| theoretical and experimental standardization of strain hardening index in tensile deformation |
| SONG Yuquan; GUAN Zhiping; MA Pinkui; SONG Jiawang |
| Superplastic and Plastic Research Institute; Jilin University; Changchun 130025 |
|
Cite this article:
SONG Yuquan; GUAN Zhiping; MA Pinkui; SONG Jiawang. theoretical and experimental standardization of strain hardening index in tensile deformation. Acta Metall Sin, 2006, 42(7): 673-680 .
|
|
|
Abstract Based on state equation that stress is a function of strain and strain-rate, the differential constitutive equation during superplastic tensile deformation is deduced, and then the mechanical meaning of strain hardening index in the equation is interpreted. The constraint equation of strain hardening index is deduced, strain hardening indexes in typical deformation paths are defined, and their interrelations are gotten. Measuring formulae of strain hardening indexes in typical deformation paths and accurate measuring methods by numerical simulation are deduced. According to them, strain hardening indexes are experimentally measured, and measuring methods & results are elaborately analyzed. The results prove that: not only does strain hardening index be non-constant, but also has close relations with the changing rule of strain and deformation path; not only does strain hardening index have close relations with deformation path, but also with adopted measuring formula. Therefore, as strain hardening index is quoted, its corresponding deformation path should be shown clearly; when strain hardening index is measured, the measuring formula of its corresponding deformation path should be adopted.
|
|
Received: 02 March 2006
|
|
|
[1] Ludwik P. Phys Z, 1909; 10: 411 [2] Hollomon J H. Trans ASM, 1944; 32: 123 [3] Song Y Q, Suo Z L,Guan Z P, Liu Y. Acta Metall Sin, 2006; 42: 337 (宋玉泉,索忠林,管志平,刘颖.金属学报,2006;42:337) [4] Song Y Q. J Jilin Univ Technol, 1985; (1): 13 (宋玉泉.吉林工业大学学报,1985;(1):13) [5] Song Y Q. J Jilin Univ Technol, 1992; 22(1): 1 (宋玉泉.吉林工业大学学报, 1992;22(1):1) [6] Song Y Q, Cheng Y C, Liu Y. Sci Chin, 2001; 44 E: 113 [7] Song Y Q, Hai J T, Guan Z P. Sci Chin, 2001; 44 E: 561 [8] Song Y Q, Cheng Y C, Wang X W. Sci Chin, 2001; 44 E:365 [9] Song Y Q, Cheng Y C. Chin Pat, ZL 00 1 17802.4 (宋玉泉,程永春.中国发明专利ZL 00 1 17802.4) [10] Song Y Q, Cheng Y C, Hou L. Chin Mech Eng, 1999; 10: 782 (宋玉泉,程永春,侯 磊.中国机械工程, 1999;10:782) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|