Please wait a minute...
Acta Metall Sin  2007, Vol. 43 Issue (4): 433-438     DOI:
Research Articles Current Issue | Archive | Adv Search |
STUDY OF BRAZING ALLOY USED IN BRAZING COMPOSITE ALLOY CLADDING REINFORCED WITH HARD PARTICLES
;;;;
大连理工大学工业装备结构分析国家重点实验室
Cite this article: 

. STUDY OF BRAZING ALLOY USED IN BRAZING COMPOSITE ALLOY CLADDING REINFORCED WITH HARD PARTICLES. Acta Metall Sin, 2007, 43(4): 433-438 .

Download:  PDF(831KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  ABSTRACT A new type of brazing alloy used in brazing composite alloy cladding reinforced with hard particles on steel substrate was developed in this paper. Using the brazing alloy, stable composite alloy cladding on surface of common steel castings was made by optimum brazed hardfacing process. The composite alloy cladding is superior to other claddings obviously in design and regulation of cladding composition, microstructure and performance as well as thickness (maximum up to 30mm) according to practical demands. Besides, it is possessed of good combination property. SEM observation, energy spectrum and XRD analysis have shown that the composite alloy cladding is in strong combination with steel parent metal, and metallurgical bonding is formed between copper brazing alloy matrix and WC grains in the cladding wherein volume fraction of granular WC phase can be up to 54%. The composite alloy was composed of copper alloy solid solution as base-alloy, Cr-phase and MnNi type of compound dispersion phases as well as WC hard phase. WC particles with different grain sizes and volume fractions were close and well distributed in dispersion strengthened copper alloy. Impingement erosion wear tests have proved that the composite alloy is far superior to 30MnSiTi low-alloy steel in wear resistance.
Key words:  composite alloy cladding      brazing alloy      brazed hardfacing      tungsten carbide (hard) alloy      wear resistan     
Received:  26 September 2006     
ZTFLH:  TG425  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2007/V43/I4/433

