Abstract Effect of high vertical magnetic field on the directional solidification
structure of eutectic MnBi/Bi has been investigated. It has been found
that high magnetic field has enhanced the formation of MnBi fiber and make
the directional solidification structure of eutectic MnBi/Bi more regular;
with the increase of the intensity of the magnetic field, the
average spacing and diameters of MnBi fibers increase at same growth
rate; magnetic field makes the morphology of MnBi phase
change and enhances the faceted growth character of MnBi phase.
|
|
Received: 02 September 2004
|
|
|
[1]Guo X,Altounian Z,Stromolser J O.J Appl Phys,1991;69:6067 [2]Pirich R G.Metall Trans,1984;15A:2139 [3]Savas M A,Smith R W.J Cryst Growth,1986;76:880 [4]Notis M R,Shah D M,Young S P,Graham C D.IEEE Trans Magn,1979;3:957 [5]Chen T.J Appl Phys,1974;45:2358 [6]Decarlo J L,Pirich R G.Metall Trans,1984;15A:2155 [7]Pirich R G.In:Rindone G E,ed.,Materials Processing in the Reduced Gravity Environment of Space.New York: Elsevier Science Publishing Co.,1982:593 [8]Pirich R G,Larson D J.In:Rindone G E,ed.,Materials Processing in the Reduced Gravity Environment of Space. New York:Elsevier Science Publishing Co.,1982:523 [9]Wang H,Ren Z M,Deng K,Xu K D.Acta Metall Sin, 2002;38:41 (王晖,任忠鸣,邓康,徐匡迪.金属学报,2002;38:41) [10]Yasuda H,Ohnaka I,Yamamoto Y,Tokieda K,Kishio K. Mater Trans,2003;44:2207 [11]Li X,Ren Z M,Wang H,Li W X,Deng K,Zhuang Y Q. Acta Metall Sin,2004;40:40 (李喜,任忠鸣,王晖,李伟轩,邓康,壮云乾.金属学报,2004;40:40) [12]Gaber F E,Wilcox W R.J Cryst Growth,1986;78:159 [13]Elloit R.Eutectic Solidification Processing Crystalline and Glossy Alloy.London:Butterworths & Co.,1983:165 [14]Feng D,Ding S Y,Zhai H R.Physics of Metal.Vol.4,Beijing:Science Press,1998:460 (冯端,丁世英,翟宏如.金属物理学(第4卷).北京;科学出版社,1998:460) [15]Yu J,Wang W,Jinag J Q,Shu G J.J Southeast Univ,1992;22(2):59 (于金,王武,蒋建清,舒光冀.东南大学学报,1992;22(2):59) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|