| Crystallographic Orientation Relationship Between a Al2O3 and Al in In Situ Al2O3 Reinforced Al-4Mg Matrix Composites |
| OUYANG Liuzhang; LUO Chengping |
| College of Mechanical Engineering; South China University of Technology; Guangzhou 510641 |
|
Cite this article:
OUYANG Liuzhang; LUO Chengping. Crystallographic Orientation Relationship Between a Al2O3 and Al in In Situ Al2O3 Reinforced Al-4Mg Matrix Composites. Acta Metall Sin, 2005, 41(7): 750-754 .
|
|
|
Abstract Al2O3 particles, in situ decomposed from
Al2(SO4)3,
reinforced Al--4Mg matrix composites were made through stir casting.
Al2O3/Al interface in the Al--4Mg matrix composites
was studied by transmission electron microscopy (TEM). The measurements
of crystallographic orientation relationship between
Al2O3 and Al at Al2O3/Al interface show that
no fixed and unique orientation relationship existed, though the following
preferential ones were observed:
:( )Al2O3//(111) Al,[ ]Al2O3//[ ] Al,[ ]Al2O3//[ ] Al。
|
|
Received: 24 October 2004
|
|
|
[1]Ouyung L Z,Luo C P,Sui X D,Luo Z X.J Chin Nonfer rous Met,2000;10:159 (欧阳柳章,罗承萍,隋贤栋,骆灼旋.中国有色金属学报,2000; 10:159) [2]Ouyang L Z,Luo C P,Sui X D,Luo Z X.Foundry Technol, 1999;6:40 (欧阳柳章,罗承萍,隋贤栋,骆灼旋.铸造技术, 1999;6: 40) [3]Lloyd D J,Jin I,Weatherly G C.Scr Metall Mater,1994; 31:393 [4]Pfeifer M.J Mater Sci,1990;25:1563 [5]Liu S A,Mei Z,Cui K.Spec Cast Nonferrous Alloy,1997; (5):7 (刘少安,梅志,崔昆.特种铸造及有色合金, 1997;(5): 7) [6]Halistedt B,Liu Z K,Agren J.Mater Sci Eng,1990;A129: 135 [7] Zhong W M, Esperance G L, Suery M. Metall Mater Trans, 1995; 26A: 2625 [8] Liu Z, Liu X M. Spec Cast Nonferrous Alloy, 1997; (5): 10 (刘 政,刘小梅.特种铸造及有色合金, 1997;(5):10) [9] Oguocha N A, Yannacopoulos S. J Mater Sci, 1999; 34: 3335 [10] Lee J C, Subramanian K N. J Mater Sci, 1994; 29: 1983 [11] Luo C P, Sui X D, Ouyang L Z, Luo Z X. Acta Metall Sin, 1999;35: 343 (罗承萍,隋贤栋,欧阳柳章,骆灼旋.金属学报, 1999;35: 343) [12] Sui X D, Luo C P, Ouyang L Z, Luo Z X. Chin J Mater Res, 2000; 14: 168 (隋贤栋,罗承萍,欧阳柳章,骆灼旋.材料研究学报, 2000; 14:168) |