.Acta Metall Sin,2002;38:703 (吴国华,马春江,王叶双,朱燕萍.丁文江.金属学报,2002;38:703)
[23]Yang M C,Xu J,Hu Z Q.Int J Refract Met Hard Mater, 2004;22:1
[24]Niu H J,Chang I T H.Scr Mater,1999;41:25
[25]Zhu H H,Lu L,Fuh J Y H.Mater Sci Eng,2004;A371: 170
[26]Das S.Adv Eng Mater,2003;5:701
[27]Tian Y S,Chen C Z,Chen L X,Huo Q H.Scr Mater, 2006;54:847
[28]Yuan Z F,Ke J J,Li J.Surface Tension of Metals and Alloys.Beijing:Science Press,2006:29 (袁章福,柯家骏,李晶.金属及合金的表面张力.北京:科学出版社,2006:29)
[29]Niu H J,Chang I T H.Scr Mater,1999;41:1229
[30]Zhao G M,Wang K L.Corros Sci,2006;48:273
[31]Gu D D,Shen Y F.J Alloys Compd,2007;432:163
[32]Zhal Q J,Guan S K,Shang Q Y.Alloy Thermo- Mechanism:Theory and Application.Beijing:Metallur- gical Industry Press,1999:142 (翟启杰,关绍康,商全义.合金热力学理论及其应用.北京:冶金工业出版社,1999:142)
[33]Wu C M L,Yu D Q,Law C M T,Wang L.Mater Sci Eng, 2004;R44:1
[34]Zhang K,Chen G N.Mater Sci Eng,2000;A292:229
[35]Zhao G M,Wang K L,Liu J J.Acta Metall Sin,2004;40: 1115 (赵高敏,王昆林,刘家浚.金属学报,2004;40:1115)
[36]Zhong H R.Chemical Heat Treatment of Steel with Rare Earth.Beijing:National Defence Industry Press,1998: 195 (钟华仁.钢的稀土化学热处理.北京:国防工业出版社,1998:195)
[1] ZHU Shize, WANG Dong, WANG Quanzhao, XIAO Bolv, MA Zongyi. Influence of Cu Content on the Negative Effect of Natural Aging in SiC/Al-Mg-Si-Cu Composites[J]. 金属学报, 2021, 57(7): 928-936.
[2] Xuexi ZHANG, Zhong ZHENG, Ying GAO, Lin GENG. Progress in High Throughput Fabrication and Characterization of Metal Matrix Composites[J]. 金属学报, 2019, 55(1): 109-125.
[3] WANG Yao, LIU Xuemei, SONG Xiaoyan, WEI Chongbin, WANG Haibin, WANG Xilong. SHORT-TERM PROCESS OF RECYCLING CEMENTED CARBIDE SCRAPS AND PREPARATION OF HIGH PERFORMANCE HARD METALS[J]. 金属学报, 2014, 50(5): 633-640.
[4] WANG Tiegang SONG Binghong HUA Weigang GONG Jun SUN Chao. INFLUENCE OF PROCESS PARAMETERS ON THE PERFORMANCE UNIFORMITY OF DETONATION GUN SPRAYED WC-Co COATINGS[J]. 金属学报, 2011, 47(1): 115-122.
[5] ;. EFFECTS OF SIZE COMBINATION AND CONTACTING STATE OF RAW POWDER PARTICLES ON SPARK PLASMA SINTERED ULTRAFINE CEMENTED CARBIDES[J]. 金属学报, 2007, 42(1): 0-112 .
[6] ;. FINITE ELEMENT SIMULATION FOR CYCLIC DEFORMATION OF SiCP/6061Al ALLOY COMPOSITES[J]. 金属学报, 2006, 42(10): 1051-1055 .
[7] WU Xiyong; ZHANG Wei; WANG Wei; YANG Fei; MIN Jiayuan; GUO Jingdong. Electric-Discharge Compaction of Nanocrystalline WC-10%Co Powders[J]. 金属学报, 2004, 40(9): 1000-1004 .
[8] WU Renjie (Shanghai Jiaotong University; Shanghai 200030). THE PRESENT CONDITION AND PROSPECTS ON METAL MATRIX COMPOSITES[J]. 金属学报, 1997, 33(1): 78-84.
[9] LI Chengming; WANG Jianming; XU Zhong (Taijuan University of Technology; Taiyuan 030024)LU Fanxiu; WANG Jianjun (University of Science and Technology Beijing; Beijing 100083). EFFECT OF EXCIMER LASER PRETREATMENT ON DIAMOND FILM DEPOSITED ON HARD ALLOY SUBSTRATE[J]. 金属学报, 1996, 32(9): 966-970.
[10] LI Wenfong; (Laboratory of Heat Treatment; No. 2 Deportment of Mechanical Engineering. South China University of Technology; Guangzhou; 501641) MENG Jilong (South China University of Technology; GuangzhouJI0641); DU Shanyi(Harbin Institute of Technology; Harbin 150001). INFLUENCE OF RESIDUAL THERMAL STRAIN ON TENSION AND COMPRESSION BEHAVIORS OF METAL MATRIX COMPOSITES[J]. 金属学报, 1995, 31(17): 226-232.
[11] YU Li; JIN Zhujing (Corrosion Science laboratory; Institute of Corrosion and Protection of Metals; Chinese Academy of Sciences; Shenyang); HUANG Yanqing; ZHU Tianjin; KICHIKAW A Ichiko (College of Engineering; Tokai University; Japan). EFFECT OF Co CONTENT ON GROWTH OF ARC DISCHARGE ION-PLATING WC-Co FILM[J]. 金属学报, 1994, 30(17): 229-232.
No Suggested Reading articles found!