Phase Structure and Magnetostriction of B element doped
;;
北京航空航天大学材料学院
Cite this article: 

. Phase Structure and Magnetostriction of B element doped. Acta Metall Sin, 2006, 42(8): 830-834 .

Download:  PDF(1134KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The phase structure and magnetostriction were first studied in the small atom B element doped (Fe0.81Ga0.19)100-xBx(x=0~20) alloys. The as-cast (Fe81Ga19)100-xBx alloys for x= 1 exhibits A2 and Fe2B phases, while possess Fe2B and A2+L12 eutectic phases for x=5, 10, 15, 20; Oil-quenched at 800℃ for 3h (Fe81Ga19)100-xBx alloys for x=1, 5 exhibit Modified-D03 and Fe2B phases, while possess Fe2B and Modified-D03+ L12 eutectic phases for x=10, 15, 20. The saturation magnetostriction (λs) of the as-cast (Fe0.81Ga0.19)100-xBx (x=0~20) alloys exhibits two peaks when x=1 and x=10; the λs of the oil-quenched alloys increases first and then decreases with increasing B content. The λs of (Fe81Ga19)90B10 reaches the maximum, 80% larger than the oil-quenched Fe81Ga19, attributing to the emergence of Modified-D03 phases in the oil-quenched alloys.
Key words:  Fe-Ga Alloy      magnetostriction      phase structure      B element addition      
Received:  24 November 2005     
ZTFLH:  TG111  
  TG113  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2006/V42/I8/830

