| MAGNETOSTRICTION AND MICROSTRUCTURE OF THE MELT-SPUN Fe83Ga17 ALLOY |
| Honglin Jiang |
| 北京科技大学新金属材料国家重点实验室 |
|
Cite this article:
Honglin Jiang. MAGNETOSTRICTION AND MICROSTRUCTURE OF THE MELT-SPUN Fe83Ga17 ALLOY. Acta Metall Sin, 2006, 42(2): 177-180 .
|
|
|
Abstract The ribbons with different thickness of Fe83Ga17 alloy were prepared by the melt-spun and the microstrcucture and magntostriction were investigated. It was found that the magnetostriction was related to the thickness of ribbons and the maximum magnetostriction of -2100 ×10-6 has been obtained in the ribbon with thickness of 75 μm. The XRD and DSC results showed that DO3 structure emerges in those ribbons with thickness of 45、55、75μm. The transition of A2+DO3→A2 occurred at 669℃ for the ribbon of 75 μm. The microstructure of ribbons showed that the increase of melt-spun cooling rate can restrain the precipitation of Ga-rich phase. It is considered that the giat magnetostriction of ribbons originates from the A2 +special DO3 structure and shape magnetic anisotropy .
|
|
Received: 20 May 2005
|
|
|
[1] Guruswamy S, Srisukhumbowornchai N, Clark A E, Restorff J B, Wun-Fogle M. Scr Mater, 2000; 43: 239 [2] Han Z Y, Zhou S Z, Zhang M C, Gao XX. J Magn Mater Devices, 2004; 35(1): 15 ??(韩智勇,周寿增,张茂才,高学绪.磁性材料及器件,2004;35(1):15) [3] Srisukhumbowornchai N, Guruswamya, S. J Appl Phys, 2002; 92: 5371 [4] Kumagai A, Fujita A, Fukamichi K, Oikawa K, Kainuma R, Ishida K. J Magn Mater, 2004; 272-276: 2060 [5] Clark A E, Hathaway K B, Wun-Fogle M, Restorff J B, Lograsso T A, Keppens V M, Petculescu G, Taylor R A. J Appl Phys, 2003; 93: 8621 [6] Ikeda O, Kainuma R, Ohnutna I, Fukamichi K, Ishida K. J Alloy Compd, 2002; 347: 198 [7] Kellogg R A, Flatau A B, Clark A E, Wun-Fogle M, Lograsso T A. J Appl Phys, 2002; 91: 7821 [8] Cheng S F, Das B N, Wun-Fogle M, Lubitz P, Clark A E. IEEE Trans Magn, 2002; 38: 2838 [9] Liu G D, Li Y X, Hu H N, Qu J P, Liu Z H, Dai X F, Zhang M, Cui Y T, Chen J L, Wu G H. Ada Phys Sin, 2004; 53: 3191(刘国栋,李养贤,胡海宁,曲静萍,柳祝红,代学芳,张铭,崔玉亭,陈京兰,吴光恒.物理学报,2004;53:3191) [10] Lograsso T A, Ross A R, Schlagel D L, Clark A E, Wun-Fogle M. J Alloy Compd, 2003; 350: 95 [11] Han Z Y, Zhang M C, Gao X X, Zhou S Z. Prog Nat Sci, 2004; 14: 593(韩智勇,张茂才,高学绪,周寿增.自然科学进展,2004;14:593) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|