Abstract  The aging of a drawn eutectoid carbon steel with true strain 2.89 at different temperatures has been studied by means of TEM and electrical resistance measurement. The results indicated that the aging at 473K for 1hr improved the tensile strengths from 2245.65MPa of as-drawn to 2448.52MPa. Better mechanical property with combination of strength and ductility was observed after aging at 673K for 1h. Further increase of aging temperatures deteriorated the property possibly due to the recrystalization. The underlying mechanism of the better mechanical properties after aging at low temperature (673K) is considered to associate with the precipitation of fine carbide dissociated in the drawing.
Key words:  eutectoid pearlite steel      cold drawing      aging precipitation      
Received:  13 February 2006     
ZTFLH:  TG113.2  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2006/V42/I10/1009

[1]Tagushira S,Sakai K,Furuhara T,Maki T.ISIJ Int,2000;40:1149
[2]Gridnev V N,Nemoshkalenko V V.Phys Status Solidi,1975;31A:201
[3]Read H G,Reynolds W T.Scr Mater,1997;37:1221
[4]Languillaume J,Kapelski G.Acta Mater,1997;45:1201
[5]Nam W J,Bae C M.Scr Mater,2000;42:457
[6]Ivanisenko Y,Lojkowski W,Valiev R Z.Acta Mater,2003;51:5555
[7]Taniyama A,Takayama T.Scr Mater,2004;51:53
[8]Hono K,Ohnuma M,Nishida S.Scr Mater,2001;44:977
[9]Gavriljuk V G.Scr Mater,2001;45:1469
[10]Haasen P.In:Cahn R W,Haasen P,Kramer E J eds.,Materials Science and Technology,Vol.5,Weinheim:VCH,
??1991
[11]Gridnev V N,Gavrilyuk V G.Phys Status Solidi,1972;14A:689
[12]Valiey R Z,Ivanisenko Y,Rauch E F.Acta Mater,1996;44:4705
[13]Shin D H,Kim Y S,Lavernia E J.Acta Mater,2001;49:2387
[14]Xu Y,Umemoto M,Tsuchiya K.Mater Trans,2002;43:2205
[15]Wilson D V.Acta Mater,1957;5:293
[16]Cottrell A H.Dislocation and Plastic Flow in Crystals.Oxford:Clarendon Press,1953:127
[17]Ivanisenko Y,Wunderlich R K,Valiev R Z.Scr Mater,2003;49:947
[18]Orowan E.Symposium on Internal Stress in Metals and Alloys.London:Institute of Metals,1948:451
[1] WANG Changsheng, FU Huadong, ZHANG Hongtao, XIE Jianxin. Effect of Cold-Rolling Deformation on Microstructure, Properties, and Precipitation Behavior of High-Performance Cu-Ni-Si Alloys[J]. 金属学报, 2023, 59(5): 585-598.
[2] GONG Xiangpeng, WU Cuilan, LUO Shifang, SHEN Ruohan, YAN Jun. Effect of Natural Aging on Artificial Aging of an Al-2.95Cu-1.55Li-0.57Mg-0.18Zr Alloy at 160oC[J]. 金属学报, 2023, 59(11): 1428-1438.
[3] CHEN Junzhou, LV Liangxing, ZHEN Liang, DAI Shenglong. Precipitation Strengthening Model of AA 7055 Aluminium Alloy[J]. 金属学报, 2021, 57(3): 353-362.
[4] Peibei JI, Lichu ZHOU, Xuefeng ZHOU, Feng FANG, Jianqing JIANG. Study on Anisotropic Mechanical Properties of Cold Drawn Pearlitic Steel Wire[J]. 金属学报, 2018, 54(4): 494-500.
[5] Lichu ZHOU,Xianjun HU,Chi MA,Xuefeng ZHOU,Jianqing JIANG,Feng FANG. EFFECT OF PEARLITIC LAMELLA ORIENTATION ON DEFORMATION OF PEARLITE STEEL WIRE DURING COLD DRAWING[J]. 金属学报, 2015, 51(8): 897-903.
[6] ZHANG Xiaodan A. Godfrey LIU Wei LIU Qing. EVOLUTIONS OF MICROSTRUCTURE AND FERRITIC MICRO–ORIENTATION AND TEXTURE IN A PEARLITIC STEEL WIRE DURING COLD DRAWING[J]. 金属学报, 2010, 46(2): 141-146.
[7] YANG Wenchao WANG Mingpu SHENG Xiaofei ZHANG Qian WANG Zheng’an. STUDY OF THE AGING PRECIPITATION AND HARDENING BEHAVIOR OF 6005A ALLOY SHEET FOR RAIL TRAFFIC VEHICLE[J]. 金属学报, 2010, 46(12): 1481-1487.
[8] HUANG Wenke KONG Fanya. MICROSTRUCTURE AND MECHANICAL PROPERTY OF COLD DRAWN HIGH STRENGTH 00Cr18Ni10N STAINLESS STEEL WIRE[J]. 金属学报, 2009, 45(3): 275-279.
No Suggested Reading articles found!