Abstract The effects of DC electric current on the precipitation of γ '-phase in a Ni-based single crystal superalloy were studied. Under the action of different current densities the superalloy was cooled at different cooling rates after solution heat treatment at 1250 ℃ for 4 h. The experiment results show that the size and volume fraction of γ '-phase increase with the increase of current density, while the planar density of γ '-phase decreases at air cooling; under the action of the same current density, the size and volume fraction of γ '-phase decrease and the planar density of γ '-phase increases with the increase of cooling rate. It is considered that the electromigration effect induced by the DC current accelerates the diffusion of atoms during γ '-phase precipitation, which enhances the precipitation of γ '-phase, and the Joule heat effect produced by the DC current reduces the cooling rate, which speeds up the growth of γ '-phase.
[1]Caron P,Khan T.Aerosp Sci Technol,1999;3:513 [2]Higginbotham G J S.Mater Sci Technol,1986;2:442 [3]Nembach E,Schanzer S,Schroer W,Trinckauf K.Acta Metall,1987;35:1471 [4]Monajati H,Jahazi M,Bahrami R,Yue S.Mater Sci Eng,2004;A373:286 [5]Ahmed S,Bond R,McKannan E C.Adv Mater Processes,1991;140:30 [6]Ahmed S,McKannan E C.Mater Sci Technol,1994;10:941 [7]Yang Y S,Zhang Q S,Hu Z Q.In:Morris D G,Naka S,Caron P,eds.,Interraetallics and Superalloys,EUROMAT 99,Vol.10,Weinheim Germany:Wiley-vch,1999:34 [8]Yang Y S,Li W F,Wang Z Z,Hu Z Q.In:Hanada S,Zhong Z,Nam S W,Wright R N,eds.,4th Pacific Rim Int Conf on Advanced Materials and Processing,Vol.1,Tokyo:The Japan Institute of Metals,2001:345 [9]Pellissier G E,Purdy S M.ASTM STP 122,1972 [10]Kearseya R M,Beddoesa J C,Jonesb P,Au P.Intermetallics,2004;12:903 [11]Conrad H.Mater Sci Eng,2000;A287:227 [12]David U F.Scr Mater,1999;40;1215 [13]Bhowal P R,Wright E F,Raymond E L.Metall Trans,1990;21A;1709a