[1]Clark A E,Wun-Forgle M,Restorff J B,Lograsso T A,Cullen J R.IEEE Trans Magn,2001;37:2678
[2]Wu R Q.J Appl Phys,2002;91:7358
[3]Xu X,Jiang C B,Xu H B.Acts Metall Sin,2005;41:483 (徐翔,蒋成保,徐惠彬.金属学报,2005;41:483)
[4]Restorff J B,Mun-Fogle M,Clark A E,Lograaso T A,Ross A R,Schlagel D L.J Appl Phys,2002;91:8225
[5]Bormio-Nunes C,Turtelli S R,Mueller H,Grossinger R,Sassik H,Tirelli M A.J Magn Magn Mater,2005;290-291:820
[6]Srisukhumbowornchai N,Guruswamy S.J Appl Phys,2001;90:11
[7]Coey J M D,Sun H.J Magn Magn Mater,1990;87:251
[8]Lograsso T A,Ross A R,Schlagel D L,Clark A E,WunFogle M.J Alloys Compd,2003;350:95
[9]Jiang C B,Feng G,Xu H B.Appl Phys Lett,2002;80:1619
[10]Kenneth A,Murphy,Hershkowitz N.Phys Rev,1973;7:23
[11]Ikeda O,Kainuma R,Ohnuma I,Fukamichi K,Ishida K.J Alloys Compd,2002;347:198
[12]Kawamiya N,Adachi K,Nakamura Y.J Phys Soc Jpn,1972;33:1318
[13]Clark A E,Hathaway K B,Wun-Fogle M,Restorff J B,Lograsso T A,Keppens V M,Petculescu G,Taylor R.A.J Appl Phys,2003;93:8621
[14]Han Z Y,Zhang M C,Gao X X,Tang H J,Zhou S Z.Prog Nat Sci,2004;14:638
[1] Shuangjie CHU,Yongjie YANG,Zhenghua HE,Yuhui SHA,Liang ZUO. Calculation of Magnetostriction Coefficient for Laser-Scribed Grain-Oriented Silicon Steel Based onMagnetic Domain Interaction[J]. 金属学报, 2019, 55(3): 362-368.
[2] Quan FU,Yuhui SHA,Zhenghua HE,Fan LEI,Fang ZHANG,Liang ZUO. Recrystallization Texture and Magnetostriction in Binary Fe81Ga19 Sheets[J]. 金属学报, 2017, 53(1): 90-96.
[3] LIU Yin, LIU Tie, WANG Qiang, WANG Huimin, WANG Li, HE Jicheng. EFFECT OF HIGH MAGNETIC FIELD ON CRYSTAL ORIENTATION, MORPHOLOGY AND MAGNETOSTRICTION OF TbFe2 AND Tb0.27Dy0.73Fe1.95 ALLOYS DURING HEAT TREATMENT PROCESS[J]. 金属学报, 2013, 49(9): 1148-1152.
[4] YAO Zhanquan, ZHAO Zengqi, JIANG Liping,HAO Hongbo, WU Shuangxia,ZHANG Guangrui, YANG Jiandong. EFFECTS OF Ce ADDITION ON THE MICROSTRUCTURE AND MAGNETOSTRICTION OF Fe83Ga17 ALLOY[J]. 金属学报, 2013, 49(1): 87-91.
[5] LI Xiaocheng DING Yutian HU Yong. MICROSTRUCTURE AND MAGNETOSTRICTION OF THE Tb0.3Dy0.7Fe1.95-xTix (x=0, 0.03, 0.06, 0.09) ALLOYS[J]. 金属学报, 2012, 48(1): 11-15.
[6] CUI Yue JIANG Chengbao XU Huibin. INTRINSIC MAGNETOSTRICTION OF Tb-Dy-Fe-Co ALLOY[J]. 金属学报, 2011, 47(2): 214-218.
[7] CHEN Libiao ZHU Xiaoxi LI Chuan LIU Jinghua JIANG Chengbao XU Huibin. <001> ORIENTED SINGLE CRYSTAL GROWTH AND MAGNETOSTRICTION OF Fe81Ga19 ALLOYS[J]. 金属学报, 2011, 47(2): 169-172.
[8] ZHANG Zhiqiang DONG Limin YANG Yang GUAN Shaoxuan LIU Yuyin YANG Rui. INFLUENCES OF QUENCHING TEMPERATURE ON THE MICROSTRUCTURE AND DEFORMATION BEHAVIORS OF TC16 TITANIUM ALLOY[J]. 金属学报, 2011, 47(10): 1257-1262.
[9] ZHANG Changsheng MA Tianyu YAN Mi PEI Yongmao GAO Xu. MAGNETOMECHANICAL DAMPING CAPACITY OF <110> ORIENTED Tb0.36Dy0.64(Fe0.85Co0.15)2 ALLOY[J]. 金属学报, 2009, 45(6): 749-753.
[10] ZHU Xiaoxi ZHANG Tianli JIANG Chengbao. ELECTROMECHANICAL COUPLING COEFFICIENT (K33) OF Fe72.5Ga27.5 MAGNETOSTRICTIVE ALLOY[J]. 金属学报, 2009, 45(4): 455-459.
[11] JIA Ao ZHANG Tianli MENG Hao JIANG Chengbao. MAGNETOSTRICTION AND EDDY CURRENT LOSS OF BONDED GIANT MAGNETOSTRICTIVE PARTICLE COMPOSITES[J]. 金属学报, 2009, 45(12): 1473-1478.
[12] Gao Xue-xu. Texture and magnetostriction in rolled Fe-Ga based alloy[J]. 金属学报, 2008, 44(9): 1031-1034 .
[13] LIN Jian; Haiyan ZHAO; Zhipeng CAI; Yongping LEI. STUDY ON THE RELATIONSHIP BETWEEN MAGNETIC FIELD AND RESIDUAL STRESS IN STEEL MATERIALS[J]. 金属学报, 2008, 44(4): 451-456 .
[14] ZHANG Su; LIU Jinghua; JIANG Chengbao; XU Huibin. Melt quenched Fe81Ga19 magnetostriction alloy[J]. 金属学报, 2008, 44(3): 361-364 .
[15] Xu Yun-Wei; MA Tian-Yu; Mi YAN. MAGNETOSTRICTION IN ANTIFERROMAGNETIC Fe1-xMnx (0.30 ≤ x ≤ 0.55) ALLOYS[J]. 金属学报, 2008, 44(10): 1235-1237 .
No Suggested Reading articles found!