[1]Ren L Q,Qiu X M,Li J Q,Xu D S.J Funct Mater,2000; 31:313 (任露泉,邱小明,李建桥,徐德生.功能材料,2000;31:313)
[2]Lu S P,Kwon O Y,Guo Y.Wear,2003;254:421
[3]Zhou X,Qu G H,Zhou J Y,Wang X W.J Mater Process Technol,2005;168:280
[4]Uzkut M,K(?)ksal N S,(?)nlüB S.J Mater Process Technol, 2005;169:409
[5]Pan L,Tao J,Wu S Q,Chen F.Tribology,2002;22:10 (潘蕾,陶杰,吴申庆,陈锋.摩擦学学报,2002;22: 10)
[6]Pan L,Chen F,Tao J,Wu S Q.Acta Mater Comp Sin, 2002;19(4):114 (潘蕾,陈锋,陶杰,吴申庆.复合材料学报,2002; 19(4):114)
[7]Lu S P,Kwon O Y.Surf Coat Technol,2002;153:40
[8]Lee W B,Kwon B D,Jung S B.Int J Refract Met Hard Mater,2006;24:215
[9]Chiu K Y,Cheng F T,Man H C.Mater Sci Eng,2005; A407:273
[10]Wang Z P,Wang H X,Di T.Aeronaut Manuf Technol, 2003;(11):33 (王忠平,王红霞,邸彤.航空制造技术,2003;(11):33)
[11]Deshpande P K,Lin R Y.Mater Sci Eng,2006;A418: 137
[1] WANG Haifeng, ZHANG Zhiming, NIU Yunsong, YANG Yange, DONG Zhihong, ZHU Shenglong, YU Liangmin, WANG Fuhui. Effect of Pre-Oxidation on Microstructure and Wear Resistance of Titanium Alloy by Low Temperature Plasma Oxynitriding[J]. 金属学报, 2023, 59(10): 1355-1364.
[2] ZHANG Yu, LOU Liyan, XU Qinglong, LI Yan, LI Changjiu, LI Chengxin. Microstructure and Wear Resistance of Ni-Based WC Coating by Ultra-High Speed Laser Cladding[J]. 金属学报, 2020, 56(11): 1530-1540.
[3] Hulin DONG,Haiping BAO,Jianhong PENG. Effect of TiC Contents on Mechanical Properties and Wear Resistance of Iron-Based Composites[J]. 金属学报, 2019, 55(8): 1049-1057.
[4] Shilu ZHAO,Zhen ZHANG,Jun ZHANG,Jianming WANG,Zhenggui ZHANG. MICROSTRUCTURE AND WEAR RESISTANCE OF TiAlZrCr/(Ti, Al, Zr, Cr)N GRADIENT FILMS DEPOSITED BY MULTI-ARC ION PLATING[J]. 金属学报, 2016, 52(6): 747-754.
[5] Wenfang CUI,Dong CAO,Gaowu QIN. MICROSTRUCTURE AND WEAR RESISTANCE OF Ti/TiN MULTILAYER FILMS DEPOSITED BY MAGNETRON SPUTTERING[J]. 金属学报, 2015, 51(12): 1531-1537.
[6] LIU Xiaobo, ZHAO Yuguang. MICROSTRUCTURE EVOLUTION AND WEAR RESISTANCE OF IN SITU Mg2Si/Al COMPOSITES UNDER DIFFERENT PREPARATION CONDITIONS[J]. 金属学报, 2014, 50(6): 753-761.
[7] NIU Yunsong, WEI Jie, ZHAO Jian, HU Jiaxiu, YU Zhiming. PREPARATION AND PROPERTIES OF NANOSIZED MUL-TILAYERED Ni COATINGS BY ULTRASOUND-ASSISTED ELECTRODEPOSITION[J]. 金属学报, 2013, 49(12): 1617-1622.
[8] YU Yipeng HUANG Jinfeng CUI Hua CAI Yuanhua ZHANG Jishan. EFFECT OF Nb ON THE MICROSTRUCTURE AND PROPERTIES OF SPRAY FORMED M3 HIGH SPEED STEEL[J]. 金属学报, 2012, 48(8): 935-940.
[9] ZHANG Fenggang ZHU Xiaopeng WANG Mingyang LEI Mingkai. SURFACE MODIFICATION OF WC-Ni CEMENTED CARBIDE FOR SEALS BY HIGH-INTENSITY PULSED ION BEAM IRRADIATION[J]. 金属学报, 2011, 47(7): 958-964.
[10] WANG Yanqiu WANG Yue CHEN Paiming SHAO Yawei WANG Fuhui. MICROSTRUCTURE, CORROSION AND WEAR RESISTANCES OF MICROARC OXIDATION COATING ON Al ALLOY 7075[J]. 金属学报, 2011, 47(4): 455-461.
[11] LEI Mingkai WANG Kesheng OU Yi Xiang ZHANG Lei. PLASMA–BASED LOW–ENERGY NITROGEN ION IMPLANTATION OF 2Cr13 MARTENSITIC STAINLESS STEEL USED IN PUMPS AND VALVES[J]. 金属学报, 2011, 47(12): 1490-1494.
[12] QiuYa Zhai; Cunkun Liang; Junping LIU; Qunsheng XUE. Study on Vacuum Brazing of 25Cr3MoA/YG6 Using Cu-based Microcrystalline Brazing Alloy[J]. 金属学报, 2008, 44(9): 1136-1140 .
[13] LI Jian; MAO Dongsheng; HUANG Liping; GUO Shaoyi; MAO Zhiyuan(Department of Materials Science and Engineering; Zhejiang University Hangzhou 310027Ion Beam Laboratory; Shanghai Institute of Metallurgy The Chinese Academy of Sciences; Shanghai 200050). PROPERTIES AND ABRASION WEAR RESISTANCE OF AN Al_2O_3-TiC-Co MODIFIED CERAMIC[J]. 金属学报, 1998, 34(3): 332-336.
[14] WANG Huaming(H.M.Wang)(Beijing University of Aeronautics and Astronautics; Beijing 100083). SURFACE MODIFICATION OF TiAl INTERMETALLIC ALLOYS BY LASER GAS ALLOYING[J]. 金属学报, 1997, 33(9): 917-920.
[15] LI Fengzhao;GU Yingni;JIANG Jiang;AO Qing;SUN Dongsheng (College of Materials Science and Engineering; Shandong University of Technology; Jinan 250061). MULTI-COMPONENT MICRO-ALLOYED AIR COOLING BAINITIC STEELS[J]. 金属学报, 1997, 33(5): 492-498.
No Suggested Reading articles